Mode-II fracture toughness of carbon fiber reinforced polymer composites interleaved with polyethersulfone (PES)/carbon nanotubes (CNTs)

被引:11
|
作者
Liu, Yue [1 ]
Wang, Gong-dong [1 ,2 ]
Shen, Yichao [1 ]
Blackie, Ebo [1 ]
He, Long [2 ]
机构
[1] Shenyang Aerosp Univ, Sch Aerosp Engn, Dept Aeronaut Engn, Shenyang 110126, Peoples R China
[2] Zhiyuan Res Inst, Hangzhou 310012, Peoples R China
关键词
Fracture toughness; Environmental treatment; Interleaf; Delamination; DELAMINATION; BUCKYPAPER; BEHAVIOR;
D O I
10.1016/j.compstruct.2023.117214
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
A comprehensive experimental investigation was carried out to evaluate the toughening behavior of polyethersulfone (PES) and carbon nanotubes (CNTs) interleaf with similar thicknesses for carbon fiber reinforced polymer (CFRP) composites under mode II fracture loading. The influence of four different environmental conditions (room temperature, -55 degrees C, temperature changes between -55 degrees C and 80 degrees C, and salt spray) on mode II fracture toughness (GIIC) was discussed. The flexural property of CFRP composites before and after introducing interleaves was employed at room temperature. Effective diffusion of CNTs is a key means to enhance the interlaminar properties of CFRP composites without sacrificing the bending properties. Results show that CNTs and PES/CNT1 (when the CNTs content is 1 wt%) interleaves could enhance the GIIC by 118.4% and 317.81%, respectively. Hybrid PES/CNTs interleaf exhibited higher mode II fracture toughness and greater adaptability to the environment. The fracture behavior was demonstrated with experimental results and related scanning electron microscopy (SEM) images.
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Effect of nanomaterial on mode I and mode II interlaminar fracture toughness of woven carbon fabric reinforced polymer composites
    Srivastava, Vijay K.
    Gries, Thomas
    Veit, Dieter
    Quadflieg, Till
    Mohr, Benjamin
    Kolloch, Martin
    ENGINEERING FRACTURE MECHANICS, 2017, 180 : 73 - 86
  • [22] Characterization of carbon nanotube enhanced interlaminar fracture toughness of woven carbon fiber reinforced polymer composites
    Chaudhry, M. S.
    Czekanski, A.
    Zhu, Z. H.
    INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2017, 131 : 480 - 489
  • [23] Influence of sprayed multi-walled carbon nanotubes on mode I and mode II interlaminar fracture toughness of carbon fiber/epoxy composites
    Rodriguez-Gonzalez, J. A.
    Rubio-Gonzalez, C.
    ADVANCED COMPOSITE MATERIALS, 2019, 28 (sup1) : 19 - 36
  • [24] Enhancing interlaminar fracture toughness of carbon fiber/epoxy composites toughened by polyethersulfone resin and hybrid carbon nanotubes/graphene oxide
    Wang, Gongdong
    Liu, Xueqing
    Wang, Meng
    Yu, Mingchi
    Zhang, Hongxiang
    He, Long
    POLYMER COMPOSITES, 2024,
  • [25] FRACTURE-TOUGHNESS AND FIBER BRIDGING OF CARBON-FIBER REINFORCED CARBON COMPOSITES
    SAKAI, M
    MIYAJIMA, T
    INAGAKI, M
    COMPOSITES SCIENCE AND TECHNOLOGY, 1991, 40 (03) : 231 - 250
  • [26] Model I Interlaminar Fracture Toughness of Carbon Fiber Reinforced Polymer Matrix Composites
    Ji, Aihong
    Lu, Min
    Zha, Meng
    Dong, Benzheng
    Gao, Lihong
    Dai, Zhendong
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING IV, PTS 1 AND 2, 2014, 887-888 : 81 - +
  • [27] EFFECTS OF STRAIN-RATE ON MODE-II INTERLAMINAR FRACTURE-TOUGHNESS IN CARBON-FIBER EPOXY LAMINATED COMPOSITES
    KUSAKA, T
    YAMAUCHI, Y
    KUROKAWA, T
    JOURNAL DE PHYSIQUE IV, 1994, 4 (C8): : 671 - 676
  • [28] Fracture toughness of additively manufactured carbon fiber reinforced composites
    Papon, Easir Arafat
    Haque, Anwarul
    ADDITIVE MANUFACTURING, 2019, 26 : 41 - 52
  • [29] Toughness and Fracture Mechanism of Carbon Fiber Reinforced Epoxy Composites
    李媛媛
    嵇宇
    谷志旗
    李秋雅
    何鸿喆
    张岩
    王萍
    眭建华
    Journal of Donghua University(English Edition), 2022, 39 (03) : 193 - 205
  • [30] Fracture toughness of carbon fiber reinforced composites with rubber modification
    Takemura, Kenichi
    ADVANCES IN COMPOSITE MATERIALS AND STRUCTURES, PTS 1 AND 2, 2007, 334-335 : 509 - 512