Investigations on microstructure, thermo-mechanical and tribological behavior of graphene oxide reinforced AA7075 surface composites developed via friction stir processing

被引:25
|
作者
Nathan, S. Ragu [1 ]
Suganeswaran, K. [2 ]
Kumar, Surya [3 ]
Thangavel, P. [4 ]
Gobinath, V. K. [2 ]
机构
[1] Sree Vidyanikethan Engn Coll, Micromachining Res Ctr MMRC, Dept Mech Engn, Tirupati 517102, Andhra Pradesh, India
[2] Kongu Engn Coll, Dept Mechatron Engn, Perundurai 638060, Tamilnadu, India
[3] Katihar Engn Coll, Dept Mech Engn, Bihar 854109, India
[4] Kongu Engn Coll, Dept Mech Engn, Perundurai 638060, Tamilnadu, India
关键词
Surface composites; Dynamic recrystallization; Microstructure; Thermal conductivity; Impact toughness; Wear resistance; HIGH THERMAL-CONDUCTIVITY; METAL-MATRIX COMPOSITES; MECHANICAL-PROPERTIES; WEAR BEHAVIOR; ALLOY COMPOSITES; IMPACT TOUGHNESS; EXPANSION; GRAPHITE;
D O I
10.1016/j.jmapro.2023.01.084
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Surface composites (SCs) are fabricated through reduced graphene oxide (RGO) particulates by adopting friction stir process (FSP) route to enhance the mechanical and thermal properties suited for cylinder liner applications. Microstructural examination reveals that both dynamic recrystallization phenomenon and particle stimulated nucleation happens in the duration of processing phase and owes to a fine and homogenous distribution of re-inforcements in the matrix surface. Moreover, no sort of noticeable defects are formed between the base matrix and SC layer with prominent interface. An indigenous experimental setup is fabricated for the measurement of thermal conductivity of SCs. Percolation effect of reduced graphene oxide (RGO) particulates enhance the thermal conductivity of single pass SC specimen (158.6 W/mK) as compared to base metal (146 W/mK). For-mation of highly conductive RGO through reduction of oxygen level owing to the heat generation at the pro-cessing stage that favors for the high heat dissipation of the five pass specimen (201.5 W/mK). Decremented interparticle spacing of the aforementioned specimen through reduced grain size (9 mu m) enhances the impact toughness. Increased number of dislocations through grain refinement in the five pass specimen relieves the internal stress at a more possible extent which significantly reduces the coefficient of thermal expansion (CTE) value to 7.18 x 10-4 K-1. Superior Vickers hardness value (2188 MPa) enhances the specimen wear resistance. The worn morphology divulges the mild adhesive with abrasive behavior.
引用
收藏
页码:139 / 150