Fine dust after sanding untreated and thermally modified spruce, oak, and meranti wood

被引:3
|
作者
Sydor, Maciej [1 ]
Majka, Jerzy [1 ]
Hanincova, Ludka [2 ]
Kucerka, Martin [3 ]
Kminiak, Richard [4 ]
Kristak, Lubos [4 ]
Pedzik, Marta [1 ,5 ]
Ockajova, Alena [3 ]
Rogozinski, Tomasz [1 ]
机构
[1] Poznan Univ Life Sci, Fac Forestry & Wood Technol, PL-60637 Poznan, Poland
[2] Mendel Univ Brno, Fac Forestry & Wood Technol, Brno 61300, Czech Republic
[3] Matej Bel Univ, Dept Technol, Banska Bystrica 97401, Slovakia
[4] Tech Univ Zvolen, Fac Wood Sci & Technol, Zvolen 96001, Slovakia
[5] Poznan Inst Technol, Ctr Wood Technol, Lukasiewicz Res Network, PL-60654 Poznan, Poland
关键词
Compilation and indexing terms; Copyright 2025 Elsevier Inc;
D O I
10.1007/s00107-023-01971-2
中图分类号
S7 [林业];
学科分类号
0829 ; 0907 ;
摘要
Airborne wood dust poses health and safety risks in the construction and furniture industry. The study verified whether the thermal modification affects the share of fine wood dust particles (< 10 & mu;m) generated during spruce, oak, and meranti wood sanding. The experimental research involved nine material variants, including three wood species in three states: untreated, thermally modified at 160 & DEG;C, and thermally modified at 220 & DEG;C). To collect at least 200 g of each dust sample, a belt sander with P80 sandpaper and a belt speed of 10 m/s was used, along with a dust collector. The collected dust was then separated into fractions using a set of sieves with aperture sizes of 2000, 1000, 500, 250, and 125 & mu;m. A laser particle sizer was employed to measure the sizes of dust particles in the under-sieve fraction (dust with particle sizes smaller than 125 & mu;m). The under-sieve fraction was decomposed into three subfractions, with particle sizes: <2.5, 2.5-4.0, and 4.0-10 & mu;m. Surprisingly the results indicate that sanding dust from thermally modified wood generates a lower average mass share of potentially harmful fine particle fractions than dust from untreated wood. Oak dust contained a higher mass share of fine particles compared to the spruce and meranti dust samples. Dust from thermally modified oak and meranti wood had a lower content of harmful particle fractions than dust from untreated wood. The average mass shares of these dust fractions for modified wood at 160 and 220 & DEG;C showed no statictically significant differences (p < 0.05). Conversely, spruce dust had a low content of fine fractions because spruce particles exhibit a more irregular elongated shape. The study considered the extreme temperatures of 160 and 220 & DEG;C used in the thermal modification of wood. Therefore, the above statements are assumed to be valid for all intermediate thermo-modification temperatures.
引用
收藏
页码:1455 / 1464
页数:10
相关论文
共 50 条
  • [31] Particle size analysis of airborne wood dust produced from sawing thermally modified wood
    Matthew D. Aro
    Stephen Monson Geerts
    Suzanne French
    Meijun Cai
    European Journal of Wood and Wood Products, 2019, 77 : 211 - 218
  • [32] Influence of Natural Surface Ageing on Bonding Quality of Thermally Modified Oak and Beech Wood
    Zivkovic, Vjekoslav
    Gabrek, Gustav
    Mihulja, Goran
    DRVNA INDUSTRIJA, 2019, 70 (03) : 273 - 278
  • [33] Cell Wall Saturation Limit and Selected Properties of Thermally Modified Oak Wood and Cellulose
    Hrcka, Richard
    Kucerova, Viera
    Hyrosova, Tatiana
    Honig, Vladimir
    FORESTS, 2020, 11 (06): : 1 - 11
  • [34] Effects of Cyclic Changes in Relative Humidity on the Sorption Hysteresis of Thermally Modified Spruce Wood
    Majka, Jerzy
    Czajkowski, Lukasz
    Olek, Wieslaw
    BIORESOURCES, 2016, 11 (02): : 5265 - 5275
  • [35] VOLATILE ORGANIC COMPOUNDS EMITTED FROM UNTREATED AND THERMALLY MODIFIED WOOD-A REVIEW
    Pohleven, Jure
    Burnard, Michael D.
    Kutnar, Andreja
    WOOD AND FIBER SCIENCE, 2019, 51 (03): : 231 - 254
  • [36] Evaluation of thermally modified beech and spruce wood and their properties by FT-NIR spectroscopy
    Baechle, Helmut
    Zimmer, Bernhard
    Windeisen, Elisabeth
    Wegener, Gerd
    WOOD SCIENCE AND TECHNOLOGY, 2010, 44 (03) : 421 - 433
  • [37] Evaluation of thermally modified beech and spruce wood and their properties by FT-NIR spectroscopy
    Helmut Bächle
    Bernhard Zimmer
    Elisabeth Windeisen
    Gerd Wegener
    Wood Science and Technology, 2010, 44 : 421 - 433
  • [38] Thermal analysis of thermally treated spruce wood after its accelerated aging
    Kacikova, Danica
    Estokova, Adriana
    Gaff, Milan
    Kmetova, Elena
    Kudela, Jozef
    Kacik, Frantisek
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2025,
  • [39] Quality of Oil- and Wax-Based Surface Finishes on Thermally Modified Oak Wood
    Vidholdova, Zuzana
    Slabejova, Gabriela
    Smidriakova, Maria
    COATINGS, 2021, 11 (02) : 1 - 17
  • [40] Wetting-induced changes on the surface of thermally modified Scots pine and Norway spruce wood
    Cai, Chenyang
    Antikainen, Jukka
    Luostarinen, Katri
    Mononen, Kirsi
    Herajarvi, Henrik
    WOOD SCIENCE AND TECHNOLOGY, 2018, 52 (05) : 1181 - 1193