Understanding the Formation Mechanism of Al-Rich Interfacial Layer during Galvanizing of Cu Pre-coated High-Strength Steel Sheet

被引:1
|
作者
Kancharla, Harikrishna [1 ]
Mandal, G. K. [2 ]
Pradeep, K. G. [3 ]
Singh, S. S. [1 ]
Mondal, K. [1 ]
机构
[1] Indian Inst Technol Kanpur, Dept Mat Sci & Engn, Kanpur 208016, India
[2] CSIR Natl Met Labs, Jamshedpur 831007, Jharkhand, India
[3] Indian Inst Technol Madras, Dept Met & Mat Engn, Chennai 600036, India
关键词
atom probe tomography; Cu pre-coating; hot-dip galvanization; interfacial layer; SELECTIVE OXIDATION; COPPER; ATMOSPHERE; BEHAVIOR;
D O I
10.1007/s11665-023-08020-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work aims at understanding the formation of a beneficial thin continuous aluminum (Al)-rich interfacial layer with uniform distribution of fine equiaxed Fe-Al crystals formed at the substrate/coating interface during the initial stages of interfacial reactions as well as hindrance of Fe dissolution in Zn layer as soon as copper (Cu) pre-coated high-strength steel substrate is immersed into the molten zinc (Zn) bath containing 0.2 wt.% Al. Pre-coated Cu does not allow the immediate interaction and interdiffusion of Fe and Zn because of the positive heat of mixing between Fe and Cu. As the Cu dissolves in liquid Zn, counter-diffusion of Al and Zn toward the steel interface allows Fe to react with Al and Zn forming the thin Fe-Al inhibition layer with finer equiaxed grains. Moreover, dissolved Cu in the Zn layer would also prevent Fe diffusion in Zn in the time span during dipping, which is beneficial. Atom probe tomography (APT) analysis at the substrate/coating interface location reveals the presence of 56.22 & PLUSMN; 1.36 at.% Al, 35.01 & PLUSMN; 1.31 at.% Fe, 6.33 & PLUSMN; 0.66 at.% Zn, and 0.032 & PLUSMN; 0.01 at.% Cu, similar to the intermetallic compound of Fe2Al(5-x)Znx, as well Cu in the Zn layer supporting the above reasoning.
引用
收藏
页码:999 / 1006
页数:8
相关论文
共 26 条
  • [21] Research on tribological behavior and mechanism of laser surface texturing on tool surface in hot stamping of Al-Si-coated high-strength steel
    Mei, Tangjie
    Zhang, Qi
    Liu, Xiaochuan
    Han, Bin
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2024, 133 (9-10): : 4347 - 4364
  • [22] High-temperature friction and wear behaviour of different tool steels during sliding against Al-Si-coated high-strength steel
    Hardell, J.
    Prakash, B.
    TRIBOLOGY INTERNATIONAL, 2008, 41 (07) : 663 - 671
  • [23] Properties and formation mechanism of cladding layer on high-strength low-alloy steel subjected to ultrasonic impact treatment with titanium alloy pin
    Liu, Chuan
    Wang, Jianfei
    Tian, Lihui
    Liu, Zhenguang
    Wang, Jianxin
    Zhang, Jianxun
    SURFACE & COATINGS TECHNOLOGY, 2021, 418
  • [24] Study on Mechanical Properties and Deformation Mechanism of Fe-28Mn-10Al-C High-Strength Steel during Dynamic Deformation Process
    Cao, Shanji
    Zhang, Hanwen
    Tang, Zhengyou
    Yu, Shuo
    METALS, 2024, 14 (01)
  • [25] The Effect of Thermal Cycle on Hot Cracking Evolution and Formation Mechanism in Thin Wall, Single Layer, and Cubic Samples of High-Strength Al-Cu-Mg-Mn Alloys Fabricated by Laser Powder Bed Fusion
    Nie, Xiaojia
    Peng, Fei
    Hu, Zhiheng
    Qi, Yang
    Zhu, Haihong
    Zhang, Hu
    3D PRINTING AND ADDITIVE MANUFACTURING, 2024, 11 (06) : 1996 - 2013
  • [26] Influence of pre-stretching on quench sensitive effect of high-strength Al−Zn−Mg−Cu-Zr alloy sheet预拉伸对高强 Al−Zn−Mg−Cu−Zr 合金板材淬火敏感性效应的影响
    Ke-zhun He
    Qun Li
    Sheng-dan Liu
    Xin-ming Zhang
    Ke-chao Zhou
    Journal of Central South University, 2021, 28 : 2660 - 2669