Liquid Metal Embrittlement Cracking in Uncoated Transformation-Induced Plasticity Steel during Consecutive Resistance Spot Welding

被引:2
|
作者
Kim, Jae Won [1 ,4 ]
Manladan, Sunusi Marwana [2 ]
Mahmud, Kaisar [2 ,5 ]
Jin, Woosung [2 ,6 ]
Krishna, Tejaswin [2 ]
Ji, Changwook [1 ]
Nam, Dae-Geun [3 ]
Park, Yeong-Do [2 ]
机构
[1] Korea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44413, South Korea
[2] Dong Eui Univ, Dept Adv Mat Engn, Busan 614714, South Korea
[3] Korea Inst Ind Technol, Dongnam Div, Busan 46938, South Korea
[4] Samsung Heavy Ind Co Ltd, Prod Technol Res Ctr, Seongnam 53261, South Korea
[5] Iota Consulting BD, Dhaka 1213, Bangladesh
[6] Tes one Co Ltd, Busan 49315, South Korea
关键词
liquid metal embrittlement; TRIP steels; resistance spot welding; consecutive welding; DEGRADATION; ELECTRODE;
D O I
10.3390/met13111826
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the automotive production line, a single pair of electrodes is employed to produce hundreds of consecutive welds before undergoing dressing or replacement. In consecutive resistance spot welding (RSW) involving Zn-coated steels, the electrodes undergo metallurgical degradation, characterized by Cu-Zn alloying, which impacts the susceptibility to liquid metal embrittlement (LME) cracking. In the present investigation, the possibility of LME crack formation in uncoated TRIP steel joints during consecutive RSW (involving 400 welds in galvannealed and uncoated TRIP steels) was investigated. The results have shown that different Cu-Zn phases were formed on the electrode surface because of its contamination with Zn from the galvannealed coating. Therefore, during the welding of the uncoated TRIP steel, the heat generated at the electrode/sheet interface would result in the melting of the Cu-Zn phases, thereby exposing the uncoated steel surface to molten Zn and Cu, leading to LME cracking. The cracks exhibited a maximum length of approximately 30 mu m at Location A (weld center) and 50 mu m at Location B (shoulder of the weld). The occurrence and characteristics of the cracks differed depending on the location as the number of welds increased due to the variation in Zn content. Type A cracks did not form when the number of welds was less than 280. Several cracks with a total length of approximately 30 mu m were suddenly formed between 280 and 400 welds. On the other hand, type B cracks began to appear after 40 welds. However, the number and size of these exhibited inconsistency as the number of welds increased. Overall, the results have shown that small LME cracks can form even in uncoated steels during consecutive welding of Zn-coated and uncoated steel joints.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Susceptibility of electrolytically galvanized dual-phase steel sheets to liquid metal embrittlement during resistance spot welding
    Frei, Julian
    Rethmeier, Michael
    WELDING IN THE WORLD, 2018, 62 (05) : 1031 - 1037
  • [22] Susceptibility of electrolytically galvanized dual-phase steel sheets to liquid metal embrittlement during resistance spot welding
    Julian Frei
    Michael Rethmeier
    Welding in the World, 2018, 62 : 1031 - 1037
  • [23] Liquid Metal Embrittlement of Galvanized TRIP Steels in Resistance Spot Welding
    Jeon, Wook-Sang
    Sharma, Ashutosh
    Jung, Jae Pil
    METALS, 2020, 10 (06) : 1 - 23
  • [24] Correction to: A Novel Shim-Assisted Resistance Spot Welding Process to Improve Weldability of Medium-Mn Transformation-Induced Plasticity Steel
    Shuoshuo Li
    Shanglu Yang
    Qi Lu
    Haiwen Luo
    Wu Tao
    Metallurgical and Materials Transactions B, 2019, 50 : 585 - 585
  • [25] A novel electrode tip geometry to mitigate liquid metal embrittlement during resistance spot welding
    Thomas Dupuy
    Welding in the World, 2022, 66 : 1715 - 1731
  • [26] A novel electrode tip geometry to mitigate liquid metal embrittlement during resistance spot welding
    Dupuy, Thomas
    WELDING IN THE WORLD, 2022, 66 (09) : 1715 - 1731
  • [27] Investigation of Liquid Metal Embrittlement during Resistance Spot Welding of Martensitic Steel with Zn Jet Vapor-Deposited Coating
    Kucera, Vojtech
    Zofkova, Zuzana
    DiGiovanni, Christopher
    He, Liu
    Vojtech, Dalibor
    METALS, 2021, 11 (11)
  • [28] Liquid Metal Embrittlement of Resistance Spot Welded 1180 TRIP Steel: Effect of Electrode Force on Cracking Behavior
    Choi, Du-Youl
    Sharma, Ashutosh
    Uhm, Sang-Ho
    Jung, Jae Pil
    METALS AND MATERIALS INTERNATIONAL, 2019, 25 (01) : 219 - 228
  • [29] Liquid Metal Embrittlement of Resistance Spot Welded 1180 TRIP Steel: Effect of Electrode Force on Cracking Behavior
    Du-Youl Choi
    Ashutosh Sharma
    Sang-Ho Uhm
    Jae Pil Jung
    Metals and Materials International, 2019, 25 : 219 - 228
  • [30] Liquid metal embrittlement in Zn-coated steel resistance spot welding: Critical electrode-contact and nugget growth for stress development and cracking
    Lalachan, Arun
    Murugan, Siva Prasad
    Jin, Woo-Sung
    Park, Yeong-Do
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2023, 318