Fatigue fracture analysis of the 42CrMo4 crankshaft used for mining dump truck

被引:13
|
作者
Luo, Yucheng [2 ]
Yue, Gao [1 ,2 ,3 ]
Chen, Biyang [1 ,3 ]
Huang, Bin [2 ]
Liu, Fei [1 ,2 ,3 ]
Zhou, Lei [2 ]
Mao, Xiaofeng [2 ]
Deng, Shigui [2 ]
Du, Juan [2 ]
Liu, Kunming [2 ]
机构
[1] Guilin Univ Elect Technol, Sch Mech & Elect Engn, Guilin 541004, Guangxi, Peoples R China
[2] Guilin Fuda Co Ltd, Guilin 541199, Guangxi, Peoples R China
[3] Guilin Univ Elect Technol, Guangxi Key Lab Mfg Syst & Adv Mfg Technol, Guilin 541004, Guangxi, Peoples R China
基金
中国博士后科学基金;
关键词
Mining dump truck; Crankshaft; Fractography; High-cycle bending fatigue; Thickness of hardening layer; Bending moment; FAILURE ANALYSIS; BENDING FATIGUE; CAST-IRON; STRESS;
D O I
10.1016/j.engfailanal.2023.107724
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
A failure investigation was performed into the fractured 42CrMo4 crankshaft used for wide-body mining dump truck in this paper. Fracture morphology, chemical composition, microstructure and mechanical properties of the crankshaft material were studied to investigate the premature failure mechanism. All the crankshaft broke at the 4th or 6th necks and a high-cycle bending fatigue type in this case could be identified by the observation of beach marks and fatigue striations in the propagation area according to fractography results. The fatigue source is underneath the hardening layer of R fillet and the root cause could be identified as the designed inadequate thickness of quenching layer at the fillets obtained through medium frequency induction quenching (MFIQ), which could not provide adequate fatigue strength upon cyclic loadings for long term. Fatigue validation test indicated that the bending moment increased with the increasing thickness of the quenching layer, and the appropriate thickness was recommended about 3.5 mm based on overall consideration.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Nanomechanical properties of duplex treated 42CrMo4 steel
    Chen, J.
    Li, X. Y.
    Ji, R.
    Khan, R.
    Fuentes, G.
    SURFACE ENGINEERING, 2013, 29 (06) : 462 - 467
  • [42] An investigation into the grindability of additively manufactured 42CrMo4 steel
    Hoier, Philipp
    Santhosh, Deepa Kareepadath
    Hryha, Eduard
    Krajnik, Peter
    CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2024, 73 (01) : 257 - 260
  • [43] Hydrogen Diffusivity in Different Microstructures of 42CrMo4 Steel
    Imdad, Atif
    Zafra, Alfredo
    Arniella, Victor
    Belzunce, Javier
    HYDROGEN, 2021, 2 (04): : 414 - 427
  • [44] TRIBOLOGICAL BEHAVIOR OF 42CrMo4 STEEL NITRIDED BY PLASMA
    Saied, Chahinez
    Chala, Abdelouahed
    Belahssen, Okba
    Benramache, Said
    ACTA METALLURGICA SLOVACA, 2015, 21 (03): : 220 - 225
  • [45] Corrosion resistance of surface treated 42CrMo4 steel
    Kusmic, D.
    Hruby, V.
    Bacharova, L.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2016, 54 (06): : 491 - 496
  • [46] Life assessment of a 42CrMo4 steel under low-cycle fatigue and thermomechanical fatigue loading conditions
    Bartosak, Michal
    Horvath, Jakub
    Spaniel, Miroslav
    INTERNATIONAL JOURNAL OF FATIGUE, 2019, 129
  • [47] Deep Cryogenic Treatment and Nitriding of 42CrMo4 Steel
    Ciski, A.
    Wach, P.
    Jelenkowski, J.
    Nawrocki, P.
    Hradil, D.
    HTM-JOURNAL OF HEAT TREATMENT AND MATERIALS, 2019, 74 (01): : 12 - 22
  • [48] Nitriding problems on rolled rings made of 42CrMo4
    Barella, S.
    Boniardi, M.
    Cincera, S.
    Bellogini, M.
    METALLURGIA ITALIANA, 2011, (02): : 5 - 10
  • [49] THE TRIBOLOGICAL PROPERTIES OF LASER HARDENED STEEL 42CrMo4
    Tarasiuk, W.
    Gordienko, A. I.
    Wolocko, A. T.
    Piwnik, J.
    Szczucka-Lasota, B.
    ARCHIVES OF METALLURGY AND MATERIALS, 2015, 60 (04) : 2939 - 2943
  • [50] Nanoindentation of alumina and multiphase inclusions in 42CrMo4 steel
    Wagner, Ruben
    Lehnert, Robert
    Storti, Enrico
    Ditscherlein, Lisa
    Schroeder, Christina
    Dudczig, Steffen
    Peuker, Urs A.
    Volkova, Olena
    Aneziris, Christos G.
    Biermann, Horst
    Weidner, Anja
    MATERIALS CHARACTERIZATION, 2022, 193