Ablation behavior of HfC coatings modified by novel HfxTa1-xC solid solution nanowires under oxyacetylene flame

被引:6
|
作者
Chen, Hui [1 ]
Zhang, Yulei [1 ,2 ]
Li, Zhenglong [1 ]
Fu, Yanqin [2 ]
Yin, Xuemin [1 ]
Li, Jingtong [1 ]
Li, Jinjing [1 ]
Wang, Jing [1 ]
机构
[1] Northwestern Polytech Univ, Carbon Carbon Composites Res Ctr, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] Henan Acad Sci, Carbon Matrix Composites Res Inst, Henan Key Lab High Performance Carbon Fiber Reinfo, Zhengzhou 450046, Peoples R China
基金
中国国家自然科学基金;
关键词
Carbon/carbon composites; HfxTa1-xC solid solution nanowires; Nanowire layer; HfC anti-ablation coating; Ablation behavior; C/C COMPOSITES; CARBON/CARBON COMPOSITES; HAFNIUM CARBIDE; MICROSTRUCTURE; RESISTANCE; OXIDATION; PHASE; TEMPERATURE; TANTALUM; GROWTH;
D O I
10.1016/j.ceramint.2023.12.285
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
HfC exhibits great potential for ablation resistant coating of carbon/carbon composites due to its ultra -high melting point and high temperature resistance. In this work, we proposed to develop the novel HfxTa1-xC solid solution nanowires with perfect ultra -high temperature property and unique one-dimensional (1D) nanostructures to modify HfC coating for further improved ablation resistance of the coating. Results showed that the novel Hf0.5Ta0.5C solid solution nanowires exhibited excellent ablation resistance, which could maintain 1D morphology under oxyacetylene flame ablation above 2100 degrees C. In addition, the morphology of Hf0.5Ta0.5C solid solution nanowire layer exhibited significant effect on the morphology and ablation behavior of coatings. The linear ablation rate of HfC anti -ablation coating with porous Hf0.5Ta0.5C solid solution nanowire layer decreased by 60.87 % compared with that without nanowires. Our works provide a basis for enhancing the protective ability of coatings under severe ablation environments.
引用
收藏
页码:9668 / 9677
页数:10
相关论文
共 11 条
  • [1] Novel HfxTa1-xC solid solution nanowire toughened HfC coating: An effective strategy for synchronous enhanced mechanical and anti-ablation performance
    Chen, Hui
    Zhang, Yulei
    Fu, Yanqin
    Gai, Wenhan
    Zhao, Junhao
    Zhang, Haohui
    JOURNAL OF ADVANCED CERAMICS, 2024, 13 (05): : 590 - 601
  • [2] Ablation behavior of HfC protective coatings for carbon/carbon composites in an oxyacetylene combustion flame
    Wang, Ya-lei
    Xiong, Xiang
    Li, Guo-dong
    Liu, Huai-fei
    Chen, Zhao-ke
    Sun, Wei
    Zhao, Xue-jia
    CORROSION SCIENCE, 2012, 65 : 549 - 555
  • [3] Design and preparation of multilayer TaC/HfC coating: Ablation behavior under oxyacetylene flame with different heat flux
    Zhang, Jian
    Zhang, Yulei
    Zhu, Xiaofei
    Fu, Yanqin
    Chen, Ruicong
    Gai, Wenhan
    CORROSION SCIENCE, 2022, 204
  • [4] Cyclic ablation behavior of mullite-modified C/C-HfC-SiC composites under an oxyacetylene flame at about 2400 °C
    Jiao, Xiaoyang
    Tan, Qing
    He, Qinchuan
    Qing, Mingcong
    Wang, Yiqun
    Yin, Xuemin
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (10) : 4309 - 4321
  • [5] Ablation behavior of CVD-TaC coatings with different crystal structures for C/C composites under oxyacetylene flame
    Kong, Jing'an
    Zhang, Yulei
    Chen, Guohui
    Zhang, Pengfei
    Gai, Wenhan
    Wang, Hanhui
    Li, Hejun
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (15) : 6898 - 6907
  • [6] Ablation behavior of mullite modified C/C-SiC-HfC composites under oxyacetylene torch for single and cyclic ablations with two heat fluxes
    Jiao, Xiaoyang
    He, Qinchuan
    Tan, Qing
    Yin, Xuemin
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (14) : 5851 - 5862
  • [7] Ablation behavior of C/C-Zr1-xHfxC-SiC composites under an oxyacetylene flame at above 2500 °C
    Jiao, Xiaoyang
    He, Qinchuan
    Qing, Mingcong
    Wang, Yiqun
    Yin, Xuemin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 24 : 3235 - 3251
  • [8] Comparison of the ablation resistance of mullite modified C/C-SiC-HfC and C/C-SiC-HfC composites under oxyacetylene flame of 2.38 MW/m2 heat flux
    Jiao, Xiaoyang
    He, Qinchuan
    Feng, Jie
    Tan, Qing
    Wang, Yiqun
    Yin, Xuemin
    CERAMICS INTERNATIONAL, 2023, 49 (22) : 36580 - 36589
  • [9] The ablation behavior of mullite modified C/C-SiC-ZrC composites under oxyacetylene flame at a heat flux of 4.18 MW/m2 with different mullite content
    Gong, Gu
    He, Qinchuan
    Wang, Yiqun
    Yin, Xuemin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1020
  • [10] Preparation and ablation behavior analysis of non-equimolar C f /(Hf 1/2 Zr 1/ 3 Ti 1/6 )C composites under oxyacetylene flame with different heat fluxes
    Song, Xin
    Zhang, Zhongwei
    Ye, Li
    Li, Weijie
    Han, Weijian
    Yan, Shengman
    CERAMICS INTERNATIONAL, 2024, 50 (15) : 26482 - 26492