Oxidation-Limited Lifetime of ODS-FeCrAl Alloys: Observations on Influence of Surface Shape

被引:1
|
作者
Wright, Ian G. [1 ]
Peraldi, Raphaelle [2 ]
机构
[1] WrightHT Inc, Denver, CO 80238 USA
[2] Airbus, Met Technol, Toulouse, France
关键词
Alumina scale-formers; Oxidation lifetime modeling; Influence of surface shape; Mode of scale failure; ODS-FeCrAl alloys; FeCrAl-RE alloys; BREAKAWAY OXIDATION; CYCLIC-OXIDATION; HIGH-TEMPERATURE; ALUMINUM DEPLETION; CHEMICAL FAILURE; OXIDE; PREDICTION; EXTENSION; BEHAVIOR; SCALES;
D O I
10.1007/s11085-023-10150-w
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Oxide dispersion-strengthened (ODS) FeCrAl ferritic steels constitute a class of alloys with a combination of mechanical strength capabilities and environmental resistance that permits operation at temperatures significantly higher than available classes of wrought alloy. A significant issue for these ODS alloys is that, because of the extreme operating temperatures, unexpected failure of the protective scale in service could lead to catastrophic degradation of high-temperature, high-pressure components. In the absence of handbook data for quantification of their high-temperature environmental degradation, significant efforts have been made to develop approaches for predictive oxidation lifetime modeling. The main basis for such models is an aspect of oxidation behavior peculiar to these alloys at very high temperatures, specifically, their ability to maintain a protective alumina scale until practically all available Al in the alloy has been consumed. At the high temperatures involved the concentration profile for Al throughout the component remains flat while the alumina scale is intact, so that knowledge of the oxidation kinetics provides a basis for calculating the time to exhaustion of the alloy's Al reservoir, hence service life. Difficulties arise when unanticipated gradients in the Al concentration profile are introduced following, for instance, premature local mechanical failure of the protective scale. The intent of this work was to consider if and how scale failures change with differences in surface shape, and how related mechanistic understanding of the actual oxidation behavior may be used to extend the utility of the modeling approaches. Experimental results for coupons of different shapes were very largely in agreement with the basic tenets of the lifetime modeling approaches, but a notable finding was that cylindrical shapes reproducibly exhibited a reduction in unexpected early scale failures, leading to more consistent oxidation-limited lifetimes.
引用
收藏
页码:183 / 200
页数:18
相关论文
共 50 条
  • [11] Effect of H2O and CO2 on the Oxidation Behavior and Durability at High Temperature of ODS-FeCrAl
    Sebastien Dryepondt
    Aurelie Rouaix-Vande Put
    Bruce A. Pint
    Oxidation of Metals, 2013, 79 : 627 - 638
  • [12] Positron annihilation lifetime spectroscopy of FeCr and FeCrAl oxide dispersion strengthened (ODS) alloys
    Ukai, S.
    Hirade, T.
    Okubo, N.
    MATERIALS CHARACTERIZATION, 2024, 211
  • [13] Predicting Oxidation-Limited Lifetime of Thin-Walled Components of NiCrW Alloy 230
    Duan, R.
    Jalowicka, A.
    Unocic, K.
    Pint, B. A.
    Huczkowski, P.
    Chyrkin, A.
    Gruener, D.
    Pillai, R.
    Quadakkers, W. J.
    OXIDATION OF METALS, 2017, 87 (1-2): : 11 - 38
  • [14] Predicting Oxidation-Limited Lifetime of Thin-Walled Components of NiCrW Alloy 230
    R. Duan
    A. Jalowicka
    K. Unocic
    B. A. Pint
    P. Huczkowski
    A. Chyrkin
    D. Grüner
    R. Pillai
    W. J. Quadakkers
    Oxidation of Metals, 2017, 87 : 11 - 38
  • [15] Oxidation-Limited 795 nm Vertical Cavity Surface Emission Laser
    Nie, Yuwei
    Li, Wei
    Lue, Jiagang
    Pan, Zhipeng
    Liu, Suping
    Ma, Xiaoyu
    CHINESE JOURNAL OF LASERS-ZHONGGUO JIGUANG, 2024, 51 (06):
  • [16] Microstructure evolution and mechanical properties of ODS FeCrAl alloys fabricated by an internal oxidation process
    Li, Jing
    Wu, Sajian
    Ma, Ping
    Yang, Ying
    Wu, Erdong
    Xiong, Liangyin
    Liu, Shi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 757 : 42 - 51
  • [17] Effect of water vapour on the oxidation of FeCrAl- and NiCrAl-base ODS alloys
    Prasanna, KMN
    Khanna, AS
    Quadakkers, WJ
    CORROSION AND ITS CONTROLS, VOLS I AND II, 1998, : 997 - 1003
  • [18] Oxidation limited life of FeCrAl based alloys during thermal cycling
    Naumenko, D
    Singheiser, L
    Quadakkers, WJ
    CYCLIC OXIDATION OF HIGH TEMPERATURE MATERIALS, 1999, (27): : 287 - 306
  • [19] Modelling the oxidation of FeCrAl-RE ODS alloys in simulated natural gas combustion environments
    Nicholls, JR
    Newton, R
    Simms, NJ
    Norton, JF
    MATERIALS AT HIGH TEMPERATURES, 2003, 20 (02) : 93 - 108
  • [20] Oxidation Behavior of ODS Fe–Cr–Al Alloys: Aluminum Depletion and Lifetime
    L. Maréchal
    B. Lesage
    A. M. Huntz
    R. Molins
    Oxidation of Metals, 2003, 60 : 1 - 28