Self-repairing and anti-fouling performance of anticorrosive coating in marine environment

被引:5
|
作者
Wu, Xiao [1 ]
Yang, Chao [2 ]
Wu, Lingli [3 ]
Zhang, Chuchu [4 ]
Cui, Gan [4 ]
Xin, Yanping [1 ]
机构
[1] Shandong Inst Petr & Chem Technol, Dongying 257061, Peoples R China
[2] SINOPEC, Technol Inspect Ctr Shengli Oilfield, Dongying 257000, Peoples R China
[3] China Petr Engn & Construct Corp Southwest Co, Engn Cost & Cost Control Ctr, Chengdu 610041, Peoples R China
[4] China Univ Petr East China, Coll Pipeline & Civil Engn, Qingdao 266580, Peoples R China
关键词
Double-walled microcapsules; Fluoropolymer; Anti-corrosion and anti-fouling coating; Marine environment; Electrochemical test; ISOCYANATE MICROCAPSULES; PICKERING EMULSION; MICROENCAPSULATION;
D O I
10.1016/j.polymertesting.2023.108090
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Microcrack damage repair and microbial contamination prevention are two major challenges for anti-corrosion coatings on the surfaces of underwater installations. In this study, water-triggered self-healing microcapsules were combined with low-surface-energy fluoropolymers to prepare a bifunctional anti-corrosion coating with underwater self-healing and bio-fouling properties. The results showed that the prepared microcapsules had good mechanical, thermal, and environmental stability, with an average diameter of 153 & mu;m and an encapsulation rate of 66.7%. When the microcapsule content in the coating was 8 wt%, the microcapsule dispersion performance and healing barrier effect of the composite coating were optimal, and the repair efficiency reached 81.6%. Furthermore, compared with the coating without microcapsules or graft fluoropolymers (PFG), the sample denoted as PFG18/4/IPDI-MC/ER showed the largest surface water contact angle and had the best protein inhibition rate of 87% when using bovine hemoglobin to detect the protein adsorption concentration on the coating surface.
引用
收藏
页数:18
相关论文
共 50 条
  • [21] Environmentally friendly marine anti-fouling additive
    Seabrook, S. G., Jr.
    Advanced Marine Materials, International Conference, 2006, : 29 - 32
  • [22] EIS study of a self-repairing microarc oxidation coating
    Wen, Lei
    Wang, Y. M.
    Liu, Yan
    Zhou, Y.
    Guo, L. X.
    Ouyang, J. H.
    Jia, D. C.
    CORROSION SCIENCE, 2011, 53 (02) : 618 - 623
  • [23] Self-repairing coating for corrosion protection of aluminum alloys
    He, Xiaodong
    Shi, Xianming
    PROGRESS IN ORGANIC COATINGS, 2009, 65 (01) : 37 - 43
  • [24] Application of graphene in anti-corrosive and anti-fouling coating
    Chen, Jian-Hua
    Li, Wen-Ge
    Zhao, Yuan-Tao
    Qian, Su-Ping
    Gerald, Odhiambo J.
    Surface Technology, 2019, 48 (06): : 89 - 97
  • [25] ANTI-FOULING OF COPPER-ALLOYS IN MARINE ENVIRONMENTS .2. EFFECTS OF ALLOYING ELEMENTS ON ANTI-FOULING
    IMAZU, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1984, 70 (13): : 1349 - 1349
  • [26] Rapid evaluation of anti-fouling coating materials for Limnopernafortunei
    State Key Laboratory of Hydroscience and Engineering, Tsinghua University, Beijing
    100084, China
    Qinghua Daxue Xuebao, 9 (957-963):
  • [27] Anti-fouling of marine organisms adhesion by zinc anode
    Ohba, T.
    Wusui, H.
    Kajiyama, T.
    Iwata, S.
    Kuwa, M.
    Zairyo to Kankyo/ Corrosion Engineering, 2001, 50 (06): : 279 - 284
  • [28] Preparation and Performance of Self-repairing Superhydrophobic Coating with Self-similar Double-layer Structure
    Lu Z.-Z.
    Tang C.
    Liang Y.
    Cai J.-H.
    Wei P.
    Surface Technology, 2022, 51 (02): : 392 - 401
  • [29] Self-repairing performance and formation mechanism of self-repairing layer of natural serpentine powder as a lubricating oil additive
    Gao, Fei
    Xu, Yi
    Xu, Bin-Shi
    Zhang, Bao-Sen
    Zhang, Bo
    Shi, Pei-Jing
    Mocaxue Xuebao/Tribology, 2011, 31 (05): : 431 - 438
  • [30] Preparation and healing property evaluation of self-repairing polymer coating
    Liao, L. P.
    Zhang, W.
    Zhao, Y.
    SURFACE ENGINEERING, 2014, 30 (02) : 138 - 141