Microstructure and Mechanical Properties of TA2/Q235 Laser Weld Joint with Copper Interlayer

被引:3
|
作者
Zhang, Liang [1 ]
Wang, Qi [1 ]
Guo, Xiaolei [1 ]
Chen, Pan [1 ]
Wang, Yinling [1 ]
Wang, Chen [1 ]
Wang, Zhanxue [1 ]
Wang, Zongling [1 ]
机构
[1] Huanghuai Univ, Coll Energy Engn, Zhumadian 463000, Peoples R China
基金
中国国家自然科学基金;
关键词
microstructure; mechanical properties; laser weld; dissimilar metal; copper interlayer; TITANIUM-ALLOY; STAINLESS-STEEL;
D O I
10.3390/ma16103838
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
For the dissimilar metal welding needs of TA2 titanium and Q235 steel, preliminary trials were conducted using laser welding methods, and the results showed that the addition of a copper interlayer and the bias of the laser beam toward the Q235 side allowed for an effective connection. The welding temperature field was simulated using the finite element method, and the optimum offset distance of 0.3 mm was obtained. Under the optimized parameters, the joint had good metallurgical bonding. Further SEM analysis showed that the microstructure of the bonding area between the weld bead and Q235 was a typical fusion weld pattern, while that of the bonding area between the weld bead and TA2 was in brazing mode. The microhardness of the cross-section showed complex fluctuations; the microhardness of the weld bead center was higher than that of the base metal due to the formation of a mixture microstructure of copper and dendritic Fe phases. The copper layer not involved in the weld pool mixing had almost the lowest microhardness. The highest microhardness was found at the bonding site of TA2 and the weld bead, mainly due to the formation of an intermetallic layer with a thickness of about 100 m. Further detailed analysis revealed that the compounds included Ti2Cu, TiCu and TiCu2, showing a typical peritectic morphology. The tensile strength of the joint was approximately 317.6 MPa, reaching 82.71% of that of the Q235 and 75.44% of the TA2 base metal, respectively. The fracture occurred in the unmixed copper layer.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Microstructure, mechanical properties and residual stress of a 2205DSS/Q235 rapidly formed LBW joint
    Du, Chengchao
    Wang, Xue
    Hu, Lei
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2018, 256 : 78 - 86
  • [22] Microstructure and Mechanical Properties of TA2/304 Weld Seam with Cu Transition Layer under Bias Oscillation Laser Welding Process
    Li, Yun-long
    Di, Hong-shuang
    Chen, Li-qing
    Wang, Xiao-nan
    Li, Tian-xiang
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (10) : 4962 - 4975
  • [23] Influence mechanism of copper interlayer on the interface bonding during wire and laser additive repair of TA1/Q235 bimetallic sheets
    Zhang, Hetian
    Xu, Rongzheng
    Zhao, Xiao
    Cheng, Jian
    Yan, Wandi
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2024, 238 (06) : 1164 - 1174
  • [24] Laser cladding of electroplated Ni-WC on surface of TA2:microstructure and mechanical properties
    Wang, Liuyong
    Song, Peng
    Wu, Haoyue
    Wang, Wenqin
    Tu, Bing
    Yan, Ming
    Li, Yulong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 967
  • [25] Mechanical properties and interfacial structure of hot-roll bonding TA2/Q235B plate using DT4 interlayer
    Yu, C.
    Xiao, H.
    Yu, H.
    Qi, Z. C.
    Xu, C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 695 : 120 - 125
  • [26] Study on explosive welding of Ta2 titanium to Q235 steel using colloid water as a covering for explosives
    Yang Ming
    Ma Hong-hao
    Shen Zhao-wu
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (06): : 5572 - 5580
  • [27] Effect of Weld Temperature on Microstructure and Properties of TM52/Q235 Transient Liquid Phase Diffusion-Bonded Joint
    Bensheng Huang
    Jinsong Chen
    Lei Zhang
    Yanqiu Wu
    Jianneng Zheng
    Journal of Materials Engineering and Performance, 2023, 32 : 7456 - 7467
  • [28] 爆炸焊接TA2/Q235钢复合板末端开裂的原因
    刘鹏
    陆明
    冀鑫炜
    庞敬军
    机械工程材料, 2012, 36 (01) : 48 - 51+93
  • [29] Effect of Weld Temperature on Microstructure and Properties of TM52/Q235 Transient Liquid Phase Diffusion-Bonded Joint
    Huang, Bensheng
    Chen, Jinsong
    Zhang, Lei
    Wu, Yanqiu
    Zheng, Jianneng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (16) : 7456 - 7467
  • [30] Effect of DT4 Interlayer on Properties of Hot-roll Bonding TA2/Q235B Plate
    Yu, Chao
    Xiao, Hong
    Li, Na
    Qi, Zichen
    Ren, Zhongkai
    2017 2ND INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS RESEARCH AND MANUFACTURING TECHNOLOGIES (AMRMT 2017), 2017, 229