Effects of Ag3Sn nanoparticles and isothermal aging on IMC layer growth, mechanical properties, and life prediction of SAC305/Cu solder joints

被引:3
|
作者
Yuan, Peng [1 ]
Chen, Dongdong [1 ]
Qin, Junhu [2 ]
Bai, Hailong [2 ]
Zhang, Xin [2 ]
Gan, Guoyou [1 ]
Leng, Chongyan [1 ]
Yan, Jikang [1 ,3 ]
机构
[1] Kunming Univ Sci & Technol, Sch Mat Sci & Engn, Kunming, Yunnan, Peoples R China
[2] Yunnan Tin Ind Tin Mat Co Ltd, Kunming, Yunnan, Peoples R China
[3] Southwest Petr Univ Sch Engn, Nanchong, Sichuan, Peoples R China
来源
关键词
INTERMETALLIC COMPOUNDS; SN-ZN; MICROSTRUCTURE; PARTICLES;
D O I
10.1177/26349833231163598
中图分类号
TB33 [复合材料];
学科分类号
摘要
In this paper, Ag3Sn nanoparticles were prepared by chemical method and added into SAC305 solder in different proportions to explore the effects of the Ag3Sn on the wettability, melting performance, metallographic structure, and mechanical property of the solder. The results show that a small amount of Ag3Sn nanoparticles were able to reduce the wetting time, increase the maximum wetting force, and expand the spreading area. The melting performance was also improved. Ag3Sn nanoparticles were also found to significantly refine the solder structure in the metallographical. The best comprehensive performance was achieved with the addition of 0.5% Ag3Sn nanoparticles. These Ag3Sn nanoparticles effectively improved the morphology of the IMC at the interface and effectively reduced the thickness of the IMC layer. The addition of nano Ag3Sn increased the diffusion activation energy and stabilized the interface. Moreover, the growth of the IMC layer was inhibited by 0.5% Ag3Sn, as indicated by aging results. The addition of Ag3Sn nanoparticles increases the tensile strength and Vickers hardness of the solder joint. When the amount of Ag3Sn nanoparticles was 0.5 wt%, the tensile strength reached the maximum of 17.45 MPa. The microhardness value of the solder is greatly increased, which reaches 311 HV. Finite element simulation showed that the service life of the solder was prolonged by adding the appropriate amount of Ag3Sn nanoparticles. The paper demonstrates a method of "nano" solder paste preparation. Results show that the addition of Ag3Sn nanoparticles plays an important role in the interfacial reaction and mechanical properties between the SAC solder and Cu substrate.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] Effect of Doped Nano-Ni on Microstructure Evolution and Mechanical Behavior of Sn-3.0Ag-0.5Cu (SAC305)/Cu-2.0Be Solder Joint during Isothermal Aging
    Yin, Zuozhu
    Lin, Mei
    Huang, Yongde
    Chen, Yuhua
    Li, Qi
    Wu, Ziyuan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (05) : 3315 - 3323
  • [42] Effect of Doped Nano-Ni on Microstructure Evolution and Mechanical Behavior of Sn-3.0Ag-0.5Cu (SAC305)/Cu-2.0Be Solder Joint during Isothermal Aging
    Zuozhu Yin
    Mei Lin
    Yongde Huang
    Yuhua Chen
    Qi Li
    Ziyuan Wu
    Journal of Materials Engineering and Performance, 2020, 29 : 3315 - 3323
  • [43] Effects of Ni Nanoparticles on the Growth Rate of Intermetallic Compounds (IMCs) Between Sn-3.0Ag-0.5Cu (SAC305) Solder and Cu-2.0Be Substrate
    Zuozhu Yin
    Mei Lin
    Qi Li
    Xiaochun Lv
    Journal of Electronic Materials, 2020, 49 : 6721 - 6726
  • [44] Mechanical Behavior of Sn-3.0Ag-0.5Cu/Cu Solder Joints After Isothermal Aging
    Van Luong Nguyen
    Chin-Sung Chung
    Ho-Kyung Kim
    Journal of Electronic Materials, 2016, 45 : 125 - 135
  • [45] Formation and evolution of intermetallic layer structures at SAC305/Ag/Cu and SAC0705-Bi-Ni/Ag/Cu solder joint interfaces after reflow and aging
    Liu, Yang
    Meerwijk, Joost
    Luo, Liangliang
    Zhang, Honglin
    Sun, Fenglian
    Yuan, Cadmus A.
    Zhang, Guoqi
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2014, 25 (11) : 4954 - 4959
  • [46] Mechanical Behavior of Sn-3.0Ag-0.5Cu/Cu Solder Joints After Isothermal Aging
    Van Luong Nguyen
    Chung, Chin-Sung
    Kim, Ho-Kyung
    JOURNAL OF ELECTRONIC MATERIALS, 2016, 45 (01) : 125 - 135
  • [47] Formation and evolution of intermetallic layer structures at SAC305/Ag/Cu and SAC0705-Bi-Ni/Ag/Cu solder joint interfaces after reflow and aging
    Yang Liu
    Joost Meerwijk
    Liangliang Luo
    Honglin Zhang
    Fenglian Sun
    Cadmus A. Yuan
    Guoqi Zhang
    Journal of Materials Science: Materials in Electronics, 2014, 25 : 4954 - 4959
  • [48] Influence of TiO2 nanoparticles on IMC growth in Sn-3.0Ag-0.5Cu-xTiO2 solder joints during isothermal aging process
    Tang, Y.
    Li, G. Y.
    Chen, D. Q.
    Pan, Y. C.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2014, 25 (02) : 981 - 991
  • [49] Simulation of IMC Layer Growth and Cu Consumption in Sn-Ag-xCu/Cu Solder Joints during Reflow
    Wang, Xiaohui
    Huang, Mingliang
    Yang, Fan
    Zhao, Ning
    2012 13TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING (ICEPT-HDP 2012), 2012, : 822 - 826
  • [50] Effect of Isothermal Aging and Copper Substrate Roughness on the SAC305 Solder Joint Intermetallic Layer Growth of High Temperature Storage (HTS)
    Ab Rahim, Rabiah Al Adawiyah
    Zulkifli, Muhammad Nubli
    Jalar, Azman
    Afdzaluddin, Atiqah Mohd
    Shyong, Kim Siow
    SAINS MALAYSIANA, 2020, 49 (12): : 3045 - 3054