Enhancing the Thermo-Mechanical Properties of Thermoplastic Starch Films Using Rice Straw Fibers as Reinforcement

被引:4
|
作者
Zeleke, Tamene Simachew [1 ]
Yihun, Fantahun Aklog [1 ]
Ayana, Misganaw Tegegne [2 ]
Kassa, Mulugeta Tesemma [2 ]
Alemante, Mekdes Fentabil [1 ]
机构
[1] Bahir Dar Univ, Dept Ind Chem, POB 79, Bahir Dar, Ethiopia
[2] Bahir Dar Univ, Dept Chem, POB 79, Bahir Dar, Ethiopia
关键词
Starch-based composite; Cellulose nanofiber; Tensile strength; Thermal stability and; Water holding capacity; MECHANICAL-PROPERTIES; PLASTICS; MUCILAGE; BLENDS;
D O I
10.1007/s42250-023-00584-9
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Nowadays, the need for biodegradable plastics is increasing because they are environmentally friendly and can replace petroleum-based non-degradable plastics that pollute the environment. Starch-based bio-plastics have huge potential to replace synthetic polymer-based plastics due to their economic and environmental advantages. However, the poor thermo-mechanical properties and high moisture sensitivity limited their application. In this study, potato peels that were readily available in the area were utilized to extract pure starch, which was then employed as a polymer matrix to develop starch-based composite films. Since rice straw is one of the most abundant agro-industrial residues worldwide, cellulose obtained from rice straw through chemical treatments was used as reinforcement. Using a simple domestic blender, the crude cellulose was disintegrated into cellulose nanofibers to boost the reinforcing efficiency. The starch-based composite films were fabricated using a simple solution casting method. The cellulose nanofibers in the composite films were at 1, 3, 5, 10, and 15 weight ratios. Thus obtained starch-based composite films were characterized in terms of their transparency, chemical structure, thermal stability, mechanical strength, and moisture sensitivity. The tensile strength of the thermoplastic composite films is remarkably enhanced by the inclusion of cellulose fibers as reinforcement. For the neat starch film, the tensile strength is 0.714 MPa and the value reaches 11.12 MPa for 10 wt% cellulose fiber addition. Increasing the concentration of the cellulose above 10 wt% reduced the tensile strength. The reason can be attributed to the fiber aggregation in the composite film, which resulted in poor interfacial interaction between the fillers and the stretch matrix. The fracture strain of the composite films was also linearly increased up to 10 wt% cellulose fiber inclusion. As the TGA data revealed, the thermal stability of the composite films was significantly enhanced due to the reinforcement effect of cellulose fibers. The addition of cellulose fibers up to 10 wt% also enhanced the moisture resistance of starch films, and the lowest water-holding composite film was obtained when the cellulose fiber content of the composite was 10 wt%. All the analysis in this work indicates that 10 wt% cellulose fibers is the optimum concentration to reinforce thermoplastic starch-based films for better industrial applications.
引用
收藏
页码:2321 / 2329
页数:9
相关论文
共 50 条
  • [21] Oxidative Degradations of Oxodegradable LDPE Enhanced with Thermoplastic Pea Starch: Thermo-Mechanical Properties, Morphology, and UV-Ageing Studies
    Raquez, Jean-Marie
    Bourgeois, Audrey
    Jacobs, Heidi
    Degee, Philippe
    Alexandre, Michael
    Dubois, Philippe
    JOURNAL OF APPLIED POLYMER SCIENCE, 2011, 122 (01) : 489 - 496
  • [22] Mechanical and Thermo-mechanical Properties of Carbon fiber Reinforced Thermoplastic Composite Fabricated Using Fused Deposition Modeling Method
    Gavali, Vinayak C.
    Kubade, Pravin R.
    Kulkarni, Hrushikesh B.
    MATERIALS TODAY-PROCEEDINGS, 2020, 22 : 1786 - 1795
  • [23] THERMO-MECHANICAL AND BAKING PROPERTIES OF THE QUINOA-RICE COMPOSITE FLOUR
    Banu, Iuliana
    Aprodu, Iuliana
    ANNALS OF THE UNIVERSITY DUNAREA DE JOS OF GALATI, FASCICLE VI-FOOD TECHNOLOGY, 2022, 46 (01) : 32 - 39
  • [24] Thermo-mechanical properties of alumina films created using the atomic layer deposition technique
    Miller, David C.
    Foster, Ross R.
    Jen, Shih-Hui
    Bertrand, Jacob A.
    Cunningham, Shawn J.
    Morris, Arthur S.
    Lee, Yung-Cheng
    George, Steven M.
    Dunn, Martin L.
    SENSORS AND ACTUATORS A-PHYSICAL, 2010, 164 (1-2) : 58 - 67
  • [25] Enhancing Thermo-Mechanical Properties of Epoxy Composites Using Fumed Silica with Different Surface Treatment
    Kim, Kyung-Min
    Kim, Hoon
    Kim, Hyun-Joong
    POLYMERS, 2021, 13 (16)
  • [26] Ablation and thermo-mechanical tailoring of EPDM rubber using carbon fibers
    Asghar, Muhammad
    Iqbal, Nadeem
    Iqbal, Sadia Sagar
    Farooq, Mohsin
    Jamil, Tahir
    JOURNAL OF POLYMER ENGINEERING, 2016, 36 (07) : 713 - 722
  • [27] Mechanical Properties of Keratin Composite Films Using Poultry Feathers as Reinforcement Fibers
    Shuming Shen
    Xuhong Yang
    Xiaofang Xu
    Fibers and Polymers, 2021, 22 : 1434 - 1440
  • [28] Mechanical Properties of Keratin Composite Films Using Poultry Feathers as Reinforcement Fibers
    Shen, Shuming
    Yang, Xuhong
    Xu, Xiaofang
    FIBERS AND POLYMERS, 2021, 22 (05) : 1434 - 1440
  • [29] Enhancing the Mechanical Properties of PBAT/Thermoplastic Starch (TPS) Biodegradable Composite Films through a Dynamic Vulcanization Process
    Cai, Kai
    Wang, Xiaodong
    Yu, Chenhao
    Zhang, Jing
    Tu, Shuhua
    Feng, Jie
    ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2024, 12 (04) : 1573 - 1583
  • [30] Optical and thermo-mechanical properties of composite films based on fish gelatin/rice flour fabricated by casting technique
    Ahmad, Mehraj
    Hani, Norziah Mohd
    Nirmal, Nilesh Prakash
    Fazial, Farah Faiqah
    Mohtar, Nor Fazliyana
    Romli, Siti Rashima
    PROGRESS IN ORGANIC COATINGS, 2015, 84 : 115 - 127