Preparation of ultrafine Sm2Fe17N3 magnetic powders without ball milling

被引:3
|
作者
Wang, Jing [1 ]
Cai, Wei [1 ]
Zheng, Jingwu [1 ]
Zhu, Junhui [1 ]
Zhang, Xinqi [1 ]
Chen, Haibo [1 ]
Qiao, Liang [1 ]
Ying, Yao [1 ]
Li, Wangchang [1 ]
Yu, Jing [1 ]
Li, Juan [1 ]
Su, Yuebin [2 ]
Che, Shenglei [1 ]
机构
[1] Zhejiang Univ Technol, Coll Mat Sci & Engn, Res Ctr Magnet & Elect Mat, Hangzhou 310014, Peoples R China
[2] Zhejiang Haoxiang Min Co Ltd, Lishui 323900, Peoples R China
基金
中国国家自然科学基金;
关键词
Ultrafine powders; CaO coating; Ultrasonic spray pyrolysis; FINE POWDER; COERCIVITY; PARTICLES; SIZE;
D O I
10.1016/j.jmrt.2023.11.144
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ultrafine Sm2Fe17N3 powders obtained via ball or airflow milling usually exhibit defects and localized demag-netization owing to their irregular morphologies. Therefore, this study employs the ultrasonic spray pyroly-sis-reduction diffusion method in conjunction with CaO coating to control the precursor size of the oxides and obtain a size-controllable nearly spherical micronano-sized pure-phase Sm2Fe17N3 magnetic powder. The investigation involved testing and analyzing the microstructure, phase composition, and magnetic properties of the magnetic powder. The results indicate that the influence of hydrogen reduction after calcium oxide coating is crucial for achieving morphology control, and the amount of calcium oxide coating can regulate the size and morphology of the powder; excessive coating can hinder the subsequent calcium reduction and nitriding pro -cesses. By using 40 wt% Ca(NO3)2 to coat the composite oxide obtained via ultrasonic spray pyrolysis and by adjusting the reduction diffusion time, further particle refinement can be achieved, ultimately resulting in a nearly spherical strontium iron nitride magnetic powder with a D50 of 0.52 mu m. The coercivity of this magnetic powder reaches 9.13 kOe, and the maximum energy product is 27.83 MGOe. This study provides new methods and avenues to address the issues of magnetic powder sintering growth and improve magnetic performance. It also lays the foundation for the further enhancement of the performance of Sm2Fe17N3 magnets.
引用
收藏
页码:6688 / 6695
页数:8
相关论文
共 50 条
  • [21] Magnetic hardening of Sm2Fe17N3 by radiation damage
    Dempsey, NM
    Ghidini, M
    Nozières, JP
    Smith, PAI
    Gervais, B
    Coey, JMD
    PHYSICAL REVIEW LETTERS, 1998, 81 (25) : 5652 - 5655
  • [22] Domain wall pinning by radiation damage in Sm2Fe17N3 powders
    Dempsey, NM
    Nozieres, JP
    Rao, XL
    Ghidini, M
    Gervais, B
    Coey, JMD
    MAGNETIC HYSTERESIS IN NOVEL MAGNETIC MATERIALS, 1997, 338 : 645 - 649
  • [23] DEPENDENCE OF COERCIVITY ON PARTICLE-SIZE IN SM2FE17N3 POWDERS
    KOBAYASHI, K
    SKOMSKI, R
    COEY, JMD
    JOURNAL OF ALLOYS AND COMPOUNDS, 1995, 222 : 1 - 7
  • [24] Magnetic coupling of the composite mixtures Sm2Co17/Sm2Fe17N3 and Sm2Co17/Fe
    OSullivan, J
    Rao, XL
    Coey, JMD
    JOURNAL OF APPLIED PHYSICS, 1997, 81 (08) : 5124 - 5126
  • [26] Anisotropic Sm2Fe17N3 sintered magnets without coercivity deterioration
    Soda, Rikio
    Takagi, Kenta
    Jinno, Miho
    Yamaguchi, Wataru
    Ozaki, Kimihiro
    AIP ADVANCES, 2016, 6 (11):
  • [27] Effects of nonmagnetic overlay metals on coercivity of Sm2Fe17N3 magnet powders
    Yamaguchi, Wataru
    Takagi, Kenta
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2020, 516
  • [28] Magnetization reversal in Sm2Fe17N3 particles
    Cent Natl de la Recherche, Scientifique, Grenoble, France
    J Magn Magn Mater, (97-98):
  • [29] Hard magnetic Sm2Fe17N3 flakes nitrogenized at lower temperature
    Zhao, Lixin
    Akdogan, Nilay G.
    Hadjipanayis, George C.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 554 : 147 - 149
  • [30] Magnetisation reversal in Sm2Fe17N3 particles
    Kobayashi, K
    Givord, D
    Coey, JMD
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1996, 157 : 97 - 98