Enhancing the wear and high-temperature oxidation behavior of NiCrBSi coatings by collaboratively adding WC and Cr3C2

被引:9
|
作者
Sun, Xingfu [1 ,2 ]
Li, Fangyi [1 ,2 ]
Li, Yanle [1 ,2 ]
Du, Jiyu [3 ]
Qi, Xiaoxia [1 ,2 ]
Cui, Weiqiang [1 ,2 ]
Niu, Jiating [1 ,2 ]
机构
[1] Shandong Univ, Sch Mech Engn, Key Lab High Efficiency & Clean Mech Manufacture, Minist Educ, Jinan 250061, Peoples R China
[2] Shandong Univ, Natl Demonstrat Ctr Expt Mech Engn Educ, Jinan 250061, Peoples R China
[3] Shandong Jianzhu Univ, Jinan 250101, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Thermal spraying; Composite coatings; Microstructure; High-temperature wear resistance; High-temperature oxidation; ALLOY COMPOSITE COATINGS; NI-BASED ALLOY; MICROSTRUCTURE; PLASMA; HVOF; PERFORMANCE; HARDNESS;
D O I
10.1016/j.surfcoat.2023.129968
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A composite coating was deposited by collaborative modification with tungsten carbide (WC) and Cr3C2 ceramic particles to improve the wear resistance of NiCrBSi coating over a wide temperature range. The original NiCrBSi coating and the composite coatings with WC and Cr3C2 collaboratively (NiCrBSi +20 wt% WC-Cr3C2-Ni) and exclusively (NiCrBSi +20 wt% WC and NiCrBSi +20 wt% Cr3C2-NiCr) added were designed and deposited by plasma spraying. The microhardness of the composite coatings added with the ceramic phase was higher than that of the NiCrBSi coating. The composite coating with the addition of WC showed the maximum microhardness (896.8 HV). The wear mechanism of the four coatings at room temperature was dominated by fatigue spalling, whereas oxidative and abrasive wear prevailed at 700 degrees C. The composite coating (NiCrBSi +20 wt% WC-Cr3C2-Ni) showed excellent abrasion resistance at room temperature and 700 degrees C. The wear volume of the composite coating (NiCrBSi +20 wt% WC-Cr3C2-Ni) decreased by 83.5 % and 46.9 % at room temperature and 700 degrees C, respectively, compared with the wear volume of the NiCrBSi coating. In general, high WC hardness was favorable for improving the microhardness of the coating. The preferential oxidation of Cr3C2 instead of WC promoted the formation of a dense oxide film on the surface of the coating and reduced oxidation within the coating. This study revealed the mechanism of the collaborative enhancement of NiCrBSi coatings by WC and Cr3C2 and the improved wear resistance of the NiCrBSi coatings at room and high temperatures.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] High-temperature oxidation and wear resistance of WC-Co based coatings with WB addition
    Yan, Xifeng
    Wang, Haibin
    Liu, Xuemei
    Hou, Chao
    Qiu, Qingfan
    Song, Xiaoyan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (10) : 3023 - 3034
  • [32] High temperature wear performance of HVOF-sprayed Cr3C2-WC-NiCoCrMo and Cr3C2-NiCr hardmetal coatings
    Zhou, Wuxi
    Zhou, Kesong
    Li, Yuxi
    Deng, Chunming
    Zeng, Keli
    APPLIED SURFACE SCIENCE, 2017, 416 : 33 - 44
  • [33] The High-Temperature Wear and Oxidation Behavior of CrC-Based HVOF Coatings
    Houdkova, Sarka
    Cesanek, Zdenek
    Smazalova, Eva
    Lukac, Frantisek
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2018, 27 (1-2) : 179 - 195
  • [34] The High-Temperature Wear and Oxidation Behavior of CrC-Based HVOF Coatings
    Šárka Houdková
    Zdeněk Česánek
    Eva Smazalová
    František Lukáč
    Journal of Thermal Spray Technology, 2018, 27 : 179 - 195
  • [35] The study of Cr3C2-25NiCr and 35WC-Co/65NiCrBSi-based HVOF coatings for high-temperature erosion resistance application
    Naik, K. Raghavendra
    Kumar, R. K.
    Saravanan, V
    Seetharamu, S.
    Sampathkumaran, P.
    TRIBOLOGY-MATERIALS SURFACES & INTERFACES, 2022, 16 (01) : 10 - 22
  • [36] Sliding Wear Behavior of HVOF-sprayed Cr3C2–NiCr/CeO2 Composite Coatings at Elevated Temperature up to 800 °C
    Bin Yin
    Guang Liu
    Huidi Zhou
    Jianmin Chen
    Fengyuan Yan
    Tribology Letters, 2010, 37 : 463 - 475
  • [37] Phase Transformation-Induced Improvement in Hardness and High-Temperature Wear Resistance of Plasma-Sprayed and Remelted NiCrBSi/WC Coatings
    Sha, Jin
    Chen, Liang-Yu
    Liu, Yi-Tong
    Yao, Zeng-Jian
    Lu, Sheng
    Wang, Ze-Xin
    Zang, Qian-Hao
    Mao, Shu-Hua
    Zhang, Lai-Chang
    METALS, 2020, 10 (12) : 1 - 15
  • [38] Wear, erosion and corrosion resistance of HVOF-sprayed WC and Cr3C2 based coatings for electrolytic hard chrome replacement
    Wang, Qun
    Luo, Sisi
    Wang, Shaoyi
    Wang, Hui
    Ramachandran, Chidambaram Seshadri
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2019, 81 : 242 - 252
  • [39] Interaction of WC and Cr3C2 Carbides at Heat Treatment of WC-Cr3C2-Cu Alloys
    Bodrova, L. E.
    Goida, E. Yu
    Melchakov, S. Yu
    Shubin, A. B.
    Fedorova, O. M.
    INORGANIC MATERIALS-APPLIED RESEARCH, 2022, 13 (02) : 560 - 568
  • [40] Effects of Cr3C2 content and temperature on sliding friction and wear behaviors of Cr3C2/Ni3Al composite materials
    Fu, Lihua
    Han, Wei
    Zhao, Lin
    Gong, Karin
    Bengtsson, Sven
    Zhou, Meng
    Li, Changhai
    Tian, Zhiling
    WEAR, 2018, 414 : 163 - 173