Friction and wear of multiple steel wires in a wire rope

被引:21
|
作者
Peng, Yuxing [1 ,2 ]
Huang, Kun [1 ,2 ]
Ma, Chenbo [3 ]
Zhu, Zhencai [1 ,2 ]
Chang, Xiangdong [1 ,2 ]
Lu, Hao [1 ,2 ]
Zhang, Qing [1 ,2 ]
Xu, Chunming [1 ,2 ]
机构
[1] China Univ Min & Technol, Sch Mech & Elect Engn, Jiangsu Key Lab Mine Mech & Elect Equipment, Xuzhou 221116, Peoples R China
[2] Jiangsu Collaborat Innovat Ctr Intelligent Min Equ, Xuzhou 221008, Peoples R China
[3] Nanjing Forestry Univ, Sch Mech & Elect Engn, Nanjing 210037, Peoples R China
基金
中国国家自然科学基金;
关键词
steel wires; fretting; friction behavior; helical contact; wear mechanism; FRETTING FATIGUE BEHAVIORS; FINITE-ELEMENT; HOISTING ROPE; COAL-MINE; STRAND; CONTACT; CABLES;
D O I
10.1007/s40544-022-0665-y
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The fretting wear among the steel wires aggravates the wire rope's fatigue damage, affects the service performance of the wire ropes, and threatens mine hoisting safety. In this paper, the practical friction behavior and wear mechanism among the wires in the wire rope are investigated. A series of tests were carried out on multiple steel wires in helical contact and tension-torsion coupling under different fretting parameters, twisting parameters, and lubrication conditions by self-made friction and wear testing machine. The results show that the coefficient of friction (COF) among the steel wires decreases slightly with increasing lateral loads and tension, and the effect of twist angle on the COF has opposite results under different lubrication conditions. Lateral loads, tension of the steel wires, twist angle, and lubrication condition all affect the fretting morphology among the steel wires. Fretting wear with larger twist angle structure leads to more energy loss. The energy loss of fretting is directly related to the fretting morphology among the contact surfaces, and the dissipated energy is lower in the two forms of complete slip and sticking. The wear depth and width increase with the increase of lateral loads, steel wire tension, and twist angle. And the wear width and depth under dry friction conditions are higher than those under oil lubrication conditions. In addition, the wear mechanism under dry friction conditions is mainly abrasive wear, adhesive wear, and fatigue wear. And the wear mechanism under oil lubrication conditions is mainly abrasive wear and fatigue wear.
引用
收藏
页码:763 / 784
页数:22
相关论文
共 50 条
  • [41] Fretting wear behaviors of hoisting rope wires in acid medium
    Xu, Linmin
    Zhang, Dekun
    Yin, Yan
    Wang, Songquan
    Wang, Dagang
    MATERIALS & DESIGN, 2014, 55 : 50 - 57
  • [42] EFFECT OF ROPE LUBRICANTS ON SYNTHETIC FIBER CORES IN STEEL WIRE ROPE
    NAUMANN, B
    GEDECKE, G
    WIRE, 1972, 22 (119): : 128 - &
  • [43] Fretting friction and wear of steel wires in tension-torsion and helical contact form
    Xu, Chun-ming
    Peng, Yu-xing
    Zhu, Zhen-cai
    Lu, Hao
    Chen, Guo-an
    Wang, Da-gang
    Peng, Xia
    Wang, Shu-jing
    WEAR, 2019, 432
  • [44] Fretting wear behaviors of steel wires under friction-increasing grease conditions
    Shen, Yan
    Zhang, Dekun
    Duan, Junjie
    Wang, Dagang
    TRIBOLOGY INTERNATIONAL, 2011, 44 (11) : 1511 - 1517
  • [45] Sliding Friction and Wear Characteristics of Wire Rope Contact with Sheave under Long-Distance Transmission Conditions
    Chang, Xiangdong
    Peng, Yuxing
    Zhu, Zhencai
    Lu, Hao
    Tang, Wei
    Zhang, Xing
    MATERIALS, 2022, 15 (20)
  • [46] FASTENING STEEL WIRE ROPE FOR TENSILE TESTING
    MALINOVSKII, VA
    INDUSTRIAL LABORATORY, 1978, 44 (05): : 720 - 721
  • [47] METAL-CORED STEEL WIRE ROPE
    BUKSHTEIN, MA
    STAL IN ENGLISH-USSR, 1967, (02): : 180 - +
  • [48] The loss of elasticity of steel wire rope.
    Hoefer, K
    ZEITSCHRIFT DES VEREINES DEUTSCHER INGENIEURE, 1939, 83 : 775 - 780
  • [49] Steel wire rope NDT: New instruments
    Sukhorukov, VV
    PREVIOUS EXPERIENCE AND CURRENT INNOVATIONS IN NON-DESTRUCTIVE TESTING, 2001, : 225 - 230
  • [50] A MACHINE FOR THE FATIGUE TESTING OF STEEL ROPE WIRE
    DORODNYKH, BN
    INDUSTRIAL LABORATORY, 1962, 28 (12): : 1628 - 1629