Micro-CT Marginal and Internal Fit Evaluation of CAD/CAM High-Performance Polymer Onlay Restorations

被引:3
|
作者
Toma, Flavia Roxana [1 ]
Moleriu, Lavinia Cristina [2 ]
Porojan, Liliana [1 ]
机构
[1] Victor Babes Univ Med & Pharm Timisoara, Fac Dent Med, Ctr Adv Technol Dent Prosthodont, Dept Dent Prostheses Technol Dent Technol, Eftimie Murgu Sq 2, Timisoara 300041, Romania
[2] Victor Babe? Univ Med & Pharm Timisoara, Dept Funct Sci, Eftimie Murgu Sq 2, Timisoara 300041, Romania
关键词
PAEK; CAD/CAM; marginal and internal fitness; onlay; micro-CT evaluation; LOAD-BEARING CAPACITY; FIXED DENTAL PROSTHESES; FATIGUE RESISTANCE; COMPOSITE RESIN; ADAPTATION; CROWNS; TECHNOLOGY; ACCURACY; STRENGTH; FRACTURE;
D O I
10.3390/polym15071715
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
(1) Background: The use of high-performance polymers for fixed restorations requires additional studies regarding their adaptability and processing with CAD/CAM technology. This in vitro study aims to assess the marginal and internal fit of PEEK and PEKK materials using microcomputed tomography. (2) Methods: Twenty-four (n = 8) MOD onlays made of PEKK (Pekkton ivory), unmodified PEEK (Juvora medical), and modified PEEK (BioHPP) were investigated. A typodont mandibular left first molar was scanned to achieve 24 resin, 3D printed abutment teeth. The onlays were fabricated with a five-axis milling machine, and after cementation of the specimens, the marginal (MG) and internal gaps (IG) were evaluated at twelve points in the mesio-distal section and thirteen points in the bucco-lingual section using microcomputed tomography. For statistical data analysis, Wilcoxon signed-rank/paired Student t-Test, Mann-Whitney/unpaired Student t-Test, and one-way ANOVA test were applied. (3) Results: Significant differences (p < 0.05; a = 0.05) were reported between the MG and IG for each material for all three polymers and also among two materials in terms of the MG and IG (except Juvora-BioHPP). The highest IG values were recorded in angular areas (axio-gingival line angle) in the mesio-distal section for all the polymers. (4) Conclusions: For all the materials, MG < IG. The type of polymer influenced the adaptability; the lowest marginal and internal gap mean values were recorded for BioHPP. The analyzed polymer used for onlays are clinically acceptable in terms of adaptability.
引用
收藏
页数:13
相关论文
共 49 条
  • [21] A Micro-computed Tomography Analysis of Marginal and Internal Fit of Endocrowns Fabricated from Three CAD/CAM Materials
    Hassouneh, L.
    Jum'ah, A.
    Ferrari, M.
    Wood, D. J.
    [J]. OPERATIVE DENTISTRY, 2023, 48 (01) : 79 - 89
  • [22] Influence of Manufacturing Methods of Implant-Supported Crowns on External and Internal Marginal Fit: A Micro-CT Analysis
    Moris, Izabela C. M.
    Monteiro, Silas Borges
    Martins, Raissa
    Ribeiro, Ricardo Faria
    Gomes, Erica A.
    [J]. BIOMED RESEARCH INTERNATIONAL, 2018, 2018
  • [23] In vitro Evaluation of the Marginal Fit and Internal Adaptation of Zirconia and Lithium Disilicate Single Crowns: Micro-CT Comparison Between Different Manufacturing Procedures
    Riccitiello, Francesco
    Amato, Massimo
    Leone, Renato
    Spagnuolo, Gianrico
    Sorrentino, Roberto
    [J]. OPEN DENTISTRY JOURNAL, 2018, 12 : 160 - 172
  • [24] Crenelated versus Conventional Ceramic Dental Veneers: Microscopy and Micro-CT Evaluations of Marginal and Internal Fit to Tooth Surface
    Maroiu, Alexandra-Cristina
    Sinescu, Cosmin
    Duma, Virgil-Florin
    Topala, Florin
    Jivanescu, Anca
    Popovici, Paul Mircea
    Tudor, Anca
    Rominu, Mihai
    [J]. ADVANCES IN 3OM: OPTO-MECHATRONICS, OPTO-MECHANICS, AND OPTICAL METROLOGY, 2022, 12170
  • [25] Flexural Behavior of Biocompatible High-Performance Polymer Composites for CAD/CAM Dentistry
    Yeslam, Hanin E.
    [J]. JOURNAL OF COMPOSITES SCIENCE, 2023, 7 (07):
  • [26] In vitro evaluation of marginal and internal adaptation of class II CAD/CAM ceramic restorations with different resinous bases and interface treatments
    Sandoval, Maria Jose
    Rocca, Giovanni Tommaso
    Krejci, Ivo
    Mandikos, Michael
    Dietschi, Didier
    [J]. CLINICAL ORAL INVESTIGATIONS, 2015, 19 (09) : 2167 - 2177
  • [27] In vitro evaluation of marginal and internal adaptation of class II CAD/CAM ceramic restorations with different resinous bases and interface treatments
    María José Sandoval
    Giovanni Tommaso Rocca
    Ivo Krejci
    Michael Mandikos
    Didier Dietschi
    [J]. Clinical Oral Investigations, 2015, 19 : 2167 - 2177
  • [28] Marginal adaptation of bulk-fill resin composites with different viscosities in class II restorations: a micro-CT evaluation
    İsmail Hakkı Baltacioğlu
    Gülbike Demirel
    Burcu Öztürk
    Fulya Aydin
    Kaan Orhan
    [J]. BMC Oral Health, 24
  • [29] Effect of various digital cement space settings on the adaptation of CAD/CAM occlusal veneer "micro-ct evaluation"
    Elbadawy, Adel A.
    Abd Elaziz, Mohammed H.
    Alnazzawi, Ahmed A.
    Borzangy, Sary S.
    [J]. DENTAL MATERIALS JOURNAL, 2021, 40 (03) : 625 - 630
  • [30] Marginal adaptation of bulk-fill resin composites with different viscosities in class II restorations: a micro-CT evaluation
    Baltacioglu, Ismail Hakki
    Demirel, Gulbike
    Ozturk, Burcu
    Aydin, Fulya
    Orhan, Kaan
    [J]. BMC ORAL HEALTH, 2024, 24 (01)