Oxidation of Hafnium Diboride-Silicon Carbide at 1500 °C in Air; Effect of Compressive Stress

被引:1
|
作者
DeGregoria, A. J. [1 ]
Ruggles-Wrenn, M. B. [1 ]
Pry, G. E. [1 ]
机构
[1] Air Force Inst Technol, Wright Patterson AFB, OH 45433 USA
关键词
hafnium diboride; oxidation; silicon carbide; ultra-high temperature ceramics; HIGH TEMPERATURE CERAMICS; ZIRCONIUM DIBORIDE; ZRB2; DENSIFICATION; COMPOSITES; RESISTANCE; BEHAVIOR; HFB2;
D O I
10.1007/s11665-022-07610-w
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The long-term oxidation behavior of HfB2 and of HfB2-20 vol.% SiC was studied. Test samples of each material were oxidized at 1500 degrees C in air using a box furnace. The exposure times were 0, 0.5, 1, 2, 3, 6, 9, 12, 15, 30, 45 and 90 h. Weight gain, oxide scale composition and oxide scale thickness were characterized for both materials. Crystal structure of the surface scales was analyzed using x-ray diffraction. Oxide scales were further characterized via scanning electron microscopy with energy dispersive spectroscopy analysis. For HfB2 the oxide scale consists predominantly of porous HfO2. For HfB2-20 vol.% SiC, the oxide scale is composed of a borosilicate glass outer layer and a porous HfO2 layer. Weight gain and the growth of oxide scale with exposure time were measured. The oxidation kinetics were determined using the weight gain as well as the scale thickness measurements, and the parabolic rate constants were calculated for both materials. The addition of SiC dramatically inhibited the oxidation of HfB2. The effects of compressive stress on oxidation of HfB2-20 vol.% SiC were also examined. Samples were oxidized while being subjected to compressive stress of 50-150 MPa for up to 30 h at 1500 degrees C in air. Compressive stress was found to have little effect on the growth of oxide scale with time. The oxidation data were analyzed in terms of mechanistic models for the oxidation of monolithic and SiC-containing refractory diborides. For HfB2-20 vol.% SiC, the model predictions agreed well with experimental data. For HfB2, the model significantly under-predicted the scale thickness, but accounted for weight gain reasonably well except for the longest exposure time of 90 h.
引用
收藏
页码:6747 / 6758
页数:12
相关论文
共 50 条
  • [21] Liquid Oxide Flow During Oxidation of Zirconium Diboride-Silicon Carbide Ultra High Temperature Ceramics
    Gangireddy, Sindhura
    Karlsdottir, Sigrun N.
    Halloran, John W.
    HIGH-PERFORMANCE CERAMICS VI, 2010, 434-435 : 144 - +
  • [22] Oxidation of zirconium diboride-silicon carbide ceramics under an oxygen partial pressure of 200 Pa: Formation of zircon
    Gao, Dong
    Zhang, Yue
    Fu, Jingying
    Xu, Chunlai
    Song, Yang
    Shi, Xiaobin
    CORROSION SCIENCE, 2010, 52 (10) : 3297 - 3303
  • [23] Micromechanics modeling of creep fracture of zirconium diboride-silicon carbide composites at 1400-1700 °C
    Yu, C. H.
    Bird, M. W.
    Huang, C. W.
    Chen, C. S.
    Gao, Y. F.
    White, K. W.
    Hsueh, C. H.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2014, 34 (16) : 4145 - 4155
  • [24] Scratch-induced microplasticity and microcracking in zirconium diboride-silicon carbide composite
    Ghosh, Dipankar
    Subhash, Ghatu
    Radhakrishnan, Ramachandran
    Sudarshan, Tirumalai S.
    ACTA MATERIALIA, 2008, 56 (13) : 3011 - 3022
  • [25] Elastic properties and microcracking behavior of particulate titanium diboride-silicon carbide composites
    Pan, MJ
    Hoffman, PA
    Green, DJ
    Hellmann, JR
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1997, 80 (03) : 692 - 698
  • [26] Titanium diboride-silicon carbide-boron carbide ceramics with super-high hardness and strength
    Neuman, Eric W.
    Brown-Shaklee, Harlan J.
    Hilmas, Gregory E.
    Fahrenholtz, William G.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2018, 101 (02) : 497 - 501
  • [27] Thermo-chemical compatibility of hafnium diboride with yttrium aluminum garnet at 1500 °C in air
    Winder, S. L.
    Ruggles-Wrenn, M. B.
    Parthasarathy, T.
    Key, T.
    Carney, C. M.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2015, 35 (09) : 2437 - 2444
  • [28] Processing, properties and arc jet oxidation of hafnium diboride/silicon carbide ultra high temperature ceramics
    Gasch, M
    Ellerby, D
    Irby, E
    Beckman, S
    Gusman, M
    Johnson, S
    JOURNAL OF MATERIALS SCIENCE, 2004, 39 (19) : 5925 - 5937
  • [29] Processing, properties and arc jet oxidation of hafnium diboride/silicon carbide ultra high temperature ceramics
    M. Gasch
    D. Ellerby
    E. Irby
    S. Beckman
    M. Gusman
    S. Johnson
    Journal of Materials Science, 2004, 39 : 5925 - 5937
  • [30] Temperature-dependent mechanical and long crack behavior of zirconium diboride-silicon carbide composite
    Bird, Marc W.
    Aune, Robert P.
    Thomas, Alfred F.
    Becher, Paul F.
    White, Kenneth W.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (12) : 3453 - 3462