Recrystallization behavior of an Al-Zn-Mg-Cu alloy during hot deformation and subsequent heat treatment

被引:8
|
作者
Long, Shuai [1 ,2 ]
Xia, Run-Ze [1 ]
Jiang, Yu-Peng [1 ]
Peng, Peng [1 ]
Wang, Shu-Yan [2 ]
Li, Shi-Shan [3 ]
Zhou, Yu-Ting [3 ]
Dai, Qing-Wei [1 ]
机构
[1] Chongqing Univ Sci & Technol, Coll Met & Mat Engn, Chongqing 401331, Peoples R China
[2] Southwest Aluminum Grp Co Ltd, Chongqing 401326, Peoples R China
[3] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400044, Peoples R China
来源
关键词
Al-Zn-Mg-Cu alloy; Hot deformation; Heat treatment; DRX; SRX; CONTINUOUS DYNAMIC RECRYSTALLIZATION; SERIES ALUMINUM-ALLOYS; PROCESSING MAPS; BP-ANN; MICROSTRUCTURE; FLOW; TI-6AL-4V; WORKING; MODEL;
D O I
10.1016/j.mtcomm.2023.107570
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The presence of excessive residual recrystallization structure in the aero-structural part of the Al-Zn-Mg-Cu alloy negatively affects its strength and stress corrosion resistance. To achieve higher service performance, it is significant to reveal the recrystallization behavior of the Al-Zn-Mg-Cu alloy during hot working and subsequent heat treatment. In this work, the isothermal compression tests of an Al-Zn-Mg-Cu alloy were performed at the temperature range 300-450 degrees C and strain rate range 0.01-10 s  1. The subsequent heat treatment of the deformed specimens was conducted. The microstructure was characterized by EBSD and XRD techniques. The natural logarithm of Zener-Hollomon parameter (lnZ) was introduced, which increases with the increasing strain rate and decreasing temperature. During hot deformation, CDRX was identified to be the predominant DRX mech-anism at high lnZ values, the corresponding recrystallization volume fraction was approximately 15 %. However, at low lnZ values, DDRX becomes the dominant mechanism, the corresponding recrystallization volume fraction was only around 5 %. Moreover, a kinetics analysis was conducted using a low proportion DRX model coupled with lnZ. By comparing the results obtained from finite element simulations with experimental findings, this model was proved to accurately predict the volume fraction of DRX during hot deformation. During the heat treatment process, due to the substantial storage of deformation energy, a significant portion (up to 84.5 %) of SRX was observed under high lnZ conditions. As the lnZ value decreases, the SRX weakens. This weakening is significant enough that under high temperature and low strain rate, the occurrence of SRX becomes extremely unlikely, which can be attributed to the low storage of deformation energy.
引用
收藏
页数:9
相关论文
共 50 条
  • [31] Deformation behavior and microstructure of an Al-Zn-Mg-Cu-Zr alloy during hot deformation
    Liang-ming Yan
    Jian Shen
    Jun-peng Li
    Zhou-bing Li
    Xiao-dong Yan
    International Journal of Minerals, Metallurgy, and Materials, 2010, 17 : 46 - 52
  • [32] Heat treatment process of Al-Zn-Mg-Cu alloy fabricated by powder hot extrusion technology
    Wang, Shao-Qing
    Yu, Hua-Shun
    Zhang, Zhen-Ya
    Wang, Hai-Tao
    Min, Guang-Hui
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2009, 30 (06): : 98 - 102
  • [33] Constitutive behavior and novel characterization of hot deformation of Al-Zn-Mg-Cu aluminum alloy for lightweight traffic
    Xindi, Hao
    Dong, Ren
    Juan, Dong
    Zong, Haiming
    Zhengfeng, Lv
    MATERIALS RESEARCH EXPRESS, 2021, 8 (01)
  • [34] Effect of hot deformation on microstructure and quenching-induced precipitation behavior of Al-Zn-Mg-Cu alloy
    Zhang, Menghan
    Li, Chengbo
    Zhang, Yong
    Liu, Shengdan
    Jiang, Jingyu
    Tang, Jianguo
    Ye, Lingying
    Zhang, Xinming
    MATERIALS CHARACTERIZATION, 2021, 172
  • [35] Hot Deformation Behavior and Mechanisms of SiC Particle Reinforced Al-Zn-Mg-Cu Alloy Matrix Composites
    Diao, Enze
    Fan, Jianzhong
    Yang, Zhiyu
    Lv, Zhaochong
    Gao, Hao
    Nie, Junhui
    MATERIALS, 2023, 16 (23)
  • [36] Hot compressive deformation behavior and microstructure characteristics of new ultra strength Al-Zn-Mg-Cu alloy
    Wang Yu
    Xiong Bai-ping
    Li Zhi-hui
    Wen Kai
    Huang Shu-hui
    Li Xi-wu
    Zhang Yong-an
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2019, 47 (02): : 99 - 106
  • [37] Investigation on deformation behaviors and dynamic recrystallization mechanism of spray formed Al-Zn-Mg-Cu alloy under hot compression
    Zhang, Zhiwu
    Liu, Ruxue
    Li, Dayong
    Peng, Yinghong
    Zhou, Guowei
    Jia, Zhihong
    Ma, Wantai
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 28 : 4401 - 4416
  • [38] Hot Deformation Behavior and Dynamic Recrystallization Kinetics of a Novel Sc and Zr Modified Ultra-high-strength Al-Zn-Mg-Cu Alloy
    Li, B.
    Chu, Z. J.
    Du, Y.
    Zhou, W.
    Zhou, X.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (12) : 7774 - 7784
  • [39] Hot Deformation Behavior and Dynamic Recrystallization Kinetics of a Novel Sc and Zr Modified Ultra-high-strength Al-Zn-Mg-Cu Alloy
    B. Li
    Z. J. Chu
    Y. Du
    W. Zhou
    X. Zhou
    Journal of Materials Engineering and Performance, 2020, 29 : 7774 - 7784
  • [40] Microstructural Evolution and Dynamic Softening Mechanisms of Al-Zn-Mg-Cu Alloy during Hot Compressive Deformation
    Shi, Cangji
    Lai, Jing
    Chen, X. -Grant
    MATERIALS, 2014, 7 (01): : 244 - 264