Microstructure and fracture toughness of SiAlCN ceramics toughened by SiCw or GNPs

被引:8
|
作者
Li, Zhijian [1 ]
Guo, Ruru [1 ]
Li, Lu [2 ]
Zheng, Ruixiao [1 ]
Ma, Chaoli [2 ]
机构
[1] Beihang Univ, Sch Mat Sci & Engn, Key Lab Aerosp Adv Mat & Performance, Minist Educ, Beijing 100191, Peoples R China
[2] Beihang Univ, Res Inst Frontier Sci, Beijing 100191, Peoples R China
基金
中国国家自然科学基金;
关键词
SiAlCN ceramics; SiC whiskers; Graphene nanoplatelets; Fracture toughness; CURVE BEHAVIOR; COMPOSITES; RESISTANCE; OXIDATION; STRENGTH; STABILITY; WHISKER; NANO;
D O I
10.1016/j.ceramint.2023.06.211
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Mechanical alloying and spark plasma sintering (SPS) were used to prepare dense SiAlCN ceramic and SiAlCN ceramic toughened by SiC whiskers (SiCw) or graphene nanoplatelets (GNPs). The influences of different reinforcements on the microstructure and fracture toughness were investigated. The SiAlCN ceramic exhibited a fracture toughness of 4.4 MPa m1/2 and the fracture characteristics of grain bridging, alternative intergranular and transgranular fracture. The fracture toughness of SiCw/SiAlCN ceramic increased to 5.8 MPa m1/2 and toughening mechanisms were crack deflection, SiCw bridging and pull-out. The fracture toughness of GNP/ SiAlCN ceramic increased significantly, which was up to 6.6 MPa m1/2. GNPs played an important role in grain refinement, which resulted in the smallest grain size. Multiple toughening mechanisms, including crack deflection, crack branch, GNP bridging and pull-out could be found. The better toughening effect could be attributed to the larger specific surface area of GNPs and the appropriate interface bonding between GNPs and matrix.
引用
收藏
页码:29709 / 29718
页数:10
相关论文
共 50 条
  • [31] Relationship between microstructure, toughening mechanisms, and fracture toughness of reinforced silicon nitride ceramics
    Inst fuer Werkstoffwissenschaft, Stuttgart, Germany
    J Am Ceram Soc, 10 (2619-2624):
  • [32] Measurement of indentation fracture toughness of silicon nitride ceramics: I, effect of microstructure of materials
    Miyazaki, Hiroyuki
    Hyuga, Hideki
    Yoshizawa, Yu-Ichi
    Hirao, Kiyoshi
    Ohji, Tatsuki
    INNOVATION IN CERAMICS SCIENCE AND ENGINEERING, 2007, 352 : 41 - +
  • [33] Fracture toughness, microstructure and toughening mechanism of leucite and lithium disilicate glass ceramics.
    Albakry, M
    Guazzato, M
    Swain, M
    BIOCERAMICS 15, 2003, 240-2 : 955 - 958
  • [34] The relationship between microstructure and fracture toughness of zirconia toughened alumina (ZTA) added with MgO and CeO2
    Rejab, Nik Akmar
    Azhar, Ahmad Zahirani Ahmad
    Ratnam, Mani Maran
    Ahmad, Zainal Arifin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2013, 41 : 522 - 530
  • [35] Effect of loading velocity on fracture toughness of a SiCw/A6061 composite
    Wang, L
    Kobayashi, T
    MATERIALS TRANSACTIONS JIM, 1997, 38 (07): : 615 - 621
  • [36] Dynamic Fracture Toughness of Piezoelectric Ceramics
    Chen Hao-Sen
    Yu Xia
    Guo Ya-Zhou
    Fang Dai-Ning
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2013, 96 (07) : 2036 - 2038
  • [37] Evaluation of fracture toughness of porous ceramics
    Sakaida, Y
    Tanaka, K
    JSME INTERNATIONAL JOURNAL SERIES A-SOLID MECHANICS AND MATERIAL ENGINEERING, 2003, 46 (01) : 30 - 39
  • [38] DYNAMIC FRACTURE-TOUGHNESS OF CERAMICS
    KISHI, T
    TAKEDA, N
    KIM, BN
    SUZUKI, K
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1989, 97 (11): : 1392 - 1397
  • [39] Fracture toughness of ceramics and ceramic composites
    Gogotsi, GA
    CERAMICS INTERNATIONAL, 2003, 29 (07) : 777 - 784
  • [40] Fracture toughness of a toughened silicon nitride by ASTM C 1421
    Quinn, GD
    Swab, JJ
    Motyka, MJ
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (06) : 1043 - 1045