Effect of Sc on the microstructure and mechanical properties of ZrB2 particles reinforced spray formed 7055 aluminum alloy TIG welded joint

被引:0
|
作者
Huang, Ting [1 ,2 ]
Xu, Junhua [2 ]
Yu, Lihua [2 ]
Zhao, Lijun [2 ]
机构
[1] Jiangsu Univ, Coll Mat Sci & Engn, Zhenjiang 212000, Peoples R China
[2] Jiangsu Univ Sci & Technol, Sch Mat Sci & Engineer, Zhenjiang 212003, Peoples R China
关键词
Sc; ZrB2; particles; Spray formed 7055 aluminum alloy; TIG welded joint; PRECIPITATION KINETICS; PERFORMANCE; AIRCRAFT; BEHAVIOR; GD;
D O I
10.1016/j.jmrt.2023.09.145
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Adding nano ceramic particles to the weld seam is an effective way to improve the strength of the spray formed 7055 aluminum alloy welded joint. However, nano ceramic particles are prone to agglomeration, and the agglomerated nano ceramic particles in welded joint can cause stress concentration and brittle fracture of the specimen. In order to improve the aggregation of nano ZrB2 ceramic particles in the weld seam and further improve the mechanical properties of spray formed 7055 aluminum alloy TIG welded joint, Sc/ZrB2-7055 (SZ7) and ZrB2-7055 (Z7) welded joints were prepared in this study. Compared to the Z7 weld seam with coarse grains and severe aggregation of ZrB2 particles, the SZ7 weld seam has fine grains, and the distribution of ZrB2, Al-3(Sc, Zr), and Sc modified ZrB2 particles in the weld seam was more uniform. The tensile strength and elongation of Z7 welded joints were 281 MPa and 2.0%, while the tensile strength and elongation of SZ7 welded joints were 320 MPa and 4.9%. The tensile strength and elongation values of SZ7 welded joints have increased by 13.8% and 145% respectively compared to Z7 welded joints. Sc elements formed a rich Sc layer on the surface of ZrB2 particles, which passivated the sharp corners of ZrB2 particles and increased the wettability between ZrB2 particles and Al liquid, resulting in uniform distribution of ZrB2 particles in the weld seams. Fine grain strengthening, dispersion strengthening, and dislocation strengthening are the main reasons for improving the mechanical properties of SZ7 welded joints.(c) 2023 The Authors. Published by Elsevier B.V.
引用
收藏
页码:9039 / 9048
页数:10
相关论文
共 50 条
  • [21] Microstructure and mechanical properties of 5554 aluminum alloy TIG-welded seam
    Wang, Hongfeng
    Zuo, Dunwen
    Wang, Hongyu
    Shao, Dinglin
    Nanjing Hangkong Hangtian Daxue Xuebao/Journal of Nanjing University of Aeronautics and Astronautics, 2010, 42 (06): : 753 - 757
  • [22] Microstructure and Mechanical properties of Molybdenum alloys doped with ZrB2 particles
    Zhang Guo-jun
    Zhuo Jun
    Ren Shuai
    MATERIALS SCIENCE AND ENGINEERING APPLICATIONS, PTS 1-3, 2011, 160-162 : 1828 - 1833
  • [23] Influence of thermo-mechanical conditions on the microstructure and mechanical property of spray-formed 7055 aluminum alloy
    Shao, Yong
    Shi, Jiahui
    Pan, Jiachen
    Liu, Qihang
    Yan, Lin
    Guo, Pingyi
    MATERIALS TODAY COMMUNICATIONS, 2022, 31
  • [24] Effect of hot deformation on the microstructure of spray-formed 7055 aluminum alloy extruded plate
    Lin, Xiao-min
    Wu, Xiao-dong
    Cao, Ling-fei
    Tang, Song-bai
    Bai, Min
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2023, 30 (12) : 3950 - 3963
  • [25] Effect of Rotation Speed on Performance of Friction Stir Welded Spray-Formed 7055 Aluminum Alloy
    Jiang, Yumo
    Zhao, Yong
    Zhao, Zhixia
    Ma, Shengchong
    Yan, Keng
    PHYSICS OF METALS AND METALLOGRAPHY, 2021, 122 (13): : 1419 - 1425
  • [26] Effect of Rotation Speed on Performance of Friction Stir Welded Spray-Formed 7055 Aluminum Alloy
    Yong Yumo Jiang
    Zhixia Zhao
    Shengchong Zhao
    Keng Ma
    Physics of Metals and Metallography, 2021, 122 : 1419 - 1425
  • [27] Microstructures and mechanical properties of the in-situ formed nanocomposites of (ZrB2 + Al2O3) and AA7055 alloy
    Xu, Zhuangzhuang
    Zhao, Yutao
    Kai, Xizhou
    Miao, Chang
    Cao, Rui
    MATERIALS LETTERS, 2022, 316
  • [28] Microstructure and mechanical properties of VPPA welded 7075 aluminum alloy joint
    Li, Guowei
    Han, Yongquan
    Chen, Furong
    Li, Yang
    Hanjie Xuebao/Transactions of the China Welding Institution, 2015, 36 (10): : 5 - 8
  • [29] Appropriate amount of TiB2 particles causes the ductile fracture of the un-weldable spray-formed 7055 aluminium alloy TIG-welded joint
    Huang, Ting
    Xu, Junhua
    Yu, Lihua
    Cheng, Yun
    Hu, Yunxuan
    Zhang, Hao
    MATERIALS RESEARCH EXPRESS, 2021, 8 (09)