Research on hole inhibiting mechanism of 5A06 aluminum alloy during laser oscillating fuse deposition forming

被引:4
|
作者
Song, Yongda [1 ]
Yuan, Chengwei [1 ]
Huang, Wenhao [2 ]
Zhao, Yun [3 ]
Jia, Yazhou [4 ]
机构
[1] Shandong Univ Technol, Sch Mech Engn, Zibo 255000, Peoples R China
[2] Wenzhou Univ, Wenzhou 325035, Peoples R China
[3] Jiangsu Automat Res Inst, Lianyungang 222006, Jiangsu, Peoples R China
[4] North China Inst Aerosp Engn, Langfang 065000, Peoples R China
来源
关键词
Circular oscillation; Numerical simulation; Molten pool flow; Additive manufacturing; Laser fuse; Porosity; POROSITY FORMATION;
D O I
10.1016/j.optlastec.2023.109530
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
To meet the requirements of aerospace components integration and lightweight, it is urgent to improve the forming and manufacturing technology for lightweight materials. Laser fuse material increasing technology can satisfy the integrated forming of large and complex components, but due to the high energy of the laser, pore appears in aluminum alloy after rapid cooling after heat melting, which leads to the high porosity of formed components and poor overall deposition performance. This paper proposes the effect of reducing workpiece porosity by adding laser oscillation in laser fuse material increasing technology. The research simulates the deposition process of laser fuse material increasing under different process parameters, compares and analyses the experiment and simulation results of laser swing fuse material increasing, and summarizes the influence of swing parameters on laser fuse forming by combining the experiment overall forming morphology, section morphology and simulation results. The results show that during the manufacturing process of laser fuse material increasing, due to the heating and impact of the laser, depressions are formed at the front of the melting pool, and the contact surface between the depression and air layer is blocked by the melting pool, then small holes are formed so that the air inside the small holes can not escape completely and then form pores. When adding a laser circular swing, the shallower the orifice position, the faster the pressure diffusion inside the molten pool, the higher the possibility of the orifice discharging air, and the smaller the number and size of the pore. The surface finish and flatness of the workpiece are also better than those without a swing. High-frequency circular oscil-lation increases the possibility of hole wall breakage, makes the air inside the hole exhaust longer, and suppresses the pore better. The research is helping to improve the understanding of the deposition process in laser -oscillating augmentation manufacturing of aluminum alloy, to reduce the pore problems encountered in laser -fused augmentation of aluminum alloy, and to provide the selection of corresponding process parameters.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Microbial corrosion behavior and mechanism of 5A06 aluminum alloy under low dose proton radiation
    Chen, Nana
    Liu, Qianqian
    Feng, Yali
    Zou, Shiwen
    Yao, Qiong
    Lu, Lin
    Wu, Junsheng
    Xiao, Kui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 4533 - 4540
  • [32] Joint performance of laser-TIG double-side welded 5A06 aluminum alloy
    Chen Yan-bin
    Miao Yu-gang
    Li Li-qun
    Wu Lin
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2009, 19 (01) : 26 - 31
  • [33] Microstructure and porosity characteristics of 5A06 aluminum alloy joints using laser-MIG hybrid welding
    Zhan, Xiaohong
    Zhao, Yanqiu
    Liu, Zemin
    Gao, Qiyu
    Bu, Hengchang
    JOURNAL OF MANUFACTURING PROCESSES, 2018, 35 : 437 - 445
  • [34] Grain size characterization of 5A06 aluminum alloy plates with different deformation amounts based on laser ultrasonic
    Ning, Xinfei
    Han, Xinghui
    Wang, Xiaokai
    Hua, Lin
    Hu, Xuan
    Ren, Chaoshan
    MEASUREMENT, 2024, 238
  • [35] Study on corrosion behavior and mechanism of 5A06 aluminum alloy in N2O4 medium
    Yao, Xiuquan
    Wen, Lei
    Yu, Zhigang
    Guo, Wei
    Huang, Feifei
    Qiang, Yujie
    Jin, Ying
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 931
  • [36] Research on Measurement of Residual Stress of Welded 5A06 Aluminum Alloy Based on Synchrotron Radiation Diffraction Technology
    Han, Yuelin
    Qi, Junfeng
    Cai, Quan
    Yang, Guanghui
    Yang, Bin
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (01): : 205 - 212
  • [37] Research on Measurement of Residual Stress of Welded 5A06 Aluminum Alloy Based on Synchrotron Radiation Diffraction Technology
    Han Yuelin
    Qi Junfeng
    Cai Quan
    Yang Guanghui
    Yang Bin
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (01) : 205 - 212
  • [38] Vertical up welding characteristics of 5A06 aluminum alloy by 10 KW-level oscillation laser beam
    Disheng Fang
    Fujia Xu
    Ruisheng Huang
    Linlin Li
    Kai Xu
    Jipeng Zou
    Welding in the World, 2022, 66 : 2091 - 2105
  • [39] WC nano-particle surface injection via laser shock peening onto 5A06 aluminum alloy
    Lu, Liang
    Huang, Ting
    Zhong, Minlin
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (22): : 4525 - 4530
  • [40] Study on the formation of welding, microstructure, and properties of 5A06 aluminum alloy by ultrasonic laser-assisted filler welding
    Guo H.
    Zhang D.
    Zhao Y.
    Lei Z.
    Li Q.
    Yang Y.
    Xu Y.
    Zhongguo Kexue Jishu Kexue/Scientia Sinica Technologica, 2020, 50 (11): : 1521 - 1528