Features of Helium and Tritium Release from Li2TiO3 Ceramic Pebbles under Neutron Irradiation

被引:3
|
作者
Kulsartov, Timur [1 ,2 ,3 ]
Zaurbekova, Zhanna [2 ,4 ]
Chikhray, Yevgen [2 ,3 ]
Kenzhina, Inesh [1 ,2 ,5 ,6 ]
Askerbekov, Saulet [2 ,3 ]
Shaimerdenov, Asset [5 ]
Akhanov, Assyl [5 ]
Aitkulov, Magzhan [5 ]
Begentayev, Meiram [1 ]
机构
[1] Satbayev Univ, 22 Satbayev Str, Alma Ata 050013, Kazakhstan
[2] Inst Appl Sci & Informat Technol, 280 Bayzakov Str, Alma Ata 050040, Kazakhstan
[3] Al Farabi Kazakh Natl Univ, Inst Expt & Theoret Phys, 71-23 Al Farabi Ave, Alma Ata 050040, Kazakhstan
[4] Al Farabi Kazakh Natl Univ, 71-23 Al Farabi Ave, Alma Ata 050040, Kazakhstan
[5] Inst Nucl Phys, 1 Ibragimov Str, Alma Ata 050032, Kazakhstan
[6] Kazakh British Tech Univ, 59 Tole Bi, Alma Ata 050000, Kazakhstan
关键词
lithium ceramics; helium; tritium; neutron irradiation; desorption; DEFECTS;
D O I
10.3390/ma16175903
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The operation of fusion reactors is based on the reaction that occurs when two heavy hydrogen isotopes, deuterium and tritium, combine to form helium and a neutron with an energy of 14.1 MeV D + T ? He + n. For this reaction to occur, it is necessary to produce tritium in the facility itself, as tritium is not common in nature. The generation of tritium in the facility is a key function of the breeder blanket. During the operation of a D-T fusion reactor, high-energy tritium is generated as a result of the Li-6(n,a)T reaction in a lithium-containing ceramic material in the breeder blanket. Lithium metatitanate Li2TiO3 is proposed as one of the promising materials for use in the solid breeder blanket of the DEMO reactor. Several concepts for test blanket modules based on lithium ceramics are being developed for testing at the ITER reactor. Lithium metatitanate Li2TiO has good tritium release parameters, as well as good thermal and thermomechanical characteristics. The most important property of lithium ceramics Li2TiO is its ability to withstand exposure to long-term high-energy radiation at high temperatures and across large temperature gradients. Its inherent thermal stability and chemical inertness are significant advantages in terms of safety concerns. This study was a continuation of research regarding tritium and helium release from lithium metatitanate Li(2)TiO3 with 96% Li-6 during irradiation at the WWR-K research reactor using the vacuum extraction method. As a result of the analysis of experiments regarding the irradiation of lithium metatitanate in vacuum conditions, it has been established that, during irradiation, peak releases of helium from closed pores of the ceramics are observed, which open during the first 7 days of irradiation. The authors assumed that the reasons samples crack are temperature gradients over the ceramic sample, resulting from the internal heating of pebbles under the conditions of their vacuum evacuation, and contact with the bottom of the evacuated capsule. The temperature dependence of the effective diffusion coefficient of tritium in ceramics at the end of irradiation and the parameters of helium effusion were also determined.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Effect of surface water on tritium release behavior from Li2TiO3
    Hanada, T.
    Nishikawa, M.
    Kanazawa, T.
    Yamasaki, H.
    Yamashita, N.
    Fukada, S.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 417 (1-3) : 735 - 738
  • [32] Fabrication of Li2TiO3 ceramic pebbles with fine microstructure by microwave sintering
    Yang, Mao
    Wang, Hailiang
    Dang, Chen
    Huang, Zhangyi
    Ran, Guangming
    Chen, Xiaojun
    Lu, Tiecheng
    Xiao, Chengjian
    JOURNAL OF NUCLEAR MATERIALS, 2018, 509 : 330 - 334
  • [33] Tritium and helium release from neutron irradiated beryllium pebbles from the EXOTIC-8 irradiation
    Scaffidi-Argentina, F
    FUSION ENGINEERING AND DESIGN, 2001, 58-59 : 641 - 645
  • [34] Fabrication and Characterization of Li2TiO3–Li4SiO4 Pebbles for Tritium Breeder
    Maoqiao Xiang
    Yingchun Zhang
    Yun Zhang
    Shuya Liu
    Hui Liu
    Chaofu Wang
    Journal of Fusion Energy, 2015, 34 : 1341 - 1347
  • [35] In situ tritium recovery behavior from Li2TiO3 pebble bed under neutron pulse operation
    Tsuchiya, K
    Kikukawa, A
    Hoshino, T
    Nakamichi, M
    Yamada, H
    Yamaki, D
    Enoeda, M
    Ishitsuka, E
    Kawamura, H
    Ito, H
    Hayashi, K
    JOURNAL OF NUCLEAR MATERIALS, 2004, 329 : 1248 - 1251
  • [36] Influence of Lithium Mass Transfer on Tritium Behavior in Pebbles of Li2TiO3 with Excess Lithium
    Katayama, Kazunari
    Ipponsugi, Akito
    Hoshino, Tsuyoshi
    FUSION ENGINEERING AND DESIGN, 2020, 161
  • [37] Preparation of tritium breeding Li2TiO3 ceramic pebbles via newly developed piezoelectric micro-droplet jetting
    Cai, Jili
    Xu, Gaoyong
    Lu, Hui
    Xu, Chenguang
    Hu, Yifei
    Cai, Chao
    Suo, Jinping
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2022, 105 (06) : 3753 - 3764
  • [38] Surface inventory of tritium on Li2TiO3
    Kawagoe, T
    Nishikawa, M
    Baba, A
    Beloglazov, S
    JOURNAL OF NUCLEAR MATERIALS, 2001, 297 (01) : 27 - 34
  • [39] Tritium inventory in Li2TiO3 blanket
    Hashimoto, K
    Nishikawa, M
    Nakashima, N
    Beloglazov, S
    Enoeda, M
    FUSION ENGINEERING AND DESIGN, 2002, 61-62 : 375 - 381
  • [40] Tritium diffusivity in crystal grain of Li2TiO3 and tritium release behavior under several purge gas conditions
    Kinjyo, T.
    Nishikawa, M.
    Enoeda, M.
    Fukada, S.
    FUSION ENGINEERING AND DESIGN, 2008, 83 (04) : 580 - 587