Insights into the Mechanical Properties and Correlation Between Strain Path and Crystallographic Texture of the AA2024 Alloy During Severe Plastic Deformation

被引:4
|
作者
Naseri, Majid [1 ]
Reihanian, Mohsen [2 ]
Moghaddam, Ahmad Ostovari [1 ]
Gholami, Davood [3 ]
Alvand, Mohammad [4 ]
Borhani, Ehsan [4 ]
Trofimov, Evgeny [1 ]
机构
[1] South Ural State Univ, 76 Lenin Ave, Chelyabinsk 454080, Russia
[2] Shahid Chamran Univ Ahvaz, Fac Engn, Dept Mat Sci & Engn, Ahvaz, Iran
[3] Iran Univ Sci & Technol, Sch Met & Mat Engn, Tehran, Iran
[4] Semnan Univ, Fac New Sci & Technol, Dept Nanotechnol, Semnan, Iran
关键词
Bulk nanostructured materials; Severe plastic deformation; Strain path; Microstructure characterization; Crystallographic texture; Mechanical properties; ROLL-BONDING ARB; HIGH-STRENGTH; ELECTROCHEMICAL-BEHAVIOR; NANOSTRUCTURED MATERIALS; HYBRID COMPOSITE; CUBE TEXTURE; PURE COPPER; MICROSTRUCTURE; RECRYSTALLIZATION; EVOLUTION;
D O I
10.1007/s12540-023-01515-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study examined mechanical properties of AA2024 alloy and its correlation between strain path and crystallographic texture. Accumulative roll bonding (ARB) and cross accumulative roll bonding (CARB) were used to severely deform AA2024 alloys. Electron backscatter diffraction (EBSD) studies demonstrated that nano/ultrafine grains were formed by the strain routes after eight cycles. It was also found that the lamellar boundary spacing and the mean boundary spacing were similar to 360 +/- 10 nm and 845 +/- 10 nm after eight ARB cycles. In contrast to the ARB, the CARB specimen had equiaxed microstructures characterized by grains with a size of 150 and 100 nm. The CARB processed specimen exhibited a mean misorientation angle of 41.83 degrees and a fraction of high angle grain boundaries of 78%, these values were 34.57 degrees and 67% for ARB treated specimen, respectively. It was observed that the evolved texture is greatly affected by the strain paths. The ARB processed specimen revealed strong Copper {112} <111>, Dillamor {4 4 11} <11 11 8>, S {123} <634>, and Brass {011} <211> components. In contrast, the CARB processed specimen showed major texture with prominent Copper {112} <111>, Brass {011} <211>, Rotated Cube {001} <110>, S {123} <634>, and Goss {011} <100> components. In the CARB specimen, the Goss/Brass texture ratio was intensified and the mechanical properties were superior (tensile strength: 535 MPa, microhard-ness: 182 HV, elongation: 11.9%) compared with the ARB processed specimen (tensile strength: 455 MPa, microhardness: 145 HV, elongation: 9.2%). Further, the change in strain path did not significantly affect the intensity of Goss and Cube components, ruling out any further recrystallization tendency.
引用
收藏
页码:412 / 424
页数:13
相关论文
共 50 条
  • [41] Effect mechanism of serrated joint design on microstructure and mechanical properties of AA2024 and AA7075 alloy friction stir welding
    Yutao Zhou
    Yongfang Deng
    Jincheng Zeng
    Yangxin Ou
    Liang Hu
    Zihang Li
    Baixiong Liu
    [J]. The International Journal of Advanced Manufacturing Technology, 2024, 130 : 459 - 473
  • [42] Temperature Evolution and Mechanical Properties of Dissimilar Friction Stir Weldments when Joining AA2024 and AA7075 with an AA6056 Alloy
    R. Zettler
    F. Potomati
    J. F. dos Santos
    N. G. de Alcantara
    [J]. Welding in the World, 2006, 50 (11-12) : 107 - 116
  • [43] Texture variations and mechanical properties of aluminum during severe plastic deformation and friction stir processing with SiC nanoparticles
    Khorrami, M. Sarkari
    Saito, N.
    Miyashita, Y.
    Kondo, M.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 744 : 349 - 364
  • [44] Asymmetric cold rolling of AA7075 alloy: The evolution of microstructure, crystallographic texture, and mechanical properties
    Kazemi-Navaee, Amir
    Jamaati, Roohollah
    Aval, Hamed Jamshidi
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 824
  • [45] Influence of temperature on microstructure, crystallographic texture and mechanical properties of EN AW 6016 alloy during plane strain compression
    Ghosh, Arkajit
    Roy, Avinava
    Ghosh, Abhishek
    Ghosh, Manojit
    [J]. MATERIALS TODAY COMMUNICATIONS, 2021, 26
  • [46] Improving the mechanical properties of magnesium and a magnesium alloy through severe plastic deformation
    Yamashita, A
    Horita, Z
    Langdon, TG
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 300 (1-2): : 142 - 147
  • [47] Effect of Severe Plastic Deformation on the Mechanical Properties of Al6061 Alloy
    Mishra, Vagish D.
    Palaniappan, Karthik
    Rao, Balkrishna C.
    Murthy, H.
    [J]. TMS 2020 149TH ANNUAL MEETING & EXHIBITION SUPPLEMENTAL PROCEEDINGS, 2020, : 2113 - 2116
  • [48] Effect of severe plastic deformation on mechanical properties and microstructure in 7075 aluminum alloy
    Kuramoto, Shigeru
    Horibuchi, Kayo
    Aoi, Ichiro
    Oh-Ishi, Keiichiro
    [J]. Keikinzoku/Journal of Japan Institute of Light Metals, 2014, 64 (06): : 241 - 248
  • [49] Improving the mechanical properties of magnesium and a magnesium alloy through severe plastic deformation
    [J]. Langdon, T.G. (langdon@usc.edu), 1600, Elsevier BV (300): : 1 - 2
  • [50] Nanoparticles Addition in AA2024 Aluminum/Pure Copper Plate: FSSW Approach, Microstructure Evolution, Texture Study, and Mechanical Properties
    Behrouz Bagheri
    Mehdi Alizadeh
    Seyyed Ehsan Mirsalehi
    Ali Shamsipur
    Amin Abdollahzadeh
    [J]. JOM, 2022, 74 : 4420 - 4433