Development of textured lead-free NBT-based piezoelectric materials in a matrix, synthesized by an alternative route, via templated grain growth

被引:2
|
作者
Coban-Tetik, Hatice Sule [1 ,2 ,5 ]
Suvaci, Ender [1 ,3 ]
Avci, A. Murat [3 ]
Adem, Umut [4 ]
Karakaya, Merve [4 ]
机构
[1] Eskisehir Tech Univ, Dept Mat Sci & Engn, TR-26555 Eskisehir, Turkiye
[2] Agri Ibrahim Cecen Univ, Cent Res & Applicat Lab, TR-04100 Agri, Turkiye
[3] Entekno Mat Corp, Eskisehir, Turkiye
[4] Izmir Inst Technol, Dept Mat Sci & Engn, TR-35430 Izmir, Turkiye
[5] Agri Ibrahim Cecen Univ, Dept Comp Engn, TR-04100 Agri, Turkiye
关键词
SODIUM BISMUTH TITANATE; ELECTRIC-FIELD; FERROELECTRIC PROPERTIES; CERAMICS; MICROSTRUCTURE;
D O I
10.1007/s10854-022-09710-8
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
In this study, (1-x)(K0.5Bi0.5TiO3-BaTiO3)-xNa(0.5)Bi(0.5)TiO(3) KBT:BT = 2:1 where x = 0.8 (KBT-BT-NBT) (001) textured lead-free piezoelectric ceramics were fabricated using BT template by templated grain growth with tape casting. Unlike the commonly used matrix preparation method, which is the calcination of all raw materials in one step, the matrix phase was prepared in a different way by first preparing KBT, BT and NBT powders separately and then by calcining the mixtures of these powders, so that effect of the matrix, synthesized by this alternative route, on texture development properties was evaluated. In addition, the effect of BT template content on the grain orientation with different sintering temperature and time, structure evolution, phase stability and piezoelectric properties were investigated to assess the materials' actuating performance. The highest Lotgering factor of 81% was achieved for the textured ceramics with 10 wt% BT templates sintered at 1150 degrees C for 48 h. Compared to the one-step synthesis method, similar Lotgering factor values were obtained at lower sintering temperatures in the matrix, synthesized by the alternative 2-step method. The highest piezoelectric constant, remnant polarization, strain value and depolarization temperature were also obtained from the same sample, as similar to 190 pC/N, 30 kV/cm, 25% at 50 kV/cm and similar to 165 degrees C, respectively. The results show that the textured, lead free K0.5Bi0.5TiO3-BaTiO3-Na0.5Bi0.5TiO3 (KBT-BT-NBT) ceramics that are developed by using the matrix, synthesized by the alternative 2-step method, can be very promising lead-free electroceramics for high performance actuator applications.
引用
收藏
页数:14
相关论文
共 23 条
  • [21] Abnormal grain growth and new core-shell structure in (K,Na)NbO3-based lead-free piezoelectric ceramics
    Zhen, Yuhua
    Li, Jing-Feng
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (11) : 3496 - 3502
  • [22] Grain-oriented sodium bismuth titanate-based lead-free piezoelectric ceramics prepared using the pulsed strong magnetic field and template grain growth
    Zhao, Jun
    Wang, Fajun
    Li, Wen
    Li, Hui
    Zhou, Dongxiang
    Gong, Shuping
    Hu, Yunxiang
    Fu, Qiuyun
    JOURNAL OF APPLIED PHYSICS, 2010, 108 (07)
  • [23] NaNbO3 templates-induced phase evolution and enhancement of electromechanical properties in <001> grain oriented lead-free BNT-based piezoelectric materials
    Bai, Wangfeng
    Chen, Daqin
    Zheng, Peng
    Xi, Junhua
    Zhou, Yang
    Shen, Bo
    Zhai, Jiwei
    Ji, Zhenguo
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (07) : 2591 - 2604