Processing of ZrB2 tribo-ceramics by reactive spark plasma sintering of ZrH2+2B subjected to high-energy pre-ball-milling
被引:4
|作者:
Lopez-Arenal, Jesus
[1
]
Moshtaghioun, Bibi Malmal
[1
]
Gomez-Garcia, Diego
[1
]
Ortiz, Angel L.
[2
]
机构:
[1] Univ Seville, Dept Fis Mat Condensada, Seville 41080, Spain
[2] Univ Extremadura, Dept Ingn Mecan Energet & Mat, Badajoz 06006, Spain
关键词:
ZrB2;
Reactive spark plasma sintering;
High-energy ball-milling;
Tribo-ceramics;
Sliding wear;
HIGH-TEMPERATURE CERAMICS;
SLIDING-WEAR RESISTANCE;
ABRASIVE WEAR;
TRIBOLOGICAL PROPERTIES;
ZIRCONIUM DIBORIDE;
B4C CERAMICS;
COMPOSITES;
KINETICS;
DRY;
FABRICATION;
D O I:
10.1016/j.jeurceramsoc.2023.04.047
中图分类号:
TQ174 [陶瓷工业];
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
The reactive spark plasma sintering (RSPS) of monolithic ZrB2 ceramics from ZrH2+2B powder mixtures subjected to shaker pre-milling was investigated, and compared with other three sintering approaches. It was found that RSPS is optimal at 1850 degrees C, which results in fully-dense ZrB2 ceramics with similar to 20 GPa hardness. Comparatively, at 1850 degrees C RSPS from the simply-mixed ZrH2+2B powder mixture, SPS from the commercial ZrB2 powder, and SPS from the shaker-milled ZrB2 powder result in non-dense (76.7-86.7%) and softer (6.0-11.8 GPa) ZrB2 ceramics. Furthermore, the optimally RSPS-ed ZrB2 ceramic was subjected to unlubricated sliding-wear tests against diamond under 40 N load for 1000 m of sliding, demonstrating that it is a promising tribo-ceramic that only undergoes mild tribo-oxidative wear at 10(-8) mm(3)/(N.m) in the form of a slight plasticity-dominated two-body abrasion with eventual formation and partial loss of a self-lubricating and protective oxide tribolayer.