Optimization of microstructure and properties in U75V steel rail cladding layers manufactured by laser melting deposition and laser shock peening

被引:9
|
作者
Wu, Hulin [1 ]
Huang, Shuhai [1 ]
Li, Zhongsheng [1 ]
Chen, Peng [2 ]
Tan, Hong [3 ]
Xia, Zhixin [2 ,4 ]
机构
[1] Southwest Technol & Engn Res Inst, Chongqing 400039, Peoples R China
[2] Soochow Univ, Shagang Sch Iron & Steel, Suzhou 215021, Peoples R China
[3] Soochow Univ, Engn Training Ctr, Suzhou 215100, Peoples R China
[4] 8 Jixue Rd, Suzhou 215021, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
U75V steel rail; Pearlite; Wear; Laser melting deposition; Laser shock peening; ROLLING-CONTACT FATIGUE; RCF PERFORMANCE; WEAR-RESISTANCE; BEHAVIOR; DAMAGE; ALLOY; DEFECTS;
D O I
10.1016/j.optlastec.2023.109436
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
Onsite rail repair is essential to ensure service security and reduce operational costs. In this study, laser melting deposition (LMD) was used to repair damaged U75V steel rail. When the substrate of U75V steel rail was pre-heated at 350 degrees C, thermal cycling and heat accumulation characterized using LMD contributed to the formation of a pearlitic microstructure, same as that of the U75V steel rail substrate. Compared with the U75V steel rail substrate, mechanical properties and friction and wear properties of the cladding layers were improved mean-time. To further improve wear resistance, laser shock peening (LSP) was performed on the surface of the cladding layers during post treatment, such that the lamellar Fe3C phase in pearlite was refined into a type of "degen-erated" pearlitic microstructure. The dry friction and wear tests were conducted on the substrate, cladding layers, and cladding layer post LSP. Results indicated that oxidative wear was caused by heat accumulation and the heavy load during the dry friction and wear tests, and ploughing groove and spalling were observed as the main forms of wear. The cladding layers after LSP exhibited minimum wear loss and the best wear resistance.
引用
收藏
页数:6
相关论文
共 50 条
  • [1] Tailoring microstructure and mechanical properties of U75V steel manufactured by laser direct energy deposition combining cobalt addition with preheating treatment
    Liu, Zhonghan
    Yu, Yunhe
    Chen, Peng
    Hou, Jixin
    Xia, Zhixin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 860 - 869
  • [2] Formation mechanism of pearlite during thermal cycling in U75V steel rail repaired by laser directed energy deposition
    Chen, Peng
    Chen, Lei
    Xu, Jiachao
    Huang, Shuhai
    Xia, Zhixin
    JOURNAL OF LASER APPLICATIONS, 2021, 33 (03)
  • [3] Research on Multilayer and Multipass Laser Cladding Process for U75V Rails
    Tong Tong
    Zhu Jialei
    Liang Xu
    LASER & OPTOELECTRONICS PROGRESS, 2021, 58 (07)
  • [4] Effects of Quenching Temperature and Cooling Rate on the Microstructure and Mechanical Properties of U75V Rail Steel
    Lan, Yuzhe
    Zhao, Gang
    Xu, Yaowen
    Ye, Chuanlong
    Zhang, Shaocheng
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2019, 8 (02) : 249 - 255
  • [5] Effects of Quenching Temperature and Cooling Rate on the Microstructure and Mechanical Properties of U75V Rail Steel
    Yuzhe Lan
    Gang Zhao
    Yaowen Xu
    Chuanlong Ye
    Shaocheng Zhang
    Metallography, Microstructure, and Analysis, 2019, 8 : 249 - 255
  • [6] The dynamic load-bearing performance of the laser cladding Fe-based alloy on the U75V rail
    Yang, Jiaoxi
    Ma, Wenyu
    Zhang, Wentao
    Wang, Xiaojian
    Huang, Kai
    Liu, Zhe
    Zhou, Zheng
    Xu, Hongchao
    Xiao, Junheng
    INTERNATIONAL JOURNAL OF FATIGUE, 2022, 165
  • [7] Influence of CDFW Process Parameters on Microstructure and Mechanical Properties of U75V Rail Steel Welded Joint
    Zhang, Han
    Li, Chang'an
    Zhu, Zhiming
    METALS, 2022, 12 (05)
  • [8] Optimization of the dilution parameters to improve wear resistance of laser cladding 15-5PH steel coating on U75V pearlitic steel
    Zhang, Bo
    Wang, Huaming
    Zhang, Shuquan
    He, Bei
    SURFACE & COATINGS TECHNOLOGY, 2023, 465
  • [9] A study on the effects of laser shock peening on the microstructure and substructure of Ti-6Al-4V manufactured by Selective Laser Melting
    Leo, J. R. O.
    Zabeen, S.
    Fitzpatrick, M. E.
    Zou, J.
    Attallah, M. M.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2023, 316
  • [10] Microstructure and corrosion resistance of stainless steel manufactured by laser melting deposition
    Yang, S. F.
    Li, C. W.
    Chen, A. Y.
    Gan, B.
    Gu, J. F.
    JOURNAL OF MANUFACTURING PROCESSES, 2021, 65 : 418 - 427