Recovery of Vanadium and Nickel from a High CaCO3 Containing Petroleum Coke Ash by Roasting and Acidic Leaching

被引:0
|
作者
Yurtseven, Ozgun [1 ]
Ibrahim, Ahmedaljaali Ibrahim Idrees [1 ]
Top, Soner [2 ]
Kursunoglu, Sait [3 ]
Altiner, Mahmut [1 ]
机构
[1] Cukurova Univ, Dept Min Engn, Div Mineral Proc, TR-01330 Adana, Turkiye
[2] Abdullah Gul Univ, Dept Engn Sci, TR-38100 Kayseri, Turkiye
[3] Batman Univ, Dept Petr & Nat Gas Engn, TR-72100 Batman, Turkiye
关键词
Extraction; Vanadium; Nickel; Petroleum coke; Roasting; Acidic leaching; SULFURIC-ACID; FLY-ASH; SPENT CATALYSTS; EXTRACTION; SLAG; KINETICS; PRECIPITATION; LEACHATE; TITANIUM; PLANT;
D O I
10.1007/s40831-023-00762-6
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
In this study, it was aimed to extract vanadium (V) and nickel (Ni) from a petroleum coke ash (PCA) using a roasting process without additives, followed by leaching with sulfuric acid (H2SO4). The experiments were designed based on the Taguchi approach, taking into account the parameters of temperature, acid concentration, time, and solid ratio. Additional leaching tests were conducted on the non-roasted PCA for comparison, to assess the effect of roasting on the extractions of V and Ni. The results showed that no extra reducing agent was needed as the PCA contained high levels of CaCO3, which could be used as a reducing agent during roasting. It was found that roasting was essential for high Ni extractions, but had no strong effects on V extractions. The Ni extraction was found to be between 13.3 and 80.8% for the non-roasted PCA and between 43.6 and 99.3% for the roasted PCA. The V extraction was between 36 and 97.9% for the non-roasted PCA and between 45.4 and 99.9% for the roasted PCA. The optimal leaching conditions were determined to be a sulfuric acid of 4.5 M, a solid ratio of 10%, a temperature of 75 degrees C, and a time of 75 min. In addition, it was determined that the leaching conditions had a great effect on the oxidation state of vanadium ions, and an increase in the acid concentration led to the formation of V3+ ions (green color) instead of VO2+ ions (blue color) in the pregnant leach solution. The final pregnant leach solution containing 1056.50 mg/L V, and 251.85 mg/L Ni was achieved with an extraction yields of > 98%. The experimental results were greatly fitted by the shrinking core model and the activation energy (E-a) for V and Ni was calculated as 3.60 and 4.01 kJ/mol, indicating that the leaching mechanism can be explained by the diffusion control model.
引用
收藏
页码:1744 / 1758
页数:15
相关论文
共 28 条
  • [21] Unveiling high-performance carburized mild steel using coconut shell ash and CaCO3 nanoparticles derived from periwinkle shell
    Adedipe, Oyewole
    Aigbodion, Victor Sunday
    Agbo, Nicholas Agbese
    Lawal, Sunday Albert
    Oyeladun, Oyebola Wahab Akanni
    Mokwa, James Baba
    Dauda, Emmanuel Toi
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 126 (9-10): : 4711 - 4721
  • [22] Recovery of Li from waste Li-containing Al electrolytes with high F and Na contents by using a CaO roasting-water leaching process
    Zhao, Shuai
    Li, Yongli
    Guo, Qiang
    Wang, Lina
    Qi, Tao
    Zhang, Ling
    JOURNAL OF ENVIRONMENTAL MANAGEMENT, 2024, 368
  • [23] Recovery of vanadium and tungsten from waste selective catalytic reduction catalysts by K2CO3 roasting and water leaching followed by CaCl2 precipitation
    Liu, Xianghui
    Yang, Qiaowen
    INTERNATIONAL JOURNAL OF COAL SCIENCE & TECHNOLOGY, 2021, 8 (04) : 727 - 736
  • [24] Recovery of vanadium and tungsten from waste selective catalytic reduction catalysts by K2CO3 roasting and water leaching followed by CaCl2 precipitation
    Xianghui Liu
    Qiaowen Yang
    International Journal of Coal Science & Technology, 2021, 8 : 727 - 736
  • [25] Microwave-enhanced selective leaching calcium from steelmaking slag to fix CO2 and produce high value-added CaCO3
    Liu, Lincheng
    Fan, Xiaohui
    Gan, Min
    Wei, Jiaoyang
    Gao, Zitan
    Sun, Zengqing
    Ji, Zhiyun
    Wu, Yufeng
    Li, Jinhua
    SEPARATION AND PURIFICATION TECHNOLOGY, 2024, 330
  • [26] Glycine-mediated leaching-mineralization cycle for CO2 sequestration and CaCO3 production from coal fly ash: Dual functions of glycine as a proton donor and receptor
    Zheng, Xuan
    Liu, Jiayao
    Wei, Yibin
    Li, Kangkang
    Yu, Hai
    Wang, Xiaolong
    Ji, Long
    Yan, Shuiping
    CHEMICAL ENGINEERING JOURNAL, 2022, 440
  • [27] Efficient lithium recovery from lithium-containing spent aluminium electrolyte via NaF fluorination roasting and Al2(SO4)3 leaching
    Han, Zexun
    Wu, Yongchong
    Hao, Pengcheng
    Tan, Xuan
    Wei, Mingren
    Lv, Xiaojun
    JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2023, 11 (05):
  • [28] Nano- and micro-scale characterisation of interfacial transition zone (ITZ) of high volume slag and slag-fly ash blended concretes containing nano SiO2 and nano CaCO3
    Hosan, Anwar
    Shaikh, Faiz Uddin Ahmed
    Sarker, Prabir
    Aslani, Farhad
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 269