The Effects of Oscillating Frequency on Microstructure and Hardness of W-Ni-Fe Refractory Alloy Sintered by Hot Oscillating Pressure

被引:1
|
作者
Gao, Ka [1 ]
Hu, Yanghu [2 ]
Zhang, Zixiang [1 ]
Ren, Chunyang [1 ]
Zhao, Wei [3 ]
Sun, Dejian [4 ]
Gao, Yang [4 ]
An, Linan [5 ]
Kong, Qingquan [6 ]
机构
[1] Univ Shanghai Sci & Technol, Sch Mech Engn, Shanghai 200093, Peoples R China
[2] China Natl Heavy Machinery Res Inst Co Ltd, State Key Lab Met Extrus & Forging Equipment Techn, Xian 710000, Peoples R China
[3] Changhai Hosp, Dept Gen Med, Shanghai 200000, Peoples R China
[4] Zhengzhou Univ Aeronaut, Sch Mat Sci & Engn, Zhengzhou 450015, Peoples R China
[5] Dongguan Univ Technol, Sch Mech Engn, Dongguan 523808, Peoples R China
[6] Chengdu Univ, Sichuan Prov Engn Technol Res Ctr Powder Met, Chengdu 610106, Peoples R China
基金
中国国家自然科学基金;
关键词
hardness; hot oscillating pressure; microstructure; oscillating frequency; W-Ni-Fe alloy; MECHANICAL-PROPERTIES; HEAVY ALLOYS; TUNGSTEN; DENSIFICATION; TEMPERATURE;
D O I
10.1002/adem.202301326
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
90 W-7Ni-3Fe refractory alloys are first sintered by hot oscillating pressure (HOP) under different oscillating frequencies (0, 1, and 10 Hz) in this work. The effects of oscillating frequencies on the microstructure and Vickers hardness are investigated. With the oscillating frequency increasing, the relative density and hardness of refractory alloys are obviously improved. Especially, the alloy sintered at the oscillating frequency of 10 Hz had the highest relative density of approximately 98.9% and the smallest average grain size of 3.26 mu m. Moreover, the narrowest average thickness of the bonding phase is about 0.18 mu m, and the lowest tungsten contiguity is about 61.1%. Then its excellent hardness (456.8 HV30) is obtained, which is nearly 16.1% higher than that of the 0 Hz frequency alloy. The refractory alloy with high densification, small grain size, and good hardness could be obtained by HOP with a high oscillating frequency. W-Ni-Fe refractory alloy is prepared by hot oscillating pressure at different oscillating frequencies (0, 1, and 10 Hz). The higher relative density (98.9%) and excellent hardness (456.8 HV30) of sintered alloys with the narrowest average thickness bonding phase (0.18 mu m), lowest tungsten contiguity (61.1%), and smallest grain size (3.26 mu m) are significantly improved through higher oscillating frequency applied.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:6
相关论文
共 50 条
  • [41] Densification, Microstructure Evolution, and Mechanical Properties of Low-Temperature-Sintered 90W-4.9Ni-2.1Fe-3Cu Alloy
    Wentan Zhu
    Wensheng Liu
    Yunzhu Ma
    Qingshan Cai
    Jianning Wang
    Youteng Duan
    Journal of Materials Engineering and Performance, 2021, 30 : 2761 - 2771
  • [42] Microstructure and mechanical properties of spark plasma-sintered La2O3 dispersion-strengthened W–Ni–Fe alloy
    Muthuchamy AyyappaRaj
    Digvijay Yadav
    Dinesh K. Agrawal
    Raja Annamalai Arunjunai Rajan
    Rare Metals, 2021, 40 : 2230 - 2236
  • [43] Densification, Microstructure Evolution, and Mechanical Properties of Low-Temperature-Sintered 90W-4.9Ni-2.1Fe-3Cu Alloy
    Zhu, Wentan
    Liu, Wensheng
    Ma, Yunzhu
    Cai, Qingshan
    Wang, Jianning
    Duan, Youteng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (04) : 2761 - 2771
  • [44] Effects of Al2O3 micro/nanoparticles on the microstructure and corrosion behavior of W-Ni-Fe matrix through spark plasma sintering process
    Hasanabadi, Mostafa
    Azadi, Mahboobeh
    Yousefpour, Mardali
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 747 - 759
  • [45] Effect of heat treatment on microstructure and mechanical properties of hot-hydrostatically extruded 93W-4.9Ni-2.1Fe alloy
    Yu, Yang
    Zhang, Wencong
    Wang, Erde
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 622 : 880 - 884
  • [46] Microstructure and mechanical characterizations of liquid phase sintered W-Ni-Cu heavy alloy modified with La2O3 and Fe addition
    Shakunt, Navindra Shekhar
    Gouthama
    Upadhyaya, Anish
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2025, 127
  • [47] Effects of Spark Plasma Sintering Temperature on Microstructure and Dynamic Mechanical Properties of 93W-4.9Ni-2.1Fe Alloy
    Wang Yingchun
    Li Shukui
    Wang Fuchi
    Luo Hongzhi
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (10) : 1807 - 1810
  • [48] Effects of spark plasma sintering temperature on microstructure and dynamic mechanical properties of 93W-4.9Ni-2.1Fe alloy
    Wang, Yingchun
    Li, Shukui
    Wang, Fuchi
    Luo, Hongzhi
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2010, 39 (10): : 1807 - 1810
  • [49] Effects of Y2O3 on the microstructure and mechanical properties of spark plasma sintered fine-grained W-Ni-Mn alloy
    Yanlin Pan
    Lei Ding
    Hui Li
    Daoping Xiang
    Journal of Rare Earths, 2017, 35 (11) : 1149 - 1155
  • [50] Effects of Y2O3 on the microstructure and mechanical properties of spark plasma sintered fine-grained W-Ni-Mn alloy
    Pan, Yanlin
    Ding, Lei
    Li, Hui
    Xiang, Daoping
    JOURNAL OF RARE EARTHS, 2017, 35 (11) : 1149 - 1155