Microstructural characterization and mechanical properties of (TiB ? TiC) reinforced Ti-6Al-4V prepared by melt hydrogenation

被引:3
|
作者
Jiang, Botao [1 ]
Wang, Liang [1 ]
Yan, Hui [1 ]
Teng, Jiliang [1 ]
Wang, Binbin [1 ]
Luo, Liangshun [1 ]
Chen, Ruirun [1 ]
Su, Yanqing [1 ]
Guo, Jingjie [1 ]
Fu, Hengzhi [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
关键词
Microstructural characterization; Titanium matrix composites; Melt hydrogenation; Nano-hardness; CORROSION BEHAVIOR; COMPOSITES; ALLOY; ARCHITECTURE; EVOLUTION;
D O I
10.1016/j.jmrt.2023.01.094
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
TiB and TiC reinforced Ti-6Al-4V matrix composites were prepared by melt hydrogena-tion, in which the total fraction of the reinforcements was 5 vol % and the ratio of TiB to TiC was 1:1. The effects of melt hydrogenation on the solidification process, phase composi-tion, and microstructure of the titanium matrix were studied. The morphology and dis-tribution of the reinforcement without and with hydrogen were observed. Moreover, the nano-hardness of the composites was measured. The results show that the solidification process of the matrix can be changed by melt hydrogenation, which resulting the increase of b phase and refining of a lamellar in titanium alloy. Hydrogen increased the size of the reinforcements, which aggregated at the grain boundary of the primary b phase and formed a network structure. Hydrogen reduced the nano-hardness both of the titanium alloy and the reinforcements slightly. In summary, melt hydrogenation can maintain or slightly reduce the strength of the composites at room temperature and decrease the nano -hardness.(c) 2023 Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:2389 / 2398
页数:10
相关论文
共 50 条
  • [21] Microstructure Evolution and Enhanced Hot Workability of TiC/Ti-6Al-4V Composites Fabricated by Melt Hydrogenation
    Wang, Xuan
    Chen, Siyu
    Tan, Yingmei
    Yao, Longhui
    Wang, Liang
    Su, Yanqing
    Guo, Jingjie
    MATERIALS, 2022, 15 (24)
  • [22] Mechanical properties of tungsten fiber reinforced Ti-6Al-4V alloy
    Nishida, S
    Hayashi, K
    Hattori, N
    Nakano, K
    Yanagida, Y
    Tamasaki, H
    FRACTURE AND STRENGTH OF SOLIDS, PTS 1 AND 2, 2000, 183-1 : 1243 - 1248
  • [23] Microstructure evolution and mechanical properties of TIG cladded TiB reinforced composite coating on Ti-6Al-4V alloy
    An, Qi
    Huang, Lujun
    Jiang, Shan
    Li, Xinting
    Gao, Yanan
    Liu, Yue
    Geng, Lin
    VACUUM, 2017, 145 : 312 - 319
  • [24] Synthesis and mechanical properties of TiAl particle reinforced Ti-6Al-4V
    Decker, Sabine
    Lindemann, Janny
    Krueger, Lutz
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 674 : 361 - 365
  • [25] Fabrication of TiC/TiB/Ti3AlC2 phases reinforced coatings on Ti-6Al-4V substrate
    Zhang, H. X.
    Dai, J. J.
    Sun, C. X.
    Ma, Z. W.
    Wang, X. Y.
    Du, J. J.
    MATERIALS AND MANUFACTURING PROCESSES, 2018, 33 (10) : 1037 - 1042
  • [26] Microstructural Characterization of Hot Deformed Ti-6Al-4V
    Warchomicka, F.
    Poletti, C.
    Stockinger, M.
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL I, 2012, : 729 - 732
  • [27] Microstructural characterization of Ti-6Al-4V subjected to fretting
    Swalla, DR
    Neu, RW
    McDowell, DL
    JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2004, 126 (04): : 809 - 816
  • [28] Effect of hydrogen on superplastic deformation of (TiB + TiC)/Ti-6Al-4V composite
    Lu, Junqiang
    Qin, Jining
    Lu, Weijie
    Chen, Yifei
    Zhang, Di
    Hou, Hongliang
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2009, 34 (19) : 8308 - 8314
  • [29] Hot Deformation Behaviors in Ti-6Al-4V/(TiB+TiC) Composites
    Xuejian Lin
    Hongjun Huang
    Fuyu Dong
    Yue Zhang
    Xiaoguang Yuan
    Bowen Zheng
    Xiaojiao Zuo
    Acta Metallurgica Sinica(English Letters), 2021, 34 (12) : 1747 - 1757
  • [30] Superplasticity of coarse-grained (TiB + TiC)/Ti-6Al-4V composite
    Lu, Junqiang
    Qin, Jining
    Chen, Yifei
    Zhang, Zhiwei
    Lu, Weijie
    Zhang, Di
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 490 (1-2) : 118 - 123