Saliva with different concentrations of enzyme with esterolytic activity, and its effect on the immediate and long-term bond strength of adhesive systems to dentin

被引:1
|
作者
Barros, Leonardo Santos [1 ]
Basting, Roberta Tarkany [1 ]
Vieira-Junior, Waldemir Francisco [1 ]
Franca, Fabiana Mantovani Gomes [1 ]
do Amaral, Flavia Lucisano Botelho [1 ]
Turssi, Cecilia Pedroso [1 ,2 ]
机构
[1] Sao Leopoldo Mandic Dent Inst, Div Cariol & Restorat Dent, Dept Orthodont, Campinas, SP, Brazil
[2] Inst & Ctr Pesquisas Odontol Sao Leopoldo Mandic, Rua Jose Rocha Junqueira 13, BR-13045755 Campinas, SP, Brazil
关键词
Aging; Albumin; Enzymatic degradation; Hybrid layer; Micro; -tensile; ETCH ADHESIVE; RESIN; BIODEGRADATION; LEACHABILITY; DEGRADATION; COMPOSITES; STRATEGIES; ESTERASE; WATER; MMPS;
D O I
10.1016/j.ijadhadh.2024.103657
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The present study evaluated whether different concentrations of albumin would influence the immediate or longterm bond strength of adhesive systems to dentin. Human third molars (N = 90) were sectioned at the dentinenamel junction to obtain middle dentin occlusal surfaces. After sectioning into discs, the molars were restored with resin composite (Filtek Z250, 3 M/ESPE) by using an etch-and-rinse (Adper Scotchbond MultiPurpose, 3 M/ESPE) or a self-etch (Clearfil SE Bond, Kuraray) adhesive system. The specimens were then sectioned into beams and stored in artificial saliva containing albumin in regular (100 mu g/mL; SA100) or elevated (700 mu g/mL; SA700) concentration-both concentrations simulated the range in which this enzyme may be present clinically, depending on the patient's periodontal condition. Beams from the control group (CO) were kept in artificial saliva with no addition of albumin. Half of the beams from each group were stored for 24 h, and the remainder, for 12 months. Then, the microtensile bond strength test was performed, and the failure mode was analyzed (adhesive, cohesive, or mixed). Bond strength data were submitted to the generalized linear model, followed by the Tukey tests, and failure modes were compared using chi-square tests (alpha = 5%). There were no significant interactions, but there was a significant effect between the albumin concentration (p = 0.015) and the time factor (p = 0.016). The beams stored in SA700 had significantly lower bond strength in comparison with the CO beams, regardless of the adhesive system. At 12 months, the bond strength decreased significantly for all groups. SA700 caused a significant increase in the adhesive failures after 12 months (p = 0.005). It was concluded that the bond strength of both adhesive systems was impaired by the albumin concentration aging.
引用
收藏
页数:7
相关论文
共 50 条
  • [41] Effect of tin–chloride pretreatment on bond strength of two adhesive systems to dentin
    Anne Peutzfeldt
    Tamara Koch
    Carolina Ganss
    Simon Flury
    Adrian Lussi
    Clinical Oral Investigations, 2014, 18 : 535 - 543
  • [42] Halloysite nanotube incorporation into adhesive systems—effect on bond strength to human dentin
    Mohammed S. Alkatheeri
    Jadesada Palasuk
    George J. Eckert
    Jeffrey A. Platt
    Marco C. Bottino
    Clinical Oral Investigations, 2015, 19 : 1905 - 1912
  • [43] Effect of 2% Chlorhexidine on the Bond Strength of Two Adhesive Systems to Human Dentin
    Bengtson, Camilla Regina Galvao
    Bengtson, Antonio Lucindo
    Bengtson, Nadya Galvao
    Turbino, Miriam Lacalle
    PESQUISA BRASILEIRA EM ODONTOPEDIATRIA E CLINICA INTEGRADA, 2008, 8 (01): : 51 - 56
  • [44] Dentin desensitizer effect's on adhesive systems's microtensile bond strength
    Massarotto, JA
    Oliveira, LV
    Seara, S
    Kroll, L
    Pereira, GDS
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B60 - B60
  • [45] Effect of remaining dentin thickness on microtensile bond strength of current adhesive systems
    Ting, Shihchun
    Chowdhury, A. F. M. Almas
    Pan, Feng
    Fu, Jiale
    Sun, Jihow
    Kakuda, Shinichi
    Hoshika, Shuhei
    Matsuda, Yasuhiro
    Ikeda, Takatsumi
    Nakaoki, Yasuko
    Abe, Shigeaki
    Yoshida, Yasuhiro
    Sano, Hidehiko
    DENTAL MATERIALS JOURNAL, 2015, 34 (02) : 181 - 188
  • [46] The effect of different pretreatment methods of PMMA-based crowns on the long-term tensile bond strength to dentin abutments
    Keul, Christine
    Kohen, Daliah
    Eichberger, Marlis
    Roos, Malgorzata
    Gernet, Wolfgang
    Stawarczyk, Bogna
    CLINICAL ORAL INVESTIGATIONS, 2015, 19 (01) : 35 - 43
  • [47] The effect of different pretreatment methods of PMMA-based crowns on the long-term tensile bond strength to dentin abutments
    Christine Keul
    Daliah Kohen
    Marlis Eichberger
    Malgorzata Roos
    Wolfgang Gernet
    Bogna Stawarczyk
    Clinical Oral Investigations, 2015, 19 : 35 - 43
  • [48] Long-term shear bond strength of luting cements to dentin.
    Piwowarczyk, A.
    Lindemann, K.
    Zipprich, H.
    Lauer, H. -C.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B194 - B194
  • [49] Effect of epigallocatechin gallate, green tea extract and chlorhexidine application on long-term bond strength of self-etch adhesive to dentin
    Gerhardt, K. M. F.
    Oliveira, C. A. R.
    Franca, F. M. G.
    Basting, R. T.
    Turssi, C. P.
    Amaral, F. L. B.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2016, 71 : 23 - 27
  • [50] Effect of chlorhexidine application or Nd:YAG laser irradiation on long-term bond strength of a self-etching adhesive system to dentin
    Menezello S.A.
    França F.M.G.
    Basting R.T.
    Turssi C.P.
    de Souza-Gabriel A.E.
    Palma-Dibb R.G.
    do Amaral F.L.B.
    Lasers in Dental Science, 2017, 1 (1) : 41 - 46