Effect of post-annealing on the oxidation behavior of hot rolled ODS-FeCrAl steel in liquid lead

被引:3
|
作者
Du, Qian [1 ]
Chen, Jianye [1 ]
Yun, Di [1 ]
Gu, Long [2 ]
Long, Bin [3 ]
Lu, Chenyang [1 ]
Li, Yanfen [4 ]
Guo, Shaoqiang [1 ]
机构
[1] Xi An Jiao Tong Univ, Sch Nucl Sci & Technol, Shaanxi Key Lab Adv Nucl Energy & Technol, Xian 710049, Shaanxi, Peoples R China
[2] Lanzhou Univ, Sch Nucl Sci & Technol, Lanzhou 730000, Gansu, Peoples R China
[3] China Inst Atom Energy, Beijing 102413, Peoples R China
[4] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China
关键词
A; Steel; B; SEM; C; TEM; D; EBSD; E. High temperature oxidation; CORROSION BEHAVIOR; DIFFUSION; OXYGEN; MICROSTRUCTURE; EVOLUTION; ALLOYS; CR;
D O I
10.1016/j.corsci.2023.111815
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure of the hot-rolled and annealed ODS-FeCrAl steels and related oxide scales formed in the oxygen-containing liquid lead at 600 degree celsius was investigated by SEM-EDS, EBSD and TEM. The post-annealing caused partial recrystallization of hot-rolled ODS steel, which significantly reduced the intense theta-fiber (<001>||ND) and local dislocation density. After corrosion, the hot-rolled ODS steels exhibited complex and locally uneven oxide scales while the annealed ODS steels formed a uniform triple-layered oxide scale. A new insight into the relationship between oxidation depth and grain orientation was proposed, highlighting the significance of orientation-dependent dislocations on the transition of external/internal oxidation mechanisms.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Influence of continuous annealing on the interfacial compound evolution and mechanical behavior of hot-rolled titanium/steel composite plates
    Wei, Zhenxiong
    Huang, Peng
    Gao, Qiang
    Su, Xixi
    Feng, Zhanhao
    Peng, Lin
    Li, Jun
    Sun, Yonghui
    Zu, Guoyin
    MATERIALS & DESIGN, 2025, 253
  • [32] Effect of the annealing temperature on the mechanical properties, formability and corrosion resistance of hot-rolled duplex stainless steel
    Fargas, G.
    Anglada, M.
    Mateo, A.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (04) : 1770 - 1782
  • [33] Effect of annealing temperature on properties and second phase characteristics of 443 stainless steel hot-rolled sheets
    Sheng, Jie
    Man, Kun
    Ma, Guocai
    Meng, Yahui
    Li, Yufeng
    Gao, Yang
    Yang, Penghui
    Wei, Jiafu
    La, Peiqing
    FERROELECTRICS, 2024, 618 (13-14) : 2181 - 2195
  • [34] Effect of diffusion annealing on interface microstructure of hot rolled high boron alloyed stainless steel composite plate
    Liu, Jing
    Xie, Guo-Liang
    Zhang, Ke
    Han, Jing-Tao
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2013, 34 (04): : 90 - 94
  • [35] Effect of Coiling Temperature on Microstructure and Tensile Behavior of a Hot-Rolled Ferritic Lightweight Steel
    Junfeng Wang
    Qi Yang
    Xiaodong Wang
    Li Wang
    Metallurgical and Materials Transactions A, 2016, 47 : 5918 - 5931
  • [36] Effect of Coiling Temperature on Microstructure and Tensile Behavior of a Hot-Rolled Ferritic Lightweight Steel
    Wang, Junfeng
    Yang, Qi
    Wang, Xiaodong
    Wang, Li
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2016, 47A (12): : 5918 - 5931
  • [37] Effect of small amounts of Ni on liquid-Cu embrittlement in hot-rolled mild steel after high-temperature oxidation
    Electronics Engineering Labs., Sumitomo Metal Inds., Ltd., 1-8 Fuso-cho, Amagasaki 660-0891, Japan
    不详
    Oxid Met, 3 (177-194):
  • [38] Effect of Small Amounts of Ni on Liquid-Cu Embrittlement in Hot-Rolled Mild Steel After High-Temperature Oxidation
    Tomoki Fukagawa
    Hisao Fujikawa
    Oxidation of Metals, 1999, 52 : 177 - 194
  • [39] Effect of small amounts of Ni on liquid-Cu embrittlement in hot-rolled mild steel after high-temperature oxidation
    Fukagawa, T
    Fujikawa, H
    OXIDATION OF METALS, 1999, 52 (3-4): : 177 - 194
  • [40] Corrosion behavior of 9Cr-ODS steel in stagnant liquid lithium and lead-lithium at 873 K
    Li, Yanfen
    Abe, Hiroaki
    Nagasaka, Takuya
    Muroga, Takeo
    Kondo, Masatoshi
    JOURNAL OF NUCLEAR MATERIALS, 2013, 443 (1-3) : 200 - 206