Fatigue strength improvement of linear friction welded butt joints of low carbon steel by pressurizing after oscillation

被引:2
|
作者
Miao, Huilin [1 ]
Tsutsumi, Seiichiro [2 ]
Yamashita, Takayuki [1 ]
Morisada, Yoshiaki [1 ]
Fujii, Hidetoshi [1 ]
机构
[1] Osaka Univ, Joining & Welding Res Inst, Osaka 5670047, Japan
[2] Osaka Univ, Grad Sch Engn, Osaka 5650871, Japan
基金
日本学术振兴会;
关键词
Linear friction welding; Fatigue strength; Weld toe radius; TUNGSTEN INERT-GAS; LOW-CYCLE; MECHANICAL-PROPERTIES; TI-6AL-4V; MICROSTRUCTURE; PARAMETERS; TENSILE; LASER; LIFE;
D O I
10.1016/j.jmapro.2023.08.004
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Although linear friction welding (LFW) has received significant attention as an effective solid-state welding method, the fatigue properties of LFW joints have not been fully investigated. In this study, the fatigue strength of the steel joints fabricated using LFW was investigated and improved by increasing the pressure after oscillation. Low-carbon steel SM490A was successfully joined using LFW without unbonded areas or apparent softening in the heat-affected zone (HAZ). The microhardness, microstructure, weld toe shape, and fatigue life were assessed to investigate their relationships with the pressure conditions after oscillation. The results indicated that increasing the pressure after oscillation improved the area fraction of martensite (M) and the hardness of the weld interface center. The weld toe radius (rho) and weld toe angle (alpha) also increased regardless of the upset control condition. The increasing of the pressure after oscillation from 50 MPa to 300 MPa increased rho from 0.4 mm to 2.1 mm and the alpha increased from 92.7 degrees to 103.4 degrees at the weld center, accompanied by a reduced stress concentration factor (Kt) from 3.0 to 1.7. Under the fatigue test conditions of the stress range of 380 MPa, the fatigue life of the LFW as-welded joints was increased by approximately 31 % when the pressure after oscillation was 250 MPa compared to that of 50 MPa and by 87 % when it was 300 MPa compared to that of 250 MPa. Despite the possibility of fracture initiation at the weld toe at the edge of the LFW joints, the fatigue strength demonstrated a substantially longer fatigue life than the S -N design curve FAT90 recommended by the International Institute of Welding.
引用
收藏
页码:795 / 805
页数:11
相关论文
共 50 条
  • [21] Study on strength properties of butt-welded joints with stainless and carbon steel
    Aramaki, S.
    Shimozato, T.
    Tai, M.
    Matsushita, H.
    Shimura, Y.
    BRIDGE MAINTENANCE, SAFETY, MANAGEMENT, LIFE-CYCLE SUSTAINABILITY AND INNOVATIONS, 2021, : 1301 - 1307
  • [22] Fatigue Strength Improvement of Lap Welded Joints by Low Transformation Temperature Welding Wire — Superior Improvement with Strength of Steel
    A. Ohta
    N. Suzuki
    Y. Maeda
    S. J. Maddox
    Welding in the World, 2003, 47 (3-4) : 38 - 43
  • [23] Fatigue strength of welded butt joints in thin and slender specimens
    Lillemae, Ingrit
    Lammi, Heikki
    Molter, Lars
    Remes, Heikki
    INTERNATIONAL JOURNAL OF FATIGUE, 2012, 44 : 98 - 106
  • [24] FATIGUE-STRENGTH OF VIBRATION WELDED THERMOPLASTIC BUTT JOINTS
    STOKES, VK
    POLYMER ENGINEERING AND SCIENCE, 1992, 32 (09): : 593 - 599
  • [25] Fatigue strength assessment of butt-welded joints with undercuts
    Steimbreger, Ceferino
    Chapetti, Mirco D.
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 105 : 296 - 304
  • [26] Fatigue strength of friction-welded joints of aluminum bronze to stainless steel
    Ochi, Hiizu
    Isshiki, Yoshihiro
    Kawai, Gosaku
    STRENGTH FRACTURE AND COMPLEXITY, 2020, 13 (02) : 81 - 90
  • [27] Fatigue Crack Growth on Flash Butt Welded and Laser Beam Welded Joints in a High-Strength Low-Alloy Steel
    Henrique Varella Ribeiro
    Milton Sérgio Fernandes Lima
    José Benedito Marcomini
    Filipe Corrêa Pinto
    Carlos Antonio Reis Pereira Baptista
    Journal of Materials Engineering and Performance, 2022, 31 : 7686 - 7694
  • [28] FATIGUE STRENGTH OF BUTT-WELDED JOINTS IN LOW-ALLOY STRUCTURAL STEELS
    FROST, NE
    DENTON, K
    BRITISH WELDING JOURNAL, 1967, 14 (04): : 157 - &
  • [29] Fatigue Crack Growth on Flash Butt Welded and Laser Beam Welded Joints in a High-Strength Low-Alloy Steel
    Ribeiro, Henrique Varella
    Lima, Milton Sergio Fernandes
    Marcomini, Jose Benedito
    Pinto, Filipe Correa
    Baptista, Carlos Antonio Reis Pereira
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (09) : 7686 - 7694
  • [30] Strength model for mismatched butt welded joints of high strength steel
    Sun, Fei-Fei
    Ran, Ming-Ming
    Li, Guo-Qiang
    Kanvinde, Amit
    Wang, Yan-Bo
    Xiao, Robert Y.
    JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2018, 150 : 514 - 527