共 50 条
Corrosion behavior of PS-PVD spray Yb2Si2O7 environmental barrier coatings during continuous water vapor exposure
被引:23
|作者:
Wu, Jian
[1
,2
]
Yang, Wenchao
[1
]
Zhang, Xiaofeng
[2
]
Wang, Chao
[2
]
Zhuo, Xueshi
[2
]
Zhan, Yongzhong
[1
]
Liu, Min
[2
]
Zhou, Kesong
[2
]
机构:
[1] Guangxi Univ, Sch Resources Environm & Mat, Nanning 530004, Guangxi, Peoples R China
[2] Guangdong Acad Sci, Inst New Mat, Natl Engn Lab Modern Mat Surface Engn Technol, Guangzhou 510651, Peoples R China
基金:
中国国家自然科学基金;
关键词:
Environmental barrier coatings;
Plasma spray-physical vapor deposition;
Continuous steam exposure;
Thermally grown oxide;
RECESSION BEHAVIOR;
VOLATILITY;
COMPOSITES;
EVOLUTION;
PROPERTY;
MULLITE;
PHASE;
D O I:
10.1016/j.corsci.2022.110831
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
The corrosion behavior of Si/Yb2Si2O7 environmental barrier coatings prepared by plasma spray-physical vapor deposition during continuous water vapor exposure were investigated at 1350-1450 degrees C over 500 h. The results showed that the temperature had a major impact on the corrosion morphology of the EBCs. The various corrosion morphologies of Yb2Si2O7 affected the oxidation kinetics of the TGO, and therefore the TGO had a porous structure, as was attributed to the Si-SiO2 phase transition and H2 placeholder aggregation. Consequently, the Si/ Yb2Si2O7 EBCs need to be added a protecting layer or film that is more resistant to steam corrosion.
引用
收藏
页数:10
相关论文