Crystallographic analysis of slip system activation in bimodal Ti-6Al-3Nb-2Zr-1Mo alloy under various dwell-fatigue loadings

被引:11
|
作者
Fan, Jiangkun [1 ,2 ]
Zhang, Wenyuan [1 ]
Li, Bobo [3 ]
Li, Kaidi [1 ]
Wang, Yang [4 ]
Jiang, Peng [4 ]
Wang, Chuanyun [1 ]
Xue, Xiangyi [1 ]
Kou, Hongchao [1 ,2 ]
Li, Jinshan [1 ,2 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] Northwestern Polytech Univ, Chongqing Innovat Ctr, Chongqing 401135, Peoples R China
[3] Luoyang Sunrui Titanium Precis Casting Co Ltd, Luoyang 471023, Peoples R China
[4] Luoyang Ship Mat Res Inst, Luoyang 471000, Peoples R China
基金
中国国家自然科学基金;
关键词
Titanium alloy; Dwell fatigue; Slip; Crystallographic orientation; Schmid factor; ALPHA/BETA-TITANIUM-ALLOY; STRAIN-RATE SENSITIVITY; CRYSTAL-PLASTICITY; CRACK-INITIATION; MICRO-TEXTURE; MICROSTRUCTURE; DEFORMATION; ORIENTATION; CREEP;
D O I
10.1016/j.msea.2023.144610
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microscopic deformation behavior is always been of significant interest in revealing the mechanism of the dwell fatigue effect. This study systematically characterized the deformation system activation in Ti-6Al-3Nb-2Zr-1Mo (Ti6321) alloy using in situ tensile and quasi-in situ dwell fatigue tests. The critical resolved shear stresses of the basal and prismatic slip systems in the Ti6321alloy were first calculated using the slip trace analysis method. The study demonstrated that, under dwell fatigue, basal and prismatic slips consist of major microscopic deformation modes. Most of the slip deformation occurred rapidly during the early stage of dwell fatigue and was independent of the dwell loading. The basal slip was found to be the predominant slip mode regardless of the dwell conditions. The results suggested that the elastic anisotropy of the hexagonal -closed-packed (HCP) structure could lead to heterogeneous microscopic stress, thus activating more basal slip activities. Such activities were found to participate in the crack initiation through two unique cracking modes: basal plane crack and (0001) twist boundary crack.
引用
收藏
页数:11
相关论文
共 50 条
  • [11] Hot Deformation Behavior and Processing Map of Ti-6Al-3Nb-2Zr-1Mo Titanium Alloy
    Chen Haisheng
    Liu Xianghong
    Liu Guangfa
    Tang Xiaodong
    Feng Yong
    Li Jinshan
    Fu Hengzhi
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (04) : 900 - 905
  • [12] The corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy: Effects of HCl concentration and temperature
    Baoxian Su
    Binbin Wang
    Liangshun Luo
    Liang Wang
    Yanqing Su
    Fuxin Wang
    Yanjin Xu
    Baoshuai Han
    Haiguang Huang
    Jingjie Guo
    Hengzhi Fu
    Journal of Materials Science & Technology, 2021, 74 (15) : 143 - 154
  • [13] The corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy: Effects of HCl concentration and temperature
    Su, Baoxian
    Wang, Binbin
    Luo, Liangshun
    Wang, Liang
    Su, Yanqing
    Wang, Fuxin
    Xu, Yanjin
    Han, Baoshuai
    Huang, Haiguang
    Guo, Jingjie
    Fu, Hengzhi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 74 : 143 - 154
  • [14] Effect of laser shock peening on the corrosion properties of Ti-6Al-3Nb-2Zr-1Mo alloy
    Luo, Gaoli
    Zhang, Lingfeng
    Xiong, Yi
    Zhang, Baofeng
    Chen, Xuepeng
    Wu, Yongli
    Wang, Shubo
    Cao, Wei
    SURFACE & COATINGS TECHNOLOGY, 2022, 440
  • [15] Investigation on microstructure and texture evolution of Ti-6Al-3Nb-2Zr-1Mo alloy during hot deformation
    Lu, Longlong
    Zhang, Yanmin
    Zhang, Zaoli
    Song, Kexing
    Li, Shanguang
    Li, Yan
    Zhou, Fei
    Cao, Qigao
    Feng, Qing
    Zhang, Binbin
    MATERIALS RESEARCH EXPRESS, 2021, 8 (09)
  • [16] Corrosion behaviour of a wrought Ti-6Al-3Nb-2Zr-1Mo alloy in artificial seawater with various fluoride concentrations and pH values
    Su, Baoxian
    Wang, Binbin
    Luo, Liangshun
    Wang, Liang
    Su, Yanqing
    Xu, Yanjin
    Li, Binqiang
    Li, Ting
    Huang, Haiguang
    Guo, Jingjie
    Fu, Hengzhi
    Zou, Yu
    MATERIALS & DESIGN, 2022, 214
  • [17] Effect of Laser Shock Peening on Microstructure and Properties of Ti-6Al-3Nb-2Zr-1Mo Titanium Alloy
    Luo Gaoli
    Zhang Lingfeng
    Xiong Yi
    Zhang Baofeng
    Chen Xuepeng
    CHINESE JOURNAL OF LASERS-ZHONGGUO JIGUANG, 2022, 49 (08):
  • [18] An investigation on fatigue and dwell-fatigue crack growth in Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    Shen, W
    Soboyejo, WO
    Soboyejo, ABO
    MECHANICS OF MATERIALS, 2004, 36 (1-2) : 117 - 140
  • [19] The effect of temperature on slip in microtextured Ti-6Al-2Sn-4Zr-2Mo under dwell fatigue
    Harr, M. E.
    Daly, S.
    Pilchak, A. L.
    INTERNATIONAL JOURNAL OF FATIGUE, 2021, 147
  • [20] Deformation Behavior of Ti-6Al-3Nb-2Zr-1Mo Titanium Alloy at Low Temperatures and High Strain Rates
    Li, Yanxing
    Wang, Lin
    An, Rui
    Zhao, Pingluo
    Yan, Zhiwei
    Cheng, Huanwu
    Cheng, Xingwang
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2022, 51 (12): : 4369 - 4375