Durability of Resin Bonding to Dental 3Y-TZP Zirconia Using Different Adhesive Systems

被引:1
|
作者
Yazigi, Christine [1 ]
Alawi, Shila [1 ]
Wille, Sebastian [1 ]
Lehmann, Frank [1 ]
Kern, Matthias [1 ]
机构
[1] Christian Albrechts Univ Kiel, Sch Dent, Dept Prosthodont Propaedeut & Dent Mat, D-24105 Kiel, Germany
关键词
adhesive bonding; luting resins; MDP; primer; zirconia ceramic; self-adhesive luting resin; conventional luting resin; PREPARATION DESIGNS; CERAMIC INLAYS; STRENGTH; CEMENTS; COMPOSITE; RESTORATIONS; TOOTH; SHEAR; SURVIVAL; PRIMERS;
D O I
10.3390/ma17020424
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This laboratory study was conducted to evaluate and compare the resin bond strength of different adhesive resin systems in different combinations and the durability of their bonds with zirconia ceramic. Materials and methods: One hundred and twenty-eight specimens were milled from 3Y-TZP zirconia ceramic. The bonding surfaces of all disks were wet polished, steam cleaned, airborne-particle abraded and ultrasonically cleaned in 99% isopropanol. The specimens were randomly divided into four main groups according to the applied resin system; two conventional and two self-adhesive systems were used. Each group was further subdivided into two subgroups; the first was conditioned with the specified primer for conventional luting resins or not conditioned for the self-adhesive systems, whereas the second subgroup of each was conditioned with the same phosphate monomer-containing primer (Alloy Primer). The zirconia specimens were adhesively bonded, using the allocated luting resin, to plexiglass tubes filled with self-curing composite resin (Clearfil FII). Half of the specimens of each subgroup were stored in distilled water at 37 degrees C for 3 days, whereas the other half were subjected to artificial aging, 150 days of storage and additional thermal cycling. Thereafter, all specimens were subjected to TBS testing using a universal testing machine. Statistical analysis was conducted using two-way ANOVA followed by separate one-way ANOVAs. The Games-Howell post-hoc test was applied for pairwise comparisons. Results: All specimens survived storage with thermal cycling. The mean TBS values ranged from a minimum of 43.4 +/- 5.0 MPa to a maximum of 66.4 +/- 3.5 after 3 days and from a minimum of 13.6 +/- 2.5 MPa to a maximum of 50.1 +/- 9.4 MPa after 150 days. Conclusions: Artificial aging had a significantly negative effect on all test groups. The chosen adhesive-resin system had a significant effect on the resulting TBS values. The highest TBS values were achieved for the self-adhesive luting resin G-Cem One but were statistically comparable to the results obtained for the dual-cure luting resin G-Cem LinkForce.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Cavity growth simulation for superplastic deformation of tetragonal zirconia polycrystal, 3Y-TZP
    Harjo, S.
    Kojima, N.
    Motohashi, Y.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2008, 39 (4-5) : 358 - 362
  • [32] Effects of Aging on the Mechanical Properties of Dental Pigmented 3Y-TZP Ceramics
    Yi, Yuanfu
    Wen, Ning
    Bin, Den
    Shao, Longquan
    Wang, Chen
    Tian, Jiemo
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 136 - +
  • [33] TEMPERATURE EFFECT ON THERMAL CHANGES AND PHASE ANALYSIS OF 3Y-TZP ZIRCONIA RESTORATIONS
    Mordanov, O. S.
    Khabadze, Z. S.
    Nazarova, D. A.
    Shilyaeva, E. S.
    Kotelnikova, A. P.
    Mordanova, A., V
    NEW ARMENIAN MEDICAL JOURNAL, 2022, 16 (01): : 64 - 69
  • [34] Analysis of the stability of 3Y-TZP zirconia abutments after thermocycling and mechanical loading
    Almeida, Paulo J.
    Silva, Cesar L.
    Alves, Jorge L.
    Silva, Filipe S.
    Martins, Ramiro C.
    Sampaio-Fernandes, Joao
    REVISTA PORTUGUESA DE ESTOMATOLOGIA MEDICINA DENTARIA E CIRURGIA MAXILOFACIAL, 2016, 57 (04): : 197 - 206
  • [35] Stability of 3Y-TZP nano zirconia powder after hydrothermal ageing treatment
    Ahmed, Shafique
    Zou, Lifong
    Yan, Haixue
    ADVANCES IN APPLIED CERAMICS, 2022, 121 (5-8) : 159 - 165
  • [36] Biaxial flexural strength of 3D-printed 3Y-TZP zirconia using a novel ceramic printer
    Zenthoefer, Andreas
    Ilani, Ali
    Schmitt, Clemens
    Rammelsberg, Peter
    Hetzler, Sebastian
    Rues, Stefan
    CLINICAL ORAL INVESTIGATIONS, 2024, 28 (02)
  • [37] Effect of heat treatment of dental zirconia ceramic treated with three different primers on the bonding durability of resin cement
    Jung-Yun Ha
    Jun Sik Son
    Young Kyung Kim
    Kyo-Han Kim
    Tae-Yub Kwon
    Macromolecular Research, 2013, 21 : 71 - 77
  • [38] Association of Different Primers and Resin Cements for Adhesive Bonding to Zirconia Ceramics
    Maeda, Fernando Akio
    Bello-Silva, Marina Stella
    Eduardo, Carlos de Paula
    Miranda Junior, Walter Gomes
    Cesar, Paulo Francisco
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (03): : 261 - 265
  • [39] Effect of heat treatment of dental zirconia ceramic treated with three different primers on the bonding durability of resin cement
    Ha, Jung-Yun
    Son, Jun Sik
    Kim, Young Kyung
    Kim, Kyo-Han
    Kwon, Tae-Yub
    MACROMOLECULAR RESEARCH, 2013, 21 (01) : 71 - 77
  • [40] In vivo ageing of zirconia dental ceramics - Part II: Highly-translucent and rapid-sintered 3Y-TZP
    Cotic, Jasna
    Kocjan, Andraz
    Panchevska, Sanja
    Kosmac, Tomaz
    Jevnikar, Peter
    DENTAL MATERIALS, 2021, 37 (03) : 454 - 463