Corrosion of a spark plasma sintered Fe-Cr-Mo-B-C alloy in 3.5% NaCl solution

被引:1
|
作者
Farooq, Mudassir [1 ,3 ]
Muhammad, Sohail [3 ]
Sorour, A. A. [1 ,2 ]
机构
[1] King Fahd Univ Petr & Minerals KFUPM, Dept Mech Engn, Dhahran 31261, Saudi Arabia
[2] King Fahd Univ Petr & Minerals KFUPM, Interdisciplinary Res Ctr Adv Mat, Dhahran 31261, Saudi Arabia
[3] NED Univ Engn & Technol, Dept Mat Engn, Karachi 75270, Pakistan
来源
关键词
Corrosion; Powder metallurgy; Amorphous alloy powder; Passive film; BULK METALLIC GLASSES; STAINLESS-STEEL; MECHANICAL-PROPERTIES; AMORPHOUS-ALLOYS; PASSIVE FILMS; BEHAVIOR; XPS; NANOCRYSTALLIZATION; ADSORPTION; PLASTICITY;
D O I
10.55713/jmmm.v33i1.1588
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the corrosion behavior of a Fe-Cr-Mo-B-C alloy, fabricated by spark plasma sintering of an amorphous alloy powder, in 3.5% NaCl solution was analyzed. Electrochemical impedance spectroscopy and potentiodynamic polarization are techniques which were used for electrochemical performance estimation of samples and the results were further compared with conventional alloys: 1080 carbon steel and 304 stainless steel. Corrosion surface products were characterized through Scanning electron microscopy, Energy dispersive x-ray spectroscopy and X-ray photoelectron spectroscopy. Specimens sintered at 800 degrees C (S1-800) had achieved 94% densification approximately while the sample sintered at 900 degrees C (S2-900), had densified more which was 98% approximately. S2-900 had better corrosion resistance than S1-800 while in comparison to conventional alloys; it was inferior to 304 stainless steel. It was concluded that the increase in density of sintered samples favoured the formation of more uniform surface products and enhanced the formation of the passive chromium oxide (Cr2O3) layer.
引用
收藏
页码:27 / 38
页数:12
相关论文
共 50 条
  • [31] Preparation of Cu-Ni-Fe alloy coating and its evaluation on corrosion behavior in 3.5% NaCl solution
    Zhou, Qiongyu
    Jiang, Jibo
    Zhong, Qingdong
    Wang, Yi
    Li, Ke
    Liu, Huijuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 563 : 171 - 175
  • [32] Corrosion Behavior of New Cu-Sn-Fe-Ni Alloy in 3.5wt% NaCl Solution
    Xie, Wang
    Qian, Lei
    Yong, Liu
    RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (11) : 3893 - 3899
  • [33] Berberine as an Effective Corrosion Inhibitor for 7075 Aluminium Alloy in 3.5% NaCl Solution
    Singh, Ambrish
    Lin, Yuanhua
    Liu, Wanying
    Pan, Jie
    Ren, Chengqiang
    Zeng, Dezhi
    Yu, Shijie
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2014, 9 (09): : 5164 - 5176
  • [34] Microstructure and mechanical properties of a spark plasma sintered Fe-11Cr-2.3B-6Al-15Mn alloy
    Liu, Jian
    Chen, Weiping
    VACUUM, 2018, 150 : 49 - 57
  • [35] Corrosion behavior of WE54 magnesium alloy in 3.5%NaCl solution
    李卓群
    单大勇
    陈荣石
    柯伟
    韩恩厚
    Transactions of Nonferrous Metals Society of China, 2006, (S3) : 1806 - 1809
  • [36] Corrosion behavior of WE54 magnesium alloy in 3.5%NaCl solution
    Li Zhuo-qun
    Shan Da-yong
    Chen Rong-shi
    Ke Wei
    Han En-hou
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1806 - S1809
  • [37] Corrosion behavior of WE54 magnesium alloy in 3.5%NaCl solution
    Environmental Corrosion Center, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    Trans Nonferrous Met Soc China, 2006, SUPPL. 3 (1806-1809):
  • [38] Mapping the fretting corrosion behaviors of 6082 aluminum alloy in 3.5% NaCl solution
    Pu, Jian
    Zhang, Yali
    Zhang, Xiaogang
    Yuan, Xinlu
    Ren, Pingdi
    Jin, Zhongmin
    WEAR, 2021, 482
  • [39] Corrosion Resistance of Cu-modified 3Cr Low-alloy Steel in 3.5%NaCl Solution
    Wu, Qianlin
    Zhang, Zhonghua
    Liu, Yaoheng
    Qi, Yameng
    ISIJ INTERNATIONAL, 2017, 57 (05) : 905 - 912
  • [40] Corrosion behavior of HVOF sprayed Cr3C2-NiCr coating in 3.5 %NaCl solution
    Guo, Ji
    Li, Gaiye
    Wu, Yuping
    Hong, Sheng
    Hanjie Xuebao/Transactions of the China Welding Institution, 2015, 36 (02): : 109 - 112