Failure Analysis of Casting Ni-Cr-Mo Impeller After Long-Term Weak Acid Exposure

被引:1
|
作者
Ro, Yunjo [1 ]
Choi, Won-Seok [2 ]
Park, Hyunjoon [2 ]
Shin, Kyu-Chai [1 ]
机构
[1] SK Energy Co Ltd, Ulsan Complex, Ulsan, South Korea
[2] SK Innovat Inst Environm Sci & Technol, Daejeon, South Korea
关键词
Intergranular corrosion attack; Ni-Cr-Mo alloy (A494-CW6M); Topological closed phase (TCP); ELECTROCHEMICAL-BEHAVIOR; PRECIPITATION; SENSITIZATION; ALLOYS; BASE;
D O I
10.1007/s11668-023-01852-z
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The failure of the circulation pump in a sulfur recovery unit occurred after 11 years of operation, during which it was exposed to the weak acid process stream. The A494-CW6M impeller of the pump was found to be completely shattered, leading to the failure. Despite the long operating period, the failure appearance was unusual, and further investigation was needed to understand the cause of the failure. To this end, the detailed metallurgical characterization was performed using the electron microscope and commercially available thermodynamic software. The experimental results showed that the leached regions exhibited more than 50% of the impeller thickness, and those were matched with topological closed phases (M6C, Sigma, P phase), which commonly had low Cr (10 similar to 11 wt.%) and high Mo (56 similar to 58 wt.%) composition. The failure was attributed to the weak corrosion resistance of the low Cr phases when exposed to oxidizing weak acid streams. In addition, thermodynamic phase calculation showed that a large amount of TCPs precipitation was likely due to the malpractice of the heat treatment process. The detailed failure analysis result will be discussed in the present paper.
引用
收藏
页码:510 / 519
页数:10
相关论文
共 50 条
  • [31] EFFECTS OF MAGNESIUM AND LONG-TERM AGING ON INTRAGRANULAR PRECIPITATION IN FE-CR-NI-MN-MO-V-NB SUPERALLOY
    LI, YQ
    GONG, YH
    JOURNAL OF MATERIALS SCIENCE, 1992, 27 (24) : 6641 - 6645
  • [32] Microstructural evolution in the vicinity of Mo-W interfaces after long-term high-temperature exposure
    Jin, Xueyi
    Nie, Zhihua
    Xu, Chi
    Yu, Xiaodong
    Tan, Chengwen
    JOURNAL OF MATERIALS SCIENCE, 2023, 58 (17) : 7493 - 7503
  • [33] Ni-Cr-Co alloy ureteral stent: scanning electron microscopy and elemental analysis characterization after long-term indwelling
    Cauda, Valentina
    Fiori, Cristian
    Cauda, Furio
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2010, 94B (02) : 501 - 507
  • [34] MICROSTRUCTURE AND PHASE ANALYSIS OF 0.5Cr-0.5Mo-0.25V CREEP-RESISTANT STEELS AFTER LONG-TERM SERVICE
    Vyrostkova, Anna
    Svoboda, Milan
    Homolova, Viera
    Falat, Ladislav
    Kepic, Jan
    CHEMICKE LISTY, 2011, 105 : S452 - S454
  • [35] Changes in colonic microbiotas in rat after long-term exposure to low dose of okadaic acid
    Liu, Yang
    Zheng, Jian-Wei
    Peng, Xi-Chun
    Li, Hong-Ye
    Huang, Lu
    Li, Da-Wei
    Liu, Jie-Sheng
    Yang, Wei-Dong
    CHEMOSPHERE, 2020, 254
  • [36] INDUCTION OF NEPHROCALCINOSIS IN RABBIT KIDNEYS AFTER LONG-TERM EXPOSURE TO A STREPTOCOCCAL TEICHOIC-ACID
    WALTERSDORFF, RL
    FIEDEL, BA
    JACKSON, RW
    INFECTION AND IMMUNITY, 1977, 17 (03) : 665 - 667
  • [37] Analysis of Materials' Specimens After Long-Term Exposure on ISS Surface in Komplast Experiment
    Shaevich, S. K.
    Aleksandrov, N. G.
    Shumov, A. E.
    Novikov, L. S.
    Chernik, V. N.
    Petukhov, V. P.
    Samokhina, M. S.
    Sedov, V. V.
    Salnikova, I. A.
    Shindo, D. J.
    Golden, J. L.
    Kravchenko, M.
    PROTECTION OF MATERIALS AND STRUCTURES FROM THE SPACE ENVIRONMENT, ICPMSE-11, 2017, 47 : 23 - 33
  • [38] Electrochemical Properties of Zr–Mn–Cr–Ni–V Alloy in Long-Term Cycling After Air Oxidation
    Yu. M. Solonin
    O. Z. Galiy
    E. A. Graivoronska
    V. A. Lavrenko
    Powder Metallurgy and Metal Ceramics, 2018, 56 : 567 - 572
  • [39] FRACTURE TOUGHNESS AFTER LONG-TERM AGING IN 9CR-1MO-V STEEL FOR PRESSURE VESSELS
    Miyamura, Takeo
    Nanba, Shigenobu
    Nakanishi, Tomoaki
    Yamada, Masato
    ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2014, VOL 6B, 2014,
  • [40] MICROSTRUCTURE AND TENSILE PROPERTIES OF A 1.25Cr-0.5Mo MAIN STEAM PIPE AFTER LONG-TERM SERVICE
    Yang, Bin
    Jiang, Wen-Chun
    Sun, Wen-Qi
    Zhao, Yan-Ling
    Zhang, Wei-Ya
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2018, VOL 6B, 2019,