Mechanical and tribological characteristics of hypo eutectic Al-7Si alloy-based composite reinforced with Sn metal powder and Al2O3 using bottom pouring stir casting technique

被引:1
|
作者
Ajay, C. Veera [1 ]
Hariharasakthisudhan, P. [2 ]
Anand, S. [1 ]
Sivasubramanian, I [1 ]
机构
[1] Natl Engn Coll, Dept Mech Engn, Thoothukudi, Tamil Nadu, India
[2] Sri Krishna Coll Technol, Dept Mech Engn, Coimbatore, Tamil Nadu, India
关键词
hypo eutectic Al-Si alloy; alumina; mechanical properties; wear rate; coefficient of friction; WEAR BEHAVIOR; MICROSTRUCTURE;
D O I
10.1088/1402-4896/acf968
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
The present work highlights the significant effects of varying wt% of Sn metal powder in the hypo eutectic Al-7Si/10 wt% Al2O3 composite. The composites were manufactured through a multi-stage stir casting route and characterized for mechanical and wear behavior using ASTM standards. The results revealed that the increase in Sn content up to 4 wt% in the matrix enhanced the microhardness, tensile properties, and reduced the porosity. The Al-7Si/10 wt% Al(2)O(3 )composite with 4% Sn particle reinforcement shows the highest tensile strength and hardness of 132 MPa and 90 BHN, respectively. All composites exhibited a ductile mode of failure, as evidenced by the tear ridges and dimples on the tensile fracture surface. By adding of Sn metal powder to the material system, the wear rate and coefficient of friction were reduced. At 1000 m of sliding distance and 1 ms(-1 )of sliding velocity, the wear loss of 8 wt% Sn composite was decreased by 88.8% as compared to Al-7Si base alloy at a normal load of 10 N whereas, at 40 N of normal load, the wear loss was decreased by 66.6%. During the wear process, the Sn metal powder surfaced and formed a thin tribo film that mechanically mixed with the surface, resulting in reduced friction. The layer at the interface prevented direct contact between asperities on the mating surface, which reduced wear loss. The composites without Sn metal powder exhibited adhesive wear and delamination as the primary wear mechanisms, while composites with Sn showed predominantly adhesive wear. Regression analysis followed by a desirability function approach was carried out to develop the model and optimize the operating conditions of the experiments.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] Mechanical behavior of AZ31/Al2O3 magnesium alloy nanocomposites prepared using ultrasound assisted stir casting
    Khandelwal, Apratim
    Mani, Karthick
    Srivastava, Neeraj
    Gupta, Rahul
    Chaudhari, G. P.
    COMPOSITES PART B-ENGINEERING, 2017, 123 : 64 - 73
  • [32] Development and mechanical characterization of LM6/Al2O3/SiC/Graphite metal matrix composites using stir casting
    Kandpal, Bhaskar Chandra
    Ramdas, Nilesh
    Singh, Lavish Kumar
    Alam, Mahtab
    Kumar, Brijesh
    Patel, Amit Singh
    Kumar Yadav, Anand
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2024, 10 (02) : 883 - 891
  • [33] Structure, thermal and mechanical properties of in situ Al-based metal matrix composite reinforced with Al2O3 and TiC submicron particles
    Yu, P
    Mei, Z
    Tjong, SC
    MATERIALS CHEMISTRY AND PHYSICS, 2005, 93 (01) : 109 - 116
  • [34] Microstructure, microhardness and tribological behavior of Al2O3 reinforced A380 aluminum alloy composite coatings prepared by cold spray technique
    Qiu, Xiang
    Tariq, Naeem ul Haq
    Wang, Ji-qiang
    Tang, Jun-rong
    Gyansah, Lawrence
    Zhao, Zhi-po
    Xiong, Tian-ying
    SURFACE & COATINGS TECHNOLOGY, 2018, 350 : 391 - 400
  • [35] AMORPHOUS-CERAMIC Ni-BASED COMPOSITE REINFORCED WITH Al2O3 PROCESSED BY MECHANICAL ALLOYING AND POWDER CONSOLIDATION
    Oleszak, Dariusz
    Kulik, Tadeusz
    Kolesnikov, Dmitro
    COMPOSITES THEORY AND PRACTICE, 2007, 7 (04): : 195 - 199
  • [36] Characterization and Mechanical Properties of 2014 Aluminum Alloy Reinforced with Al2O3p Composite Produced by Two-Stage Stir Casting Route
    Bharath V.
    Ajawan S.S.
    Nagaral M.
    Auradi V.
    Kori S.A.
    Journal of The Institution of Engineers (India): Series C, 2019, 100 (02): : 277 - 282
  • [37] Microstructural, Mechanical and Strengthening Mechanisms of Al7075 Metal Matrix Composite with Al2O3 Nano Particle Processed Through Ultrasonic Cavitation Assisted Stir-casting
    Kumar, Malleveni Shravan
    Kumar, Jyothula Suresh
    Maddaiah, K. Chinna
    Kumar, M. Ranjith
    JOURNAL OF POLYMER & COMPOSITES, 2024, 12 (01) : 31 - 43
  • [38] Microstructure Evaluation and Wear Resistance Property of Al-Si-X/Al2O3 Composite by the Displacement Reaction in Al-Mg Alloy Melt using High Energy Mechanical Milled Al-SiO2-X Composite Powder
    Do Woo, Kee
    Kim, Dong Keon
    Lee, Hyun Bom
    Moon, Min Seok
    Ki, Woong
    Kwon, Eui Pyo
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2008, 18 (06): : 339 - 346
  • [39] Characteristics of A6061/(Glass Fibre + AL2O3 + SiC + B4C) Reinforced Hybrid Composite Prepared through STIR Casting
    Nanjan, Subramani
    Janakiram, Ganesh Murali
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2019, 2019
  • [40] Influence on Microstructural and Mechanical Properties of Al2O3/Graphite/Flyash-Reinforced Hybrid Composite Using Scrap Aluminum Alloy
    Chechi, Prashant
    Maurya, Saurabh Kumar
    Prasad, Rabindra
    Manna, Alakesh
    INTERNATIONAL JOURNAL OF METALCASTING, 2024, 18 (02) : 975 - 986