UH3 produced at the initial stage of U-H2O corrosion

被引:3
|
作者
Li, Haibo [1 ]
Wang, Shuaipeng [2 ]
Li, Gan [1 ]
Wu, Haoxi [2 ]
Pu, Zhen [2 ]
Bin, Ren [1 ]
Meng, Daqiao [2 ]
Luo, Wenhua [1 ]
机构
[1] Sci & Technol Surface Phys & Chem Lab, Mianyang 621908, Peoples R China
[2] China Acad Engn Phys, Inst Mat, Mianyang 621907, Peoples R China
基金
中国国家自然科学基金;
关键词
Interfacial UH 3; Raman spectroscopy; U-H 2 O reaction; Corrosion mechanisms; Isotopic labelling method; URANIUM HYDRIDE; LIQUID WATER; RAMAN; SPECTROSCOPY; DESORPTION; OXIDATION; KINETICS; VAPOR; AIR;
D O I
10.1016/j.corsci.2023.111143
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The characteristic Raman spectra of UH3 produced at the initial stage of U-H2O corrosion were observed, which provided direct evidence of the existence of water-formed interfacial UH3. The results were further identified and confirmed using the isotopic labelling method and other characterization techniques. The water-formed hydride layer was distributed at the interface of metallic uranium and oxide exhibiting several nanometers of thickness via the depth profile analysis. The characterizations of oxidation behavior suggested that the interfacial UH3 transformed to oxide and acted as a reaction front in the corrosion process. The experimental results supported the hydride-catalyzed corrosion mechanism of wet oxidation.
引用
收藏
页数:7
相关论文
共 50 条
  • [21] WEDGING ACTION OF UH3 DURING SLOW CRACK GROWTH IN U-0.75 WT-PERCENT TI
    MAGNANI, NJ
    CORROSION, 1975, 31 (09) : 337 - 338
  • [22] Ab initio calculations of the uranium-hydrogen system: Thermodynamics, hydrogen saturation of α-U and phase-transformation to UH3
    Taylor, Christopher D.
    Lookman, Turab
    Lillard, R. Scott
    ACTA MATERIALIA, 2010, 58 (03) : 1045 - 1055
  • [23] INITIAL STAGE SINTERING OF Y2O3
    ANDERSON, RC
    AMERICAN CERAMIC SOCIETY BULLETIN, 1966, 45 (04): : 363 - &
  • [24] NaNi(H2PO3)3•H2O as a novel corrosion inhibitor for X70-steel in saline produced water
    Deyab, M. A.
    El Bali, B.
    Essehli, R.
    Ouarsal, R.
    Lachkar, M.
    Fuess, H.
    JOURNAL OF MOLECULAR LIQUIDS, 2016, 216 : 636 - 640
  • [25] TEMPERATURE EFFECT IN RANGE FROM 20 TO 250 DEGREES C IN CASE OF SOME STRICTLY REGULAR HETEROGENEOUS U-H2O CRITICAL ASSEMBLIES
    BAT, GA
    USHAKOV, YV
    ZARUBIN, YV
    OBUKHOV, VK
    GULIMOV, VN
    SOVIET ATOMIC ENERGY-USSR, 1971, 30 (04): : 436 - &
  • [26] Reactions of Uranium Atoms with Ammonia: Infrared Spectra and Quasi-Relativistic Calculations of the U:NH3, H2N-UH, and HN=UH2 Complexes
    Wang, Xuefeng
    Andrews, Lester
    Marsden, Colin J.
    CHEMISTRY-A EUROPEAN JOURNAL, 2008, 14 (30) : 9192 - 9201
  • [27] INITIAL-STAGE SINTERING MECHANISMS IN AL2O3
    DYNYS, JM
    COBLE, RL
    CANNON, RM
    AMERICAN CERAMIC SOCIETY BULLETIN, 1979, 58 (03): : 342 - 342
  • [28] KINETICS OF INITIAL-STAGE SINTERING OF AL2O3
    BIGGERS, JV
    BIND, JM
    AMERICAN CERAMIC SOCIETY BULLETIN, 1977, 56 (03): : 291 - 291
  • [29] Molecular insights into the effect of adsorption and reaction of H2O-O2-Cl- on initial electrochemical corrosion of steel
    Nong, Yumei
    Chen, Zheng
    Chen, Ye
    Tang, Yunchao
    Wang, Yichen
    Liu, Kexin
    Qin, Mingqiang
    ELECTROCHIMICA ACTA, 2025, 511
  • [30] Probing the initial stages of iron surface corrosion: Effect of O2 and H2O on surface carbonation
    de Alwis, Chathura
    Trought, Mikhail
    Crumlin, Ethan J.
    Nemsak, Slavomir
    Perrine, Kathryn A.
    APPLIED SURFACE SCIENCE, 2023, 612