Influence of Microstructural Characteristics on the Mechanical and Wear Behavior of Wire Arc Additive Manufactured and Cast Eutectic Al-Si Alloy

被引:2
|
作者
Hemachandra, M. [1 ]
Thapliyal, Shivraman [1 ]
Mahammod, Babar Pasha [1 ]
Kumar, Adepu [1 ]
机构
[1] Natl Inst Technol Warangal, Mech Engn Dept, Warangal 506004, Telangana, India
关键词
Wire-arc additive manufacturing (WAAM); Casting; Eutectic Al-Si; Electron backscattered diffraction (EBSD); Sliding Wear; Wear Mechanisms; Subsurface; Mechanical-Mixed-Layer (MML); DRY SLIDING WEAR; CAVITATION EROSION RESISTANCE; AS-CAST; SUBSURFACE DEFORMATION; STAINLESS-STEEL; FRICTION; SOLIDIFICATION; TRIBOLOGY; PROPERTY; MG;
D O I
10.1007/s12633-024-02848-6
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The present study investigates the dry sliding wear behavior of Wire arc additive manufactured (WAAM) eutectic Al-Si alloy, with a particular focus on the effects of solidification and microstructural characteristics on wear behavior. Microstructural analysis indicated that the secondary dendrite arm spacing (SDAS) for the WAAM sample was three times higher than that of the cast sample. The WAAM sample exhibited thin, long columnar dendrites, while the cast samples displayed coarse and ripened dendrites. Furthermore, EBSD analysis revealed that the WAAM sample had a higher percentage (88.6%) of low-angle grain boundaries (LAGBs), contributing to their increased strength compared to cast samples with 78.6% LAGBs. The maximum wear rate of 5.45 x 10-6 g/m was observed at a normal load of 25 N and a sliding speed of 1.1 m/s with a coefficient of friction (CoF) of 0.59 for WAAM samples while casting samples exhibited a lower wear rate of 3.06 x 10-6 g/m and a CoF of 0.55 under identical conditions. Delamination, severe adhesion, and abrasion were the primary wear mechanisms under maximum wear rate test conditions. The subsurface of WAAM samples contained a mechanical mixed layer (MML), while cast samples revealed a stable thin oxide layer. The study found that samples with higher texture strength and lower Taylor factor (TF) values were more prone to damage.
引用
收藏
页码:2441 / 2463
页数:23
相关论文
共 50 条
  • [11] Spheroidization of the Al-Si eutectic in a cast aluminum alloy
    Páramo, V
    Colás, R
    Velasco, E
    Valtierra, S
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2000, 9 (06) : 616 - 622
  • [12] Spheroidization of the Al-Si eutectic in a cast aluminum alloy
    Víctor Páramo
    Rafael Colás
    Eulogio Velasco
    Salvador Valtierra
    Journal of Materials Engineering and Performance, 2000, 9 : 616 - 622
  • [13] Microstructural, Mechanical and Wear Properties of Al-1.3%Si Alloy as Compared to Hypo/Hyper-Eutectic Compositions in Al-Si Alloy System
    Mostafa, Ahmad
    Alshabatat, Nabeel
    CRYSTALS, 2022, 12 (05)
  • [14] Microstructural influence on dynamic fracture toughness of eutectic Al-Si casting alloy
    Hafiz, MF
    Kobayashi, T
    TRANSACTIONS OF THE AMERICAN FOUNDRYMEN'S SOCIETY, VOL 107, 1999, 107 : 803 - 806
  • [15] CAVITATION BEHAVIOR IN AL-SI EUTECTIC ALLOY
    MAHIDHARA, RK
    MUKHERJEE, AK
    MATERIALS TRANSACTIONS JIM, 1995, 36 (04): : 570 - 572
  • [16] Role of Si in the Anodizing Behavior of Al-Si Alloys: Additive Manufactured and Cast Al-Si10-Mg
    Revilla, Reynier I.
    Terryn, Herman
    De Graeve, Iris
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2018, 165 (09) : C532 - C541
  • [17] Influence of Si Content on the Microstructure and Corrosion Behavior of Additive Manufactured Al-Si Alloys
    Revilla, Reynier I.
    De Graeve, Iris
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2018, 165 (13) : C926 - C932
  • [18] The effects of Fe and Mn on microstructural and mechanical properties of modified Al-Si eutectic alloy
    Unkic, F
    Matkovic, P
    Matkovic, T
    STROJARSTVO, 1998, 40 (3-4): : 107 - 112
  • [19] Effects of Fe and Mn on microstructural and mechanical properties of modified Al-Si eutectic alloy
    Unkic, Faruk
    Matkovic, Prosper
    Matkovic, Tanja
    Strojarstvo, 1998, 40 (03): : 107 - 112
  • [20] Estimation of porosity and shrinkage in a cast eutectic Al-Si alloy
    Samavedam, S.
    Sakri, S. B.
    Rao, D. Hanumantha
    Sundarrajan, S.
    CANADIAN METALLURGICAL QUARTERLY, 2014, 53 (01) : 55 - 64