Mechanical properties of hot-pressed VB2-SiC composites with and without WC

被引:0
|
作者
Guo, Shuqi [1 ]
Okuma, Gaku [1 ]
Naito, Kimiyoshi [1 ]
Kakisawa, Hideki [1 ]
机构
[1] Natl Inst Mat Sci, Res Ctr Struct Mat, 1-2-1 Sengen, Tsukuba, Ibaraki 3050047, Japan
关键词
Vanadium diboride; SiC; WC; Mechanical properties; HIGH-TEMPERATURE STRENGTH; SILICON-NITRIDE CERAMICS; ZRB2; GRAIN-BOUNDARIES; ZIRCONIUM DIBORIDE; ZRB2-BASED COMPOSITES; OXIDATION RESISTANCE; HFB2-SIC COMPOSITE; TUNGSTEN CARBIDE; CREEP-BEHAVIOR; MICROSTRUCTURE;
D O I
10.1016/j.ceramint.2023.08.210
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, VB2-20 vol% SiC composites with and without 5 vol% WC were prepared via hot-pressing at 1800 degrees C for dwell time of 1 h under 20 MPa in Ar. Relative densities of >96% were obtained for the two compositions composites. The mechanical properties of the resulting composites were evaluated at the temperatures ranging from room temperature to 1400 degrees C. The results show that the temperature dependence of the mechanical properties was strongly related to the addition of WC. For VB2-SiC composite without WC, a maximum strength of 585 +/- 55 MPa was obtained at 1000 degrees C, then the strength decreased to 236 +/- 11 MPa at 1400 degrees C, with substantially degradation of strength accompanying increase of temperature. For VB2-SiC-WC composite, on the other hand, the addition of WC enhanced high-temperature strength up to 1400 degrees C, with strengths in the range of 464-523 MPa. The strength was higher at elevated temperature than at room temperature; and a maximum strength of 523 +/- 27 MPa was obtained at 1200 degrees C. In addition, although at or below 1000 degrees C the strength was lower for VB2-SiC-WC than for VB2-SiC, above 1000 degrees C the strength was significantly higher for the former than for the latter.
引用
收藏
页码:35368 / 35376
页数:9
相关论文
共 50 条
  • [31] Effects of boron content on the microstructures and mechanical properties of reactive hot-pressed BxC-TiB2-SiC composites
    He, Qianglong
    Xie, Jingjing
    Wang, Aiyang
    Liu, Chun
    Tian, Tian
    Hu, Lanxin
    Yi, Chenhong
    Zhang, Zhixiao
    Wang, Hao
    Wang, Weimin
    Fu, Zhengyi
    CERAMICS INTERNATIONAL, 2019, 45 (16) : 19650 - 19657
  • [32] The influence of different SiC amounts on the microstructure, densification, and mechanical properties of hot-pressed Al2O3-SiC composites
    Akbari, Elaheh
    Kakroudi, Mahdi Ghassemi
    Shahedifar, Vahideh
    Ghiasi, Hanieh
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2020, 17 (02) : 491 - 500
  • [33] Role of h-BN content on microstructure and mechanical properties of hot-pressed ZrB2-SiC composites
    Vafa, Nasser Pourmohammadie
    Kakroudi, Mahdi Ghassemi
    Asl, Mehdi Shahedi
    CERAMICS INTERNATIONAL, 2020, 46 (13) : 21533 - 21541
  • [34] Microstructures and mechanical properties of hot-pressed MoSi2-matrix composites reinforced with SiC and ZrO2 particles
    Ma, Q
    Yang, YQ
    Kang, MK
    Xue, QJ
    COMPOSITES SCIENCE AND TECHNOLOGY, 2001, 61 (07) : 963 - 969
  • [35] Hot-pressed hydroxylapatite/monoclinic zirconia composites with improved mechanical properties
    Zafer Evis
    Robert H. Doremus
    Journal of Materials Science, 2007, 42 : 2426 - 2431
  • [36] Microstructure and mechanical properties of hot-pressed WC-MgO composites with Cr3C2 or VC addition
    Ouyang, Chenxin
    Zhu, Shigen
    Dong, Weiwei
    Qu, Haixia
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2013, 41 : 41 - 47
  • [37] MECHANICAL-PROPERTIES OF HOT-PRESSED ALUMINA-SIALON COMPOSITES
    TAKATORI, K
    KAMIGAITO, O
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1988, 7 (10) : 1024 - 1026
  • [38] Hot-pressed hydroxylapatite/monoclinic zirconia composites with improved mechanical properties
    Evis, Zafer
    Doremus, Robert H.
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (07) : 2426 - 2431
  • [39] Mechanical properties and microstructures of hot-pressed MgAlON-BN composites
    Zhang, Zuotai
    Teng, Lidong
    Li, Wenchao
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (01) : 319 - 326
  • [40] PROPERTIES OF HOT-PRESSED SIC MATRIX COMPOSITES WITH INTERNALLY-SYNTHESIZED TIB2
    TANI, T
    WADA, S
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1989, 97 (10): : 1195 - 1198