The effects of V or Sn addition on the microstructural characteristics and mechanical properties of Nb-16Si-22Ti-2Al-2Cr alloy

被引:1
|
作者
Li, Zhaobo [1 ]
Luo, Liangshun [1 ]
Wang, Binbin [1 ]
Su, Baoxian [1 ]
Luo, Lei [2 ]
Wang, Liang [1 ]
Su, Yanqing [1 ]
Guo, Jingjie [1 ]
Fu, Hengzhi [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
[2] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, Nanjing 210016, Peoples R China
基金
中国国家自然科学基金;
关键词
Alloying; Fracture toughness; Compressive strength; Crystallographic orientation relationship; FRACTURE-TOUGHNESS; OXIDATION RESISTANCE; NB; PHASE; EVOLUTION; TI; STRENGTH; CR; DEFORMATION; BEHAVIOR;
D O I
10.1016/j.ijrmhm.2024.106606
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructural characteristics and mechanical properties of as-cast Nb-16Si-22Ti-2Al-2Cr-xV (x = 2, 5, 10, 15 and 20 at.%) and Nb-16Si-22Ti-2Al-2Cr-ySn (y = 1, 3, 5 and 7 at.%) alloys are systematically investigated in this study. The individual addition of V or Sn obviously promotes the eutectoid decomposition of metastable phase (Nb3Si). All alloys consist of the primary Nb5Si3 and the eutectic Nbss/Nb5Si3 structures. For the V-added alloys, the low content of added V (2 at.%) cannot change the constituent phases (Nbss and alpha-Nb5Si3) of Nb-16Si-22Ti2Al-2Cr alloy. However, the other V-added alloys consist of the primary beta-Nb5Si3 and the eutectic structures of Nbss/beta-Nb5Si3. Similarly, addition of 1 at.% Sn also cannot affect the constituent phases of Nb-16Si-22Ti-2Al-2Cr alloy, while the beta-Nb5Si3 and Nb3Sn are formed with the increase in Sn content. Moreover, the addition of V or Sn promotes the formation of chaotic eutectics and suppresses the appearance of reticulate and cellular eutectics. The fracture toughness of the alloys is continuously elevated by the V addition, while it gets weakened when the content of added Sn exceeds 1 at.%. The high-temperature compressive strength of the V-added alloys increases when the V content is below 10 at.%, and then it decreases with increasing V content. The Sn-added alloys, except 3Sn alloy, exhibit higher compressive strength than Nb-16Si-22Ti-2Al-2Cr alloy, due to the increase in volume fractions of brittle phases (beta-Nb5Si3 and Nb3Sn). Moreover, the crystallographic orientation relationships among the constituent phases are also explored before and after high-temperature compression.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] Effects of minor boron addition on phase transformation and properties of Ti-47.5Al-2Cr-2Nb alloy
    Li, ZX
    Cao, CC
    INTERMETALLICS, 2005, 13 (3-4) : 251 - 256
  • [22] Microstructural characteristics of Ti-48Al-2Cr alloy
    J. Zhang
    L. He
    Y. Cui
    H. Ye
    Journal of Materials Engineering and Performance, 2001, 10 : 378 - 389
  • [23] Effects of Ball Milling Time and Sintering Temperature on Microstructure and Room-Temperature Mechanical Properties of Nb-16Si-22Ti-2Al-2Hf-2Cr Alloy Synthesized by Powder Metallurgy
    Fu Yongming
    Liu Wei
    Zong Wei
    Sha Jiangbo
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (02) : 400 - 404
  • [24] Microstructural characteristics of Ti-48Al-2Cr alloy
    Zhang, J
    He, L
    Cui, Y
    Ye, H
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2001, 10 (03) : 378 - 389
  • [25] Effects of Zr and Y on the Mechanical Properties and the Microstructure of Ti-Al-Sn-Nb-Mo-Si Alloy
    Qin Kuiqing Wang Lida Tang Shisheng General Research Institute for Non-ferrous metals
    Rare Metals, 1990, (01) : 39 - 45
  • [26] Hot Workability of Nb-16Si-22Ti-2Cr-2Al-2Hf-xFe Alloys
    Chu Chu
    Xu Yanjin
    Hou Hongliang
    Luo Liangshun
    Su Yanqing
    Guo Jingjie
    Fu Hengzhi
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (05) : 1481 - 1487
  • [27] Hot Workability of Nb-16Si-22Ti-2Cr-2Al-2Hf-xFe Alloys
    Chu, Chu
    Xu, Yanjin
    Hou, Hongliang
    Luo, Liangshun
    Su, Yanqing
    Guo, Jingjie
    Fu, Hengzhi
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (05): : 1481 - 1487
  • [28] Transformations in the Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) alloy and mechanical and microstructural characteristics
    Tarin, P.
    Fernandez, A. L.
    Simon, A. G.
    Badia, J. M.
    Piris, N. M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 438 (SPEC. ISS.): : 364 - 368
  • [29] Microstructure and Mechanical Properties of Nb-20Ti-16Al Alloy with Carbon Addition
    Yu C.
    Xiao L.
    Zhao X.
    Liu J.
    Guo L.
    Cai Z.
    Xiyou Jinshu/Chinese Journal of Rare Metals, 2017, 41 (09): : 980 - 984
  • [30] EFFECTS OF COOLING RATE AND POURING TEMPERATURE ON MICROSTRUCTURE AND FRACTURE TOUGHNESS OF THE INDUCTION MELTED Nb-16Si-22Ti-2Hf-2Cr-2Al ALLOY
    Jia, Lina
    Ge, Jingru
    Sha, Jiangbo
    Zhang, Hu
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2010, 24 (15-16): : 2946 - 2951