Effects of hot deformation on microstructure evolution, hardness, and intergranular corrosion of 7085 aluminum alloy sheets

被引:0
|
作者
Wu, Jiangjing [1 ]
Kai, Xizhou [1 ]
Guan, Chuang [1 ]
Cao, Rui [1 ]
Zhao, Yutao [1 ]
机构
[1] Jiangsu Univ, Sch Mat Sci & Engn, Zhenjiang 212013, Jiangsu, Peoples R China
来源
KOVOVE MATERIALY-METALLIC MATERIALS | 2023年 / 61卷 / 02期
关键词
grain boundaries; recrystallization; dislocation; hardness; intergranular corrosion (IGC); MECHANICAL-PROPERTIES; RECRYSTALLIZATION BEHAVIOR; ZR; PRECIPITATION; FRACTURE; TENSILE; STRESS; SC;
D O I
10.31577/km.2023.2.69
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, slabs of 7085 aluminum alloy were fabricated by electromagnetic stirring and solidifying with copper mold and suffered hot plastic deformation. The straight hot rolling process was used when the slabs were preheated to 420 degrees C for 1 h. The thicknesses of 1-, 2-, and 3-mm sheets correspond to the thickness reduction rate of 92, 83, and 75 % of original rectangular slabs. The microstructure results show that hot rolling deformation crushes the remanent phases into small sizes, leads particles into homogeneous distribution, and changes the dendritic grain into a fiber structure. The recrystallization rate decreases with the final sheet thickness increase after heat treatment. The recrystallization is strictly restricted when the thickness reduction rate approaches 92 %. EBSD results provide a unique perspective to view grain and dislocation evolution and texture change in different tempers of sheets. The hardness and intergranular corrosion (IGC) performance show that hardness is reduced while the corrosion depth is aggravated by the rise of sheet thickness. The maximum hardness is 86.75 HRB, and theminimum corrosion depth is only 9.17 mu m in the 1-mm sheet. The effects of grain boundary precipitates (GBPs), recrystallization, and precipitate-free zone (PFZ) on hardness and IGC were studied.
引用
收藏
页码:69 / 80
页数:12
相关论文
共 50 条
  • [41] Effect of Gd Addition on Hot Deformation Behavior and Microstructure Evolution of 7075 Aluminum Alloy
    Li, Yajie
    Fan, Xuran
    Qin, Fengming
    Zhao, Xiaodong
    Cao, Kefan
    Journal Wuhan University of Technology, Materials Science Edition, 2024, 39 (06): : 1595 - 1612
  • [42] Effect of deformation temperature on microstructure evolution in aluminum alloy 2219 during hot ECAP
    Mazurina, I.
    Sakai, T.
    Miura, H.
    Sitdikov, O.
    Kaibyshev, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 486 (1-2): : 662 - 671
  • [43] Effect of Gd Addition on Hot Deformation Behavior and Microstructure Evolution of 7075 Aluminum Alloy
    李亚杰
    FAN Xuran
    QIN Fengming
    赵晓东
    CAO Kefan
    Journal of Wuhan University of Technology(Materials Science), 2024, 39 (06) : 1595 - 1612
  • [44] Hot deformation behavior and microstructure evolution of hot-extruded 6A02 aluminum alloy
    Zhang, Ying
    Jiang, Jufu
    Wang, Ying
    Liu, Yingze
    Huang, Minjie
    MATERIALS CHARACTERIZATION, 2022, 188
  • [45] Effect of Initial Microstructure on the Hot Deformation Behavior and Microstructure Evolution of Aluminum Alloy AA2060
    Chaoyang Li
    Guangjie Huang
    Lingfei Cao
    Ruoxi Zhang
    Yu Cao
    Bin Liao
    Lin Lin
    Metals and Materials International, 2022, 28 : 1561 - 1574
  • [46] Effect of Initial Microstructure on the Hot Deformation Behavior and Microstructure Evolution of Aluminum Alloy AA2060
    Li, Chaoyang
    Huang, Guangjie
    Cao, Lingfei
    Zhang, Ruoxi
    Cao, Yu
    Liao, Bin
    Lin, Lin
    METALS AND MATERIALS INTERNATIONAL, 2022, 28 (07) : 1561 - 1574
  • [47] Effects of isothermal free forging temperature on microstructure and properties of 7085 aluminum alloy
    Liang, Xin
    Chen, Kang-Hua
    Chen, Xue-Hai
    Chen, Song-Yi
    Peng, Guo-Sheng
    Zhongnan Daxue Xuebao (Ziran Kexue Ban)/Journal of Central South University (Science and Technology), 2012, 43 (03): : 900 - 905
  • [48] Microstructure Evolution and Hot Deformation Behavior of a CuNiSn Alloy
    Jiang, Yexin
    Wang, Xu
    Li, Zhou
    Xiao, Zhu
    Sheng, Xiaofei
    Jiang, Hongyun
    Cai, Gengsheng
    Zhang, Xianwei
    PROCESSES, 2021, 9 (03) : 1 - 16
  • [49] Combined deformation behavior and microstructure evolution of 7050 aluminum alloy during hot shear-compression deformation
    Sang, De-li
    Fu, Rui-dong
    Li, Yi-jun
    MATERIALS CHARACTERIZATION, 2016, 122 : 154 - 161
  • [50] Effect of multi-axial compression on microstructure and corrosion resistance of 7085 aluminum alloy extrusions
    Xu, Xiao-Jing, 1600, Editorial Office of Transactions of Materials and Heat Treatment (35):