Effect of Tip Content on the Work Hardening and Softening Behavior of Mg-Zn-Ca Alloy

被引:9
|
作者
Zhang, Jin-Kai [1 ]
Wang, Cui-Ju [1 ]
Fan, Yi-Dan [1 ]
Xu, Chao [2 ]
Nie, Kai-Bo [1 ]
Deng, Kun-Kun [1 ]
机构
[1] Taiyuan Univ Technol, Coll Mat Sci & Engn, Shanxi Key Lab Adv Magnesium Based Mat, Taiyuan 030024, Peoples R China
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Titanium particle content; Particle reinforced magnesium matrix composites; Work hardening; Softening behavior; Mechanical properties; MECHANICAL-PROPERTIES; STRESS-RELAXATION; ROOM-TEMPERATURE; MICROSTRUCTURE; DEFORMATION; COMPOSITE; NANOCOMPOSITES; EXTRUSION; EVOLUTION;
D O I
10.1007/s40195-023-01557-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The -Ti-p/ ZX60 composites with different -Ti-p contents were prepared by semi- solid stirring casting. After extrusion, the microstructure, work hardening and softening behavior of the -Ti-p/ZX60 composites were analyzed compared with the ZX60 (Mg-6Zn-0.2Ca) alloy. The results showed that the addition of -Ti-p could not only promote the nucleation of dynamic recrystallized (DRXed) grains, but also be propitious to the refinement of DRXed grains. With increasing -Ti-p content, the size of DRXed grains decreased accompanied with increasing volume fraction of DRXed grains. As the -Ti-p content increased to 15 vol.%, the average size and volume fraction of DRXed grains reached to similar to 0.32 mu m and 93.2%, respectively. Besides, both the strength and elongation were improved by the addition of -Ti-p. With increasing content of -Ti-p, a substantial increase in the strength was achieved with little change in the elongation. However, the elongation decreased sharply when the -Ti-p content further increased to 15 vol.%. The addition of -Ti-p led to an increase in the work hardening rate, which gradually increased with increasing -Ti-p content. However, the softening rate did not demonstrate the same tendency with increasing -Ti-p content. Unlike the conventional ceramic particles, the -Ti-p can be deformed in coordination with the matrix alloy, which imparted a higher softening rate to the matrix alloy. Even though the softening rate improved as the -Ti-p content increased from 5 to 10 vol.%, it dropped deeply as the -Ti-p content increased to 15 vol.% owing to the fracture of -Ti-p during extrusion.
引用
收藏
页码:551 / 560
页数:10
相关论文
共 50 条
  • [41] Mechanical properties and controlling degradation rate of Mg-Zn-Ca alloy
    Zhang, Ya-Jing
    Zuo, Li-Jing
    Xing, Xiao-Le
    Wang, Fan
    Dongbei Daxue Xuebao/Journal of Northeastern University, 2013, 34 (07): : 935 - 938
  • [42] Enhancing mechanical properties of an Mg-Zn-Ca alloy via extrusion
    Du, Yuzhou
    Du, Wei
    Zhang, Danli
    Ge, Yanfeng
    Jiang, Bailing
    MATERIALS SCIENCE AND TECHNOLOGY, 2021, 37 (06) : 624 - 631
  • [43] Mg-Zn-Ca amorphous alloys for application as temporary implant: Effect of Zn content on the mechanical and corrosion properties
    Matias, T. B.
    Roche, V.
    Nogueira, R. P.
    Asato, G. H.
    Kiminami, C. S.
    Bolfarini, C.
    Botta, W. J.
    Jorge, A. M., Jr.
    MATERIALS & DESIGN, 2016, 110 : 188 - 195
  • [44] The effect of grain size on deformation modes and deformation heterogeneity in a rolled Mg-Zn-Ca alloy
    Shou, Haoge
    He, Liuyong
    Zheng, Jiang
    Li, Tianjiao
    Xia, Lihong
    Yin, Dongdi
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 22 : 1723 - 1736
  • [45] Study on the Microstructure, Mechanical Properties and Corrosion Behavior of Mg-Zn-Ca Alloy Wire for Biomaterial Application
    Zheng, Maobo
    Xu, Guangquan
    Liu, Debao
    Zhao, Yue
    Ning, Baoqun
    Chen, Minfang
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (04) : 1837 - 1846
  • [46] Bio-Corrosion Behavior of Ceramic Coatings Containing Hydroxyapatite on Mg-Zn-Ca Magnesium Alloy
    Ding, Hong-Yan
    Li, Hong
    Wang, Guo-Qing
    Liu, Tao
    Zhou, Guang-Hong
    APPLIED SCIENCES-BASEL, 2018, 8 (04):
  • [47] Study on the Microstructure, Mechanical Properties and Corrosion Behavior of Mg-Zn-Ca Alloy Wire for Biomaterial Application
    Maobo Zheng
    Guangquan Xu
    Debao Liu
    Yue Zhao
    Baoqun Ning
    Minfang Chen
    Journal of Materials Engineering and Performance, 2018, 27 : 1837 - 1846
  • [48] In vivo degradation behavior of Ca-deficient hydroxyapatite coated Mg-Zn-Ca alloy for bone implant application
    Wang, Huanxin
    Guan, Shaokang
    Wang, Yisheng
    Liu, Hongjian
    Wang, Haitao
    Wang, Liguo
    Ren, Chenxing
    Zhu, Shijie
    Chen, Kuisheng
    COLLOIDS AND SURFACES B-BIOINTERFACES, 2011, 88 (01) : 254 - 259
  • [49] Antimicrobial Bioresorbable Mg-Zn-Ca Alloy for Bone Repair in a Comparison Study with Mg-Zn-Sr Alloy and Pure Mg
    Zhang, Chaoxing
    Lin, Jiajia
    Nhu Y Nguyen
    Guo, Yuxing
    Xu, Changlu
    Seo, Catherine
    Villafana, Edgar
    Jimenez, Hector
    Chai, Yang
    Guan, Renguo
    Liu, Huinan
    ACS BIOMATERIALS SCIENCE & ENGINEERING, 2020, 6 (01): : 517 - 538
  • [50] Hot Deformation and Work Hardening Behavior of an Extruded Mg–Zn–Mn–Y Alloy
    N.Tahreen
    D.F.Zhang
    F.S.Pan
    X.Q.Jiang
    D.Y.Li
    D.L.Chen
    Journal of Materials Science & Technology, 2015, 31 (12) : 1161 - 1170