共 50 条
- [41] THE EFFECT OF HYDROGEN ON MECHANICAL-PROPERTIES IN TI-10V-2FE-3AL METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1987, 18 (08): : 1421 - 1430
- [44] HOT DIE FORGING OF TITANIUM TI-10V-2FE-3AL - AN UPDATE JOURNAL OF METALS, 1982, 35 (12): : A52 - A52
- [45] PHASE-TRANSFORMATIONS AND TENSILE PROPERTIES OF TI-10V-2FE-3AL METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1980, 11 (12): : 1987 - 1998
- [49] THE ROLE OF DEFECT SIZE ON THE FRACTURE-TOUGHNESS OF POWDER PROCESSED TI-10V-2FE-3AL SCRIPTA METALLURGICA, 1989, 23 (07): : 1147 - 1150
- [50] Microscopic evaluation of fracture processes in powder blended elemental Ti-10V-2Fe-3Al alloy NON-AEROSPACE APPLICATIONS OF TITANIUM, 1998, : 61 - 67