Effect of pre-corrosion on the cavitation erosion performance of two aluminum bronzes in 3.5% NaCl solution

被引:4
|
作者
Song, Q. N. [1 ,2 ]
Wang, Y. [1 ]
Wu, Y. Q. [1 ]
Zhu, X. Y. [1 ]
Xu, N. [1 ]
Zhang, G. Y. [1 ]
Bao, Y. F. [1 ]
Zhao, J. H. [1 ]
Zhao, L. J. [1 ]
Gao, Y. [1 ]
Qiao, Y. X. [3 ]
机构
[1] Hohai Univ, Coll Mech & Elect Engn, 200 Jinling North Rd, Changzhou 213022, Peoples R China
[2] Mat Corros & Protect Key Lab Sichuan Prov, Zigong 643000, Sichuan, Peoples R China
[3] Jiangsu Univ Sci & Technol, Coll Mat Sci & Engn, 2 Mengxi Rd, Zhenjiang 212003, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Aluminum bronze; Corrosion; Cavitation erosion; OXIDE-FILM; BEHAVIOR; PHASES; MARINE;
D O I
10.1016/j.mtcomm.2023.107265
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The cavitation erosion (CE) behaviors of two aluminum bronzes after pre-corrosion in 3.5% NaCl solution were studied. Results indicated that the CE rate was increased by a factor of 82% for the nickel aluminum bronze (NAB) and 26.73% for the manganese aluminum bronze (MAB) after 30 days' pre-immersion, compared with the results of the corresponding fresh sample without pre-corrosion. Mechanical impact was dominantly responsible for the CE damage of the pre-corroded samples. Pre-corrosion increased the E/T (the contribution of pure erosion to the CE-corrosion damage) value from 42.66% to 65.20% for the NAB and from 72.46% to 80.13% for the MAB. After pre-immersion, pits appeared at the eutectoid microstructure in the NAB and the network-shaped 13 phases in the MAB because of selective phase corrosion. This increased the surface roughness and weakened the surface mechanical property. Therefore, large and deep cavities and remarkable material loss were created due to the collapse of eutectoid microstructure in the NAB and the detachment of kappa phases and brittle fracture of 13 phases in the MAB. The grievous CE damage of the MAB samples was highly attributed to the inferior mechanical property. In contrast, pre-corrosion had a much greater influence on the CE behavior of the NAB, because the CE resistance was remarkably deteriorated as a result of the corrosion damage at the eutectoid microstructure.
引用
下载
收藏
页数:9
相关论文
共 50 条
  • [1] Effect of Sulfide Concentration on the Corrosion and Cavitation Erosion Behavior of a Manganese-Aluminum Bronze in 3.5% NaCl Solution
    Q. N. Song
    N. Xu
    X. Jiang
    Y. Liu
    Y. Tong
    J. S. Li
    Y. F. Bao
    Y. X. Qiao
    Journal of Materials Engineering and Performance, 2019, 28 : 4053 - 4064
  • [2] Effect of Sulfide Concentration on the Corrosion and Cavitation Erosion Behavior of a Manganese-Aluminum Bronze in 3.5% NaCl Solution
    Song, Q. N.
    Xu, N.
    Jiang, X.
    Liu, Y.
    Tong, Y.
    Li, J. S.
    Bao, Y. F.
    Qiao, Y. X.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (07) : 4053 - 4064
  • [3] Cavitation Corrosion of Anodized Aluminum Alloy in 3.5% NaCl Solution
    Yong, X.
    Hou, C.
    Wu, J.
    Ji, J.
    Zhang, Z.
    Wang, J.
    CORROSION, 2011, 67 (04) : 0450031 - 0450036
  • [4] Synergistic effect of cavitation erosion and corrosion of various engineering alloys in 3.5% NaCl solution
    Kwok, CT
    Cheng, FT
    Man, HC
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 290 (1-2): : 145 - 154
  • [5] Influences of mass fraction of NaCl solution and cavitation time on cavitation erosion of corroded aluminum bronzes
    Wei X.
    Liu H.-X.
    Chen J.
    Chen J.-H.
    Deng Z.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2021, 31 (02): : 499 - 509
  • [6] Cavitation erosion of the AA7050 aluminum alloy in 3.5 wt% NaCl solution-Part 1: mitigating effect by corrosion
    Pan, Cheng-Cheng
    Xia, Da -Hai
    Hou, Meng -Yang
    Qin, Zhenbo
    Xu, Yunze
    Behnamian, Yashar
    Hu, Wenbin
    CORROSION SCIENCE, 2024, 232
  • [7] The role of Ti in cavitation erosion and corrosion behaviours of NAB alloy in 3.5 % NaCl solution
    Song, S. L.
    Li, D. G.
    Chen, D. R.
    Liang, P.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 919
  • [8] Corrosion and cavitation erosion behaviors of the manganese-aluminum-bronze cladding layer prepared by MIG in 3.5% NaCl solution
    Song, Q. N.
    Zhang, H. N.
    Li, H. L.
    Hong, H.
    Sun, S. Y.
    Xu, N.
    Zhang, G. Y.
    Bao, Y. F.
    Qiao, Y. X.
    MATERIALS TODAY COMMUNICATIONS, 2022, 31
  • [9] Synergistic effect between cavitation erosion and corrosion of Monel K500 alloy in 3.5 wt% NaCl solution
    He, Zebang
    Qin, Zhenbo
    Gao, Zhiming
    Wu, Zhong
    Hu, Wenbin
    MATERIALS CHARACTERIZATION, 2023, 205
  • [10] Corrosion wear behavior of Al-bronzes in 3.5% NaCl solution
    Li, WS
    Wang, ZP
    Lu, Y
    Yuan, LH
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2006, 15 (01) : 102 - 110