Comparative investigation on the hot corrosion failure of YSZ and GdYb-YSZ double-ceramic-layer thermal barrier coatings under Na2SO4+V2O5 molten salts

被引:15
|
作者
Xiang, Yong [1 ]
Yan, Kai [1 ]
Yu, Haiyuan [2 ]
Guo, Yuwei [2 ]
Ying, Yuxi [2 ]
Li, Zhenrui [2 ]
Sun, Jian [3 ]
Fang, Chaogang [4 ]
机构
[1] China Univ Petr, Coll Mech & Transportat Engn, Beijing 102249, Peoples R China
[2] Beijing Beiye Funct Mat Co LTD, Mat Res Inst, Beijing 100192, Peoples R China
[3] China United Gas Turbine Technol Co LTD, Beijing 100015, Peoples R China
[4] Sichuan Ind Metrol & Testing Inst, Chengdu 610031, Peoples R China
基金
北京市自然科学基金; 中国国家自然科学基金;
关键词
Thermal barrier coatings; YSZ; GdYb-YSZ; Hot corrosion; Failure mechanism; PHASE-STABILITY; THERMOPHYSICAL PROPERTIES; OPTICAL BASICITY; BEHAVIOR; SULFATE; ZRO2; RE; CONDUCTIVITY; DEGRADATION; EVOLUTION;
D O I
10.1016/j.ceramint.2023.02.245
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The 5.2Gd2O3-5.6Yb2O3-9.5Y2O3 co-doped ZrO2 (GdYb-YSZ) double-ceramic-layer (DCL) thermal barrier coat-ings (TBCs) were prepared by atmospheric plasma spraying (APS) in this work. Hot corrosion behavior and failure mechanism of the APS GdYb-YSZ DCL and single-layer yttria partially stabilized zirconia (YSZ) TBCs under the Na2SO4+V2O5 molten salts were comparably investigated. The YSZ coating suffered from severe breakage after the hot corrosion test due to its poor corrosion resistance and easy infiltration by molten salts. In contrast, GdYb-YSZ DCL coating exhibited a better resistance to crack propagation and a significantly longer corrosion lifetime than the YSZ coating, which was attributed to the protective effect of the upper GdYb-YSZ layer. On the one hand, the superior phase stability of the GdYb-YSZ DCL coating could slow down the gener-ation speed of phase transformation stress. On the other hand, the higher corrosion reaction rate of the upper GdYb-YSZ layer could suppress the further infiltration of molten salts into the inner TBCs, which improved the structural integrity of TBCs in corrosive environments.
引用
收藏
页码:18678 / 18688
页数:11
相关论文
共 50 条
  • [31] Finite element simulation of stress distribution and development in 8YSZ and double-ceramic-layer La2Zr2O7/8YSZ thermal barrier coatings during thermal shock
    Wang, L.
    Wang, Y.
    Zhang, W. Q.
    Sun, X. G.
    He, J. Q.
    Pan, Z. Y.
    Wang, C. H.
    APPLIED SURFACE SCIENCE, 2012, 258 (08) : 3540 - 3551
  • [32] Hot corrosion of Gd2Zr2O7, Gd2Zr2O7/YbSZ, YSZ + Gd2Zr2O7/YbSZ, and YSZ thermal barrier coatings exposed to Na2SO4 + V2O5
    Tabeshfar, Mohadese
    Salehi, Mehdi
    Dini, Ghasem
    Dahl, Paul Inge
    Einarsrud, Mari-Ann
    Wiik, Kjell
    SURFACE & COATINGS TECHNOLOGY, 2021, 409
  • [33] Thermal shock performance and failure behavior of Zr6Ta2O17-8YSZ double-ceramic-layer thermal barrier coatings prepared by atmospheric plasma spraying
    Liu, Q.
    Hu, X. P.
    Zhu, W.
    Liu, G. L.
    Guo, J. W.
    Bin, J.
    CERAMICS INTERNATIONAL, 2022, 48 (17) : 24402 - 24410
  • [34] Investigation of the effect of V2O5 and Na2SO4 melted salts on thermal barrier coatings under cyclic conditions
    Ozgurluk, Yasin
    Doleker, Kadir Mert
    Karaoglanli, Abdullah Cahit
    ANTI-CORROSION METHODS AND MATERIALS, 2019, 66 (05) : 644 - 650
  • [35] Evolution of hot corrosion resistance of conventional CSZ and MoSi2 self-healing thermal barrier coatings in Na2SO4+V2O5 at 950 °C
    Soltani, P.
    Keyvani, A.
    Bahamirian, M.
    CERAMICS INTERNATIONAL, 2022, 48 (07) : 9038 - 9050
  • [36] Novel double-ceramic-layer (La0.8Eu0.2)2Zr2O7/YSZ thermal barrier coatings deposited by plasma spraying
    Liu, Zhan-Guo
    Zhang, Wei-Heng
    Ouyang, Jia-Hu
    Zhou, Yu
    CERAMICS INTERNATIONAL, 2014, 40 (07) : 11277 - 11282
  • [37] Study on hot corrosion behavior of Yb2Zr2O7 ceramic against Na2SO4+V2O5 molten salts at temperatures of 900-1200°C in air
    Li, S.
    Liu, Z. -G.
    Ouyang, J. -H.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2012, 63 (04): : 303 - 309
  • [38] Degradation mechanism of dual-phase thermal barrier coatings Gd2Zr2O7+8YSZ under hot corrosion in pure Na2SO4
    Iqbal, Amjad
    Moskal, Grzegorz
    Witala, Bartosz
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2025, 150 (01) : 151 - 165
  • [39] Thermal corrosion behavior of Yb4Hf3O12 exposed to Na2SO4+V2O5 molten salt
    Li, Yang
    Sun, Zhipeng
    He, Ling
    Pan, Ling
    Xiao, Peng
    Zhu, Henghai
    Duan, Junjie
    Zhou, Wei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1008
  • [40] Hot corrosion behavior of Cr2AlC MAX phase and CoNiCrAlY compounds at 950 °C in presence of Na2SO4+V2O5 molten salts
    Shamsipoor, A.
    Farvizi, M.
    Razavi, M.
    Keyvani, A.
    Mousavi, B.
    Pan, W.
    CERAMICS INTERNATIONAL, 2021, 47 (02) : 2347 - 2357