Insights into the hot corrosion of CoCrFeNi high entropy alloy in molten Na2SO4+25 %K2SO4 at 900 °C

被引:7
|
作者
Zan, Chaofei [1 ]
Chen, Jie [1 ]
Zhang, Huihui [1 ]
Yuan, Juntao [2 ]
机构
[1] Xian Univ Sci & Technol, Sch Mat Sci & Engn, Xian 710054, Peoples R China
[2] CNPC Tubular Goods Res Inst, State Key Lab Performance & Struct Safety Petr Tub, Xian 710077, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
CoCrFeNi; High entropy alloy; Hot corrosion; Electrochemical impedance; (Na; K)2SO4; HIGH-TEMPERATURE CORROSION; ELECTROCHEMICAL IMPEDANCE; BEHAVIOR; OXIDATION; SUPERALLOYS; MIXTURES; NACL; NI;
D O I
10.1016/j.ijoes.2023.100192
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Hot corrosion is the accelerated oxidation of salt contaminants such as (Na,K)2SO4 deposited on the turbine blade surface. This paper provides an insight into the potential application of CoCrFeNi high entropy alloy (HEA) as a hot corrosion-resistant alloy working at high temperatures. The hot corrosion behavior of CoCrFeNi HEA was investigated through mass gain, EIS, SEM, EDS, and XRD. The results show that the mass gain of hot corrosion increased in the first 20 h and decreased after 30 h due to a large amount of oxide film peeling off. The EIS comprised three capacitive loops before 4 h, and two capacitive loops after 6 h. It indicates that dis-continuous spinel oxide composed of multi-elements is rapidly formed on the surface of the alloy at the initial stage of hot corrosion, and a Cr-rich (Cr,Fe)2O3 layer is formed inside the alloy as time passes. The corrosion products for 10 h are mainly composed of porous (Fe,Cr,Co)3O4 spinel in the outer layer and Cr-rich (Cr,Fe)2O3 in the inner layer. As time approaches 100 h, the outer spinel layer peels off seriously. The primary corrosion product consists of (Fe,Cr,Co)3O4. The internal sulfide phenomenon occurs in the matrix.
引用
收藏
页数:9
相关论文
共 50 条
  • [41] PRETRANSITION IN CRYSTALS OF K2SO4
    KOLONTSO.EV
    KULAGO, EE
    BYAKHOVA, NI
    MIKHAILE.IE
    DOKLADY AKADEMII NAUK SSSR, 1973, 210 (03): : 567 - &
  • [42] THE SEEBECK COEFFICIENT OF K2SO4
    LIN, CY
    HIRAYAMA, C
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1982, 129 (08) : C339 - C339
  • [43] Thermodynamic studies of mixed aqueous solutions of binary electrolytes of Na2SO4 and K2SO4
    Sirbu, R
    THERMOCHIMICA ACTA, 2000, 352 : 1 - 10
  • [44] HOT CORROSION OF NICKEL IN NA2SO4-CASO4-PBO SALT MIXTURES AT 900-DEGREES-C
    SHATYNSKI, SR
    ARBAB, M
    JOURNAL OF METALS, 1980, 32 (12): : 5 - 5
  • [45] MATRIX-ISOLATION IR AND RAMAN STUDIES OF MOLECULES NA2SO4 AND K2SO4
    ATKINS, RM
    GINGERICH, KA
    CHEMICAL PHYSICS LETTERS, 1978, 53 (02) : 347 - 349
  • [46] The efficient conversion of K2SO4 from Na2SO4 by continuous electrodialysis metathesis process
    Liu, Jie
    Li, Dandan
    Xu, Fan
    Yuan, Junsheng
    Ji, Zhiyong
    Zhao, Yingying
    Li, Fei
    Guo, Xiaofu
    Wang, Shizhao
    DESALINATION AND WATER TREATMENT, 2021, 238 : 267 - 276
  • [47] PHASE STUDIES ON SYSTEMS NA2SO4-SO3 K2SO4-SO3 AND NA2SO4-K2SO4-SO3
    COATS, AW
    DEAR, DJA
    PENFOLD, D
    JOURNAL OF THE INSTITUTE OF FUEL, 1968, 41 (326): : 129 - &
  • [48] FORMATION OF NA2SO4 AND K2SO4 IN FLAMES DOPED WITH SULFUR AND ALKALI CHLORIDES AND CARBONATES
    FRYBURG, GC
    MILLER, RA
    STEARNS, CA
    KOHL, FJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1977, 124 (08) : C315 - C315
  • [49] Modeling and simulation of continuous electrodialysis metathesis process for conversion of Na2SO4 to K2SO4
    Wang, Xu
    Du, Yawei
    Liu, Jie
    Xu, Fan
    Ji, Zhiyong
    Guo, Xiaofu
    Li, Fei
    Yuan, Junsheng
    DESALINATION, 2022, 528
  • [50] Raman spectral quantification of Li2SO4, Na2SO4, K2SO4 and Cs2SO4 at 25 to 250 °C and its potential implications for the determination of sulfate contents in natural fluid inclusions
    Chen, Chen
    Shang, Linbo
    Zhou, Yunhe
    Jiang, Ziqi
    Wang, Xinsong
    Chou, I-Ming
    Li, Jianguo
    Wang, Zhenglong
    ORE GEOLOGY REVIEWS, 2024, 168