Stress rupture of SiC/SiC composite tubes under high-temperature steam

被引:1
|
作者
Koyanagi, Takaaki [1 ,3 ]
Karakoc, Omer [1 ]
Hawkins, Charles [1 ]
Lara-Curzio, Edgar [1 ]
Deck, Christian [2 ]
Katoh, Yutai [1 ]
机构
[1] Oak Ridge Natl Lab, Mat Sci & Technol Div, Oak Ridge, TN USA
[2] Gen Atom, Nucl Technol & Mat Div, Electromagnet Syst, San Diego, CA USA
[3] Oak Ridge Natl Lab, Mat Sci and Technol Div, Oak Ridge, TN 37831 USA
关键词
composites; corrosion; corrosion resistance; oxidation; silicon carbide; OXIDATION; STRENGTH; BEHAVIOR; BRITTLE; FATIGUE; FIBERS; DAMAGE;
D O I
10.1111/ijac.14283
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
SiC-fiber-reinforced SiC matrix composite cladding for light water reactor fuel elements must withstand high-temperature steam oxidation in a loss-of-coolant accident scenario (LOCA). Current composite designs include an outer monolithic SiC layer, in part, to increase steam oxidation resistance. However, it is not clear how such a structure would behave under high-temperature steam in the case when the monolithic layer cracks and carbon interphases and SiC fibers are exposed to the environment. To fill this knowledge gap, stress-rupture tests of prototypic SiC composite cladding at 1000 degrees C under steam and inert environments were conducted. The applied stress was similar to 120 MPa, which was beyond the initial cracking stress. The failure lifetime under steam was 400-1300 s, while 75% of the composite specimens did not fail after 3 h of total exposure under inert gases. Microstructural observations suggest that steam oxidation activated slow crack growth in the fibers, which led to failure of the composite. The results from this study suggest that stress rupture in steam environments could be a limiting factor of the cladding under reactor LOCA conditions.
引用
收藏
页码:1658 / 1666
页数:9
相关论文
共 50 条
  • [41] HIGH-TEMPERATURE TIME-DEPENDENT STRENGTH OF AN SI-SIC COMPOSITE
    TRANTINA, GG
    MEHAN, RL
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1977, 60 (3-4) : 177 - 178
  • [42] High-temperature Oxidation of Electrodeposited Ni-Co-SiC Composite Coatings
    Wang, Y.
    Sun, W. C.
    Xu, J. M.
    Guo, F.
    Jia, Z. W.
    1ST INTERNATIONAL WORKSHOP ON MATERIALS SCIENCE AND MECHANICAL ENGINEERING, 2017, 281
  • [43] Enchanced high-temperature performances of SiC/SiC composites by high densification and crystalline structure
    Shimoda, Kazuya
    Hinoki, Tatsuya
    Kishimoto, Hirotatsu
    Kohyama, Akira
    COMPOSITES SCIENCE AND TECHNOLOGY, 2011, 71 (03) : 326 - 332
  • [44] HIGH-TEMPERATURE BEHAVIOR OF A SIC/TI3AL+NB COMPOSITE
    BRINDLEY, PK
    JOURNAL OF METALS, 1987, 39 (10): : A51 - A51
  • [45] Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics
    Ando, K
    Chu, MC
    Tsuji, K
    Hirasawa, T
    Kobayashi, Y
    Sato, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (08) : 1313 - 1319
  • [46] Microstructural stability of SiC and SiC/SiC composites under high temperature irradiation environment
    Kishimoto, H
    Katoh, Y
    Kohyama, A
    JOURNAL OF NUCLEAR MATERIALS, 2002, 307 : 1130 - 1134
  • [47] AlN/SiC MEMS for High-Temperature Applications
    Esteves, Giovanni
    Habermehl, Scott D.
    Clews, Peggy J.
    Fritch, Chanju
    Griffin, Benjamin A.
    JOURNAL OF MICROELECTROMECHANICAL SYSTEMS, 2019, 28 (05) : 859 - 864
  • [48] High-Temperature Reliability of SiC Power MOSFETs
    Lelis, Aivars J.
    Green, Ronald
    Habersat, Daniel
    SILICON CARBIDE AND RELATED MATERIALS 2010, 2011, 679-680 : 599 - +
  • [49] HIGH-TEMPERATURE REACTIONS BETWEEN SIC AND COPPER
    QIN, CD
    DERBY, B
    BRITISH CERAMIC TRANSACTIONS AND JOURNAL, 1991, 90 (04): : 124 - 125
  • [50] High-Temperature Ceramic Composites (SiC/SiCw)
    N. E. Shchegoleva
    S. A. Evdokimov
    I. V. Osin
    A. S. Chainikova
    A. A. Shavnev
    Glass and Ceramics, 2020, 77 : 47 - 50