Achieving excellent strength-ductility combination in Ti-6Al-4V alloy by spark plasma sintering technology using large-diameter PREP spherical powder

被引:0
|
作者
Yu, Suoqing [1 ,2 ]
Zhang, Yuqin [1 ,2 ,3 ]
Shi, Yaming [3 ]
Wang, Junsheng [3 ]
Jiang, Yehua [1 ,2 ]
机构
[1] Kunming Univ Sci & Technol, Fac Mat Sci & Engn, Kunming 650031, Peoples R China
[2] Natl local Joint Engn Res Ctr Technol, Adv Met Solidificat Forming & Equipment Technol, Kunming 650093, Peoples R China
[3] Engn Technol Res Ctr Titanium Prod & Applicat, Chuxiong 651209, Peoples R China
关键词
Ti-6Al-4V alloy; Large -diameter spherical powder; Spark plasma sintering; Microstructure evolution; Mechanical properties; ROTATING ELECTRODE PROCESS; MECHANICAL-PROPERTIES; BIMODAL MICROSTRUCTURES; VARIANT SELECTION; TITANIUM-ALLOY; PARTICLE-SIZE; PHASE; TEMPERATURE; PARAMETERS; TENSILE;
D O I
10.1016/j.jmrt.2024.02.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Powder metallurgy (PM) technology is expected to provide a promising strategy for the cost-effective and highly efficient utilization of spherical Ti-6Al-4V powders with particles size of large than 150 mu m to reduce material waste. However, how to overcome the problem of low sinterability and poor ductility of coarse lamellar microstructures of large-diameter spherical powders are still remains a significant challenge. In this study, Ti-6Al-4V alloys were prepared by spark plasma sintering (SPS) at different sintering temperatures with plasma rotating electrode process (PREP) large-diameter spherical powders (similar to 156 mu m). The microstructure evolution, grain structure, mechanical properties and fracture mechanisms were systematically investigated. Results demonstrate that the acicular martensite structure inside the unmelted particles changed to a uniform and fine alpha/beta lamellar microstructure with the increased sintering temperature. Consequently, the Ti-6Al-4V alloys exhibit excellent strength-ductility at 925 C-degrees. (ultimate tensile strength of 881 MPa and elongation up to 14.8 %). Fundamentally, the excellent strength-ductility was attributed to the uniform and dense fine alpha/beta lamellar structure that enhanced the effective bearing area during deformation. The stacked dislocations at the alpha/beta phase interface provided high strength. In addition, the high-density alpha/beta phase interface in the matrix reduced the mean free path of the dislocation, which resulted in a high strain hardening rate of the high-density geometrically necessary dislocations (GNDs) and delayed the premature fracture. The intergranular brittle fracture mode of the alloys changed to the ductile fracture mode. These findings have important implications for recycling super-large diameter spherical powders.
引用
收藏
页码:2572 / 2584
页数:13
相关论文
共 50 条
  • [21] Diffusion Bonding of Al7075 to Ti-6Al-4V by Spark Plasma Sintering and Using a Copper Interlayer
    Alhazaa, Abdulaziz
    Albrithen, Hamad
    Hezam, Mahmoud
    Shar, Muhammad Ali
    Alhwaimel, Ibrahim
    Alharbi, Yasser
    Estournes, Claude
    CRYSTALS, 2022, 12 (09)
  • [22] Superior strength-ductility balance in hot pressed swarf-Ti-6Al-4V alloy
    Zhao, Qinyang
    Pi, Ziqiang
    Lu, Xin
    Qu, Yingdong
    Bolzoni, Leandro
    Yang, Fei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 788
  • [23] Bimorphic microstructure in Ti-6Al-4V alloy manipulated by spark plasma sintering and in-situ press forging
    Kang, L. M.
    Cai, Y. J.
    Luo, X. C.
    Li, Z. J.
    Liu, X. B.
    Wang, Z.
    Li, Y. Y.
    Yang, C.
    SCRIPTA MATERIALIA, 2021, 193 : 43 - 48
  • [24] Synthesis of Ti-6Al-4V alloy with nano-TiN microstructure via spark plasma sintering technique
    Falodun, O. E.
    Obadele, B. A.
    Oke, S. R.
    Maja, M. E.
    Olubambi, P. A.
    4TH INTERNATIONAL CONFERENCE ON MECHANICAL, MATERIALS AND MANUFACTURING (ICMMM 2017), 2017, 272
  • [25] Strength-ductility improvement achieved by introducing heterostructured martensite in a Ti-6Al-4 V alloy
    Yang, Zhiyuan
    Wen, Fangming
    Sun, Qi
    Chai, Linjiang
    Ma, Xinkai
    Zhu, Minhao
    MATERIALS CHARACTERIZATION, 2022, 192
  • [26] The variation of microstructure by α-β forging and its effect on the strength and ductility in Ti-6Al-4V alloy
    Nakase, K
    Inagaki, I
    Ariyasu, N
    Tsubakino, H
    ZEITSCHRIFT FUR METALLKUNDE, 2005, 96 (12): : 1413 - 1419
  • [27] A novel Ti-6Al-4V alloy microstructure with very high strength and good ductility
    Jia, M. T.
    Zhang, D. L.
    Gabbitas, B.
    Liang, J. M.
    Kong, C.
    SCRIPTA MATERIALIA, 2015, 107 : 10 - 13
  • [28] Achieving bi-lamellar microstructure with both high tensile strength and large ductility in Ti-6Al-4V alloy by novel thermomechanical processing
    Chong, Yan
    Bhattacharjee, Tilak
    Yi, Jangho
    Zhao, Shiteng
    Tsuji, Nobuhiro
    MATERIALIA, 2019, 8
  • [29] Stereolithography coupled with spark plasma sintering to produce Ti-6Al-4V complex shapes
    Le Cloarec, Joseph
    Marinel, Sylvain
    Estournes, Claude
    Dehmas, Moukrane
    Folton, Cendrine
    Maniere, Charles
    JOURNAL OF MANUFACTURING PROCESSES, 2024, 114 : 122 - 135
  • [30] Nitridation of Ti-6Al-4V powder in thermal plasma conditions and sintering of obtained TiN powder
    Marchand, Cecile
    Maitre, Alexandre
    Grimaud, Alain
    Denoirjean, Alain
    Lefort, Pierre
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (05): : 1988 - 1994